Wetting, droplet evaporation and corrosion behavior of various composite and textured materials

被引:5
作者
Misyura, S. Y. [1 ]
Morozov, V. S. [1 ]
Orlova, E. G. [2 ]
Andryushchenko, V. A. [1 ]
机构
[1] Russian Acad Sci, Kutateladze Inst Thermophys, Siberian Branch, 1 Lavrentyev Ave, Novosibirsk 630090, Russia
[2] Natl Res Tomsk Polytech Univ, 30 Lenin Ave, Tomsk 634050, Russia
基金
俄罗斯科学基金会;
关键词
Composite material; Corrosion; Wettability; Contact angle hysteresis; Evaporation rate; SUPERHYDROPHOBIC SURFACE; SESSILE DROPLET; HEAT-TRANSFER; GRAPHENE; ALUMINUM; WATER; RESISTANCE; CONVERSION; MICRO; FABRICATION;
D O I
10.1016/j.ceramint.2024.03.026
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Experimental studies were conducted on the evaporation rate of a droplet located on the surfaces of various composite and textured materials with different wettability at varying surface temperatures. The maximum droplet evaporation rate was recorded on a textured Cu-SiC composite material with superhydrophilic properties. The minimum droplet evaporation rate corresponded to a superhydrophobic AlMg3 substrate obtained using laser texturing with subsequent hydrophobization procedure. An increase in surface temperature led to a significant deterioration of hydrophobicity for a superhydrophobic substrate and a deterioration of hydrophilicity for a superhydrophilic substrate. As a result, with increasing temperature, the influence of the droplet geometry determined by surface wettability on the droplet evaporation rate for these substrates sharply decreases. Advancing and receding dynamic contact angles, as well as contact angle hysteresis were obtained on all studied substrates. It is generally accepted that a hydrophobic surface exhibits less contact angle hysteresis than a hydrophilic one. However, Cu-Si & Scy; composite substrate with a textured hydrophobic surface exhibited the opposite behavior. The contact angle hysteresis on the hydrophobic textured surface was found to be four times higher than that on the hydrophilic polished one. A mechanism was proposed that explains the high contact angle hysteresis and four hysteresis time modes. The minimum hysteresis value corresponded to the superhydrophobic AlMg3 substrate. Anti-corrosion properties were studied for all substrates under consideration. The minimum corrosion current corresponded to a copper substrate with a graphene coating, as well as a superhydrophobic AlMg3 substrate. For a given substrate, there are two corrosion modes with a three-fold difference in the corrosion current. In addition, the wettability behavior of different surfaces was examined using molecular dynamics simulations. The simulation results were found to be consistent with the experimental data.
引用
收藏
页码:19269 / 19282
页数:14
相关论文
共 85 条
  • [21] Nanosecond laser micro- and nanotexturing for the design of a superhydrophobic coating robust against long-term contact with water, cavitation, and abrasion
    Emelyanenko, Alexandre M.
    Shagieva, Farida M.
    Domantovsky, Alexandr G.
    Boinovich, Ludmila B.
    [J]. APPLIED SURFACE SCIENCE, 2015, 332 : 513 - 517
  • [22] INCREASING THE ENERGY EFFICIENCY OF COOLING SYSTEMS FOR ENERGY-SATURATED EQUIPMENT BY SHIFTING THE SECOND KIND HEAT TRANSFER CRISIS TO THE HIGHER TEMPERATURE REGION
    Feoktistov, Dmitry, V
    Kuznetsov, Geniy, V
    Abedtazehabadi, Akram
    Orlova, Evgeniya G.
    Bondarchuk, Stepan P.
    V. Dorozhkin, Alexander
    [J]. BULLETIN OF THE TOMSK POLYTECHNIC UNIVERSITY-GEO ASSETS ENGINEERING, 2023, 334 (04): : 72 - 88
  • [23] Preparation and application of microfluidic SERS substrate: Challenges and future perspectives
    Guo, Jiuchuan
    Zeng, Fanyu
    Guo, Jinhong
    Ma, Xing
    [J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 37 (37): : 96 - 103
  • [24] Recent progress in Axisymmetric Drop Shape Analysis (ADSA)
    Hoorfar, M.
    Neumann, A. W.
    [J]. ADVANCES IN COLLOID AND INTERFACE SCIENCE, 2006, 121 (1-3) : 25 - 49
  • [25] Technical note:: Concerning the conversion of the constant phase element parameter Y0 into a capacitance
    Hsu, CH
    Mansfeld, F
    [J]. CORROSION, 2001, 57 (09) : 747 - 748
  • [26] Evaporation of a sessile droplet on a substrate
    Hu, H
    Larson, RG
    [J]. JOURNAL OF PHYSICAL CHEMISTRY B, 2002, 106 (06) : 1334 - 1344
  • [27] Surface-wetting characterization using contact-angle measurements
    Huhtamaki, Tommi
    Tian, Xuelin
    Korhonen, Juuso T.
    Ras, Robin H. A.
    [J]. NATURE PROTOCOLS, 2018, 13 (07) : 1521 - 1538
  • [28] Real-time electrical detection of nitric oxide in biological systems with sub-nanomolar sensitivity
    Jiang, Shan
    Cheng, Rui
    Wang, Xiang
    Xue, Teng
    Liu, Yuan
    Nel, Andre
    Huang, Yu
    Duan, Xiangfeng
    [J]. NATURE COMMUNICATIONS, 2013, 4
  • [29] Molecular origin of contact line friction in dynamic wetting
    Johansson, Petter
    Hess, Berk
    [J]. PHYSICAL REVIEW FLUIDS, 2018, 3 (07):
  • [30] Jovic V.D., 2022, J MAT PROTECT, V63, P50, DOI DOI 10.5937/ZASMAT2201050J