Novel Ti3SiC2-(Ti, Zr)B2 toughened (Ti, Zr)C-based composites with enhanced mechanical properties fabricated by dual in situ reactions hot-pressing at low temperature
被引:1
作者:
Wang, Liwei
[1
]
Wei, Boxin
[1
,2
]
Yao, Jia
[1
]
Wang, Dong
[3
]
Chen, Lei
[4
,5
]
Wang, Yujin
[4
,5
]
机构:
[1] Harbin Univ Sci & Technol, Sch Mat Sci & Chem Engn, Harbin 150040, Peoples R China
[2] Harbin Univ Sci & Technol, Heilongjiang Prov Key Lab Light Met Mat Modificat, Harbin 150040, Peoples R China
[3] Anhui Univ Technol, Sch Mat Sci & Engn, Maanshan 243002, Peoples R China
[4] Harbin Inst Technol, Inst Adv Ceram, Sch Mat Sci & Engn, Harbin 150080, Peoples R China
[5] Harbin Inst Technol, Key Lab Adv Struct Funct Integrat Mat & Green Mfg, Harbin 150001, Peoples R China
来源:
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T
|
2024年
/
30卷
基金:
中国国家自然科学基金;
关键词:
(Ti;
Zr)C-based composites;
In situ reactions;
Microstructure;
Mechanical properties;
MICROSTRUCTURE;
ZRC;
DENSIFICATION;
BEHAVIOR;
PHASE;
PARAMETERS;
CERAMICS;
CERMETS;
NI;
D O I:
10.1016/j.jmrt.2024.05.226
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
The fully dense Ti 3 SiC 2 -(Ti, Zr)B 2 toughened (Ti, Zr)C-based composites were fabricated at 1400-1600 degrees C for the first time by dual in situ reactions hot -pressing with TiC, ZrB 2 , and Si as the initial powders. The influence of ZrB 2 , Si content and sintering temperature on the microstructure and mechanical properties of the composite was reported. When 10 mol% ZrB 2 was added, Si combined with residual TiC to form Ti 3 SiC 2 and SiC. However, with the addition of ZrB 2 increase to 20 mol% and 30 mol%, Si participated in the formation of ZrSi and was not enough to react with TiC to form Ti 3 SiC 2 . The low -temperature in situ reactions, multiphase coupling effects, and the pinning effect of nano-SiC refine the microstructure of the composites. There are specific crystal orientation relationships between (Zr, Ti)C and (Ti, Zr)B 2 , as well as between (Ti, Zr)C and SiC. The layered Ti 3 SiC 2 and plate -like (Ti, Zr)B 2 by dual in situ reactions effectively improve the fracture toughness of the composites. The 10 ZB-15 possesses a highest fracture toughness of 6.1 MPa center dot m 1/2 . The 30 ZB-16 has the good comprehensive mechanical properties. The fracture toughness, flexural strength, and hardness of 30 ZB-16 is 5.6 MPa center dot m 1/2 , 679 MPa, and 26.4 GPa, respectively. The Ti 3 SiC 2 and TiB 2 formed during dual in situ reactions enables the composite to exhibit excellent oxidation resistance and wear resistance.
引用
收藏
页码:8822 / 8840