Microwave absorber utilization to improve grinding and particle surface structure characteristics of torrefied switchgrass particles for bioenergy applications

被引:1
|
作者
Agu, Obiora S. [1 ]
Tabil, Lope G. [1 ]
Mupondwa, Edmund [1 ,2 ]
Emadi, Bagher [1 ]
机构
[1] Univ Saskatchewan, Dept Chem & Biol Engn, 57 Campus Dr, Saskatoon, SK S7N 5A9, Canada
[2] Agr & Agri Food Canada, Govt Canada, Saskatoon Res & Dev Ctr, Bioprod & Bioproc Sci & Technol Branch, 107 Sci Pl, Saskatoon, SK S7N 0X2, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Torrefaction; Switchgrass; Specific grinding energy; Fluorescence; Microwave absorber; BIOMASS; TORREFACTION; PYROLYSIS; BIOCHAR; QUALITY; PRETREATMENT; STRAWS; WHEAT; FUEL;
D O I
10.1016/j.heliyon.2024.e32423
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Torrefaction treatment improves biomass grindability by transforming the fibrous herbaceous to a more brittle and lighter coal-like material. Microwave-assisted torrefaction is a promising technology for biomass conversion into energy, fuels, and chemicals. The study applied microwave absorbers in the torrefaction process to improve the thermochemical characteristics and grindability of switchgrass. Switchgrass in two particle sizes was torrefied in a microwave reactor with biochar added as a microwave absorber under inert conditions. After torrefaction, the geometric mean particle and size distribution and selected physical characteristics were evaluated, and the grindability of the torrefied ground and chopped with and without biochar were compared with those of untreated switchgrass. The geometric diameter results decreased, and the specific energy required for grinding torrefied switchgrass with biochar was significantly reduced with extended residence times and at a torrefaction temperature of 300 degrees C. After grinding, the lowest grinding energy of 32.82 kJ at 300 degrees C/20 min was recorded with torrefied ground switchgrass/biochar. The 10% biochar added/250 degrees C resulted in deep cell wall disarrangement, whereas at a torrefaction temperature of 300 degrees C, large surface deformation and carbonized weight fractions were observed.