Structure and property evolution of LaYbZr2O7/YSZ heterogeneous interface in double-layer thermal barrier coatings after thermal exposure

被引:2
作者
Lu, Yang [1 ]
Sun, Jian [2 ]
Liu, Guanghua [2 ]
Liu, Wei [2 ]
Liu, Xiangyang [1 ]
Pan, Wei [1 ]
Wan, Chunlei [1 ]
机构
[1] Tsinghua Univ, Sch Mat Sci & Engn, State Key Lab New Ceram & Fine Proc, Beijing 100084, Peoples R China
[2] China United Gas Turbine Technol Co Ltd, Beijing, Peoples R China
基金
国家重点研发计划;
关键词
interface stability; LYZO/YSZ; Raman spectrum; thermal barrier coatings; CERAMIC MATERIALS; CONDUCTIVITY; EXPANSION; TOUGHNESS; POROSITY; PROGRESS; DESIGN; YSZ;
D O I
10.1111/jace.19988
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Double-layer thermal barrier coatings are one of the development directions of thermal barrier coatings technology. LaYbZr2O7 (LYZO) has high toughness and low thermal conductivity, making it promising for use as a high-temperature thermal barrier coating. However, its relatively poor mechanical properties, especially low fracture toughness, limit its further application. Therefore, we prepared a double-layer coating of LYZO and Y2O3 partially stabilized ZrO2(YSZ) using atmospheric plasma spraying, with the inner layer being YSZ and the outer layer being LYZO. The results showed that after spraying, LYZO was in the metastable fluorite phase, while YSZ was in the tetragonal phase. LYZO and YSZ had good chemical compatibility, and an interaction layer formed at the interface between them, with its thickness increasing with the sintering time. Eventually, after 100 h of heat treatment, the thickness reached 12 mu m. The hardness of the LYZO/YSZ interface increased with the sintering time, reaching a maximum value after sintering at 1300 degrees C for 10 h. When evaluating the interfacial bonding strength using indentation method, the length of cracks caused by indentation significantly decreased with the increase of sintering time. The increase in bonding strength can be attributed to the formation of a reaction layer and the reduction of thermal residual stresses. Raman spectroscopy was used to measure the thermal residual strain at the LYZO/YSZ interface. Unbalanced distribution of thermal residual stress and M phase was observed near the interface. As the sintering time increased, both thermal residual stress and M phase content decreased. In summary, the double-layer thermal barrier coating of LYZO/YSZ has good potential for development.
引用
收藏
页码:7253 / 7262
页数:10
相关论文
共 50 条
[31]   Microstructures and Properties of Sm2(Zr0.7Ce0.3)2O7/8YSZ Double-Ceramic-Layer Thermal Barrier Coatings Deposited by Atmospheric Plasma Spraying [J].
Huo, Panjie ;
Song, Wenjia ;
Zhou, Xin ;
Zhang, Hao ;
Jiang, Jianing ;
Dong, Shujuan ;
Cao, Xueqiang ;
Dingwell, Donald B. .
JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2019, 28 (05) :986-999
[32]   Design, Preparation, and Characterization of Graded YSZ/La2Zr2O7 Thermal Barrier Coatings [J].
Chen, Hongfei ;
Liu, Yun ;
Gao, Yanfeng ;
Tao, Shunyan ;
Luo, Hongjie .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (06) :1732-1740
[33]   Thermal conductivity and thermal cyclic fatigue of multilayered Gd2Zr2O7/YSZ thermal barrier coatings processed by suspension plasma spray [J].
Mahade, Satyapal ;
Curry, Nicholas ;
Bjorklund, Stefan ;
Markocsan, Nicolaie ;
Nylen, Per .
SURFACE & COATINGS TECHNOLOGY, 2015, 283 :329-336
[34]   Thermal shock performance and failure behavior of Zr6Ta2O17-8YSZ double-ceramic-layer thermal barrier coatings prepared by atmospheric plasma spraying [J].
Liu, Q. ;
Hu, X. P. ;
Zhu, W. ;
Liu, G. L. ;
Guo, J. W. ;
Bin, J. .
CERAMICS INTERNATIONAL, 2022, 48 (17) :24402-24410
[35]   Composition, mechanical properties and thermal cycling performance of YSZ toughened La2Ce2O7 composite thermal barrier coatings [J].
Zhang, Hao ;
Yuan, Jieyan ;
Song, Wenjia ;
Zhou, Xin ;
Dong, Shujuan ;
Duo, Shuwang ;
Wang, Jinshuang ;
Yang, Xiong ;
Jiang, Jianing ;
Deng, Longhui ;
Huang, Jingqi ;
Cao, Xueqiang .
CERAMICS INTERNATIONAL, 2020, 46 (05) :6641-6651
[36]   Effects of Er stabilization on thermal property and failure behavior of Gd2Zr2O7 thermal barrier coatings [J].
Shen, Zaoyu ;
Liu, Guanxi ;
Mu, Rende ;
He, Limin ;
Xu, Zhenhua ;
Dai, Jianwei .
CORROSION SCIENCE, 2021, 185
[37]   Effects of europium doping on thermal property and failure behaviour of Gd2Zr2O7 thermal barrier coatings [J].
Shen, Zaoyu ;
Luo, Yuqing ;
Liu, Guanxi ;
Dai, Jianwei ;
He, Limin ;
Mu, Rende .
NPJ MATERIALS DEGRADATION, 2025, 9 (01)
[38]   Microstructural evolution and hot corrosion behavior of La0.8Ba0.2TiO3-δ-YSZ double-layer thermal barrier coatings in Na2SO4 + V2O5 molten salt at 900 °C [J].
Fang, Yongchao ;
Cui, Xiufang ;
Jin, Guo ;
Liu, Erbao ;
Zhang, Dan ;
Wen, Xin ;
Mi, Qingbo .
SURFACE & COATINGS TECHNOLOGY, 2020, 399
[39]   The enhanced thermal shock resistance performance induced by interface effect in blade-level La2Ce2O7/YSZ thermal barrier coating [J].
Yan, Gang ;
Sun, Yu ;
Zhao, Xianli ;
Liu, Wei ;
Wang, Qianwen ;
Li, Cong ;
Yang, Li ;
Zhou, Yichun .
APPLIED SURFACE SCIENCE, 2023, 619
[40]   Failure analysis of Gd2Zr2O7/YSZ multi-layered thermal barrier coatings subjected to thermal cyclic fatigue [J].
Mahade, Satyapal ;
Curry, Nicholas ;
Bjorklund, Stefan ;
Markocsan, Nicolaie ;
Nylen, Per .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 689 :1011-1019