Environmentally Assisted Cracking of Duplex and Lean Duplex Stainless Steel Reinforcements in Alkaline Medium Contaminated with Chlorides

被引:0
|
作者
Martin, Ulises [1 ,2 ]
Bastidas, David M. [2 ,3 ]
机构
[1] Texas A&M Univ, Dept Mat Sci & Engn, College Stn, TX 77843 USA
[2] Univ Akron, Natl Ctr Educ & Res Corros & Mat Performance, NCERCAMP UA, 302 E Buchtel Ave, Akron, OH 44325 USA
[3] ROSEN USA, 14120 Interdr East, Houston, TX 77032 USA
关键词
environmentally assisted cracking (EAC); slow strain rate test (SSRT); stainless steel; electrochemical kinetics; PITTING CORROSION-RESISTANCE; SUSCEPTIBILITY; MICROSTRUCTURE;
D O I
10.3390/cryst14070651
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
Herein, the corrosion performance of different stainless steel (SS) reinforcing bar grades in alkaline solution is presented, including UNS S32205 duplex stainless steel (DSS), UNS S32304 and UNS S32001 lean DDS (LDSS). The electrochemical dissolution kinetics were studied by potentiodynamic polarization and the Tafel slope method. The environmentally assisted cracking (EAC) mechanisms of the different SS grades in the presence of Cl- were revealed with the slow strain rate test (SSRT). The higher activation of the anodic branch and the loss of toughness were related to the austenite-to-ferrite phase ratio. UNS S32205 DSS presented the slowest anodic dissolution kinetics, mainly due to the higher austenite content compared to the other LDSS; however, it suffered a more severe EAC than the UNS S32304 LDSS. In the case of UNS S32001 LDSS, even while having the lowest Ni content (i.e., large ferrite alpha-phase ratio), it experienced the least decrease in elongation as well as low anodic dissolution kinetics for Cl- contents up to 8 wt.%, where the Cl- threshold was reached.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Investigating the Anisotropic Behaviour of Lean Duplex Stainless Steel 2101
    Ameri, A. A. H.
    Escobedo-Diaz, J. P.
    Ashraf, M.
    Quadir, Md. Z.
    CHARACTERIZATION OF MINERALS, METALS, AND MATERIALS 2017, 2017, : 181 - 190
  • [42] ε-Martensite formation for low strains in a lean duplex stainless steel
    Braga Maria, Graziele Gianini
    Rodrigues, Daniella Gomes
    Fraga Freitas, Erico Tadeu
    Santos, Dagoberto Brandao
    MATERIALS LETTERS, 2019, 234 : 283 - 286
  • [43] Localized hydrogen cracking in the austenitic phase of a duplex stainless steel
    Oltra, R
    Bouillot, C
    Magnin, T
    SCRIPTA MATERIALIA, 1996, 35 (09) : 1101 - 1105
  • [44] Stress corrosion cracking of sensitized duplex stainless steel weldment
    Osaka Univ, Ibaraki, Japan
    Zairyo, 6 (602-606):
  • [45] Correction to: Hot cracking in duplex stainless steel weldments — a review
    Elin M. Westin
    Welding in the World, 2022, 66 (8) : 1501 - 1502
  • [46] Stress Corrosion Cracking Behaviour of Welded Duplex Stainless Steel
    Khoshnaw, Fuad Mohamed
    Rahmatalla, Hussein Bakir
    THERMEC 2009 SUPPLEMENT: 6TH INTERNATIONAL CONFERENCE ON PROCESSING & MANUFACTURING OF ADVANCED MATERIALS, 2010, 89-91 : 709 - +
  • [47] Hydrogen-enhanced cracking of 2205 duplex stainless steel
    Tsay, L. W.
    Young, M. C.
    Shin, C. -S.
    Chan, S. L. I.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2007, 30 (12) : 1228 - 1236
  • [48] CRACKING OF DUPLEX STAINLESS-STEEL DUE TO DISSOLVED HYDROGEN
    HUANG, JH
    ALTSTETTER, CJ
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1995, 26 (05): : 1079 - 1085
  • [49] CHARACTERIZATION OF WELD SOLIDIFICATION CRACKING IN A DUPLEX STAINLESS-STEEL
    VAROL, I
    BAESLACK, WA
    LIPPOLD, JC
    METALLOGRAPHY, 1989, 23 (01): : 1 - 19
  • [50] Cracking Process Related to Hydrogen Behavior in a Duplex Stainless Steel
    Yousefi, Afshin
    Itoh, Goroh
    Ghorani, Zoha
    Kuramoto, Shigeru
    ISIJ INTERNATIONAL, 2019, 59 (12) : 2319 - 2326