Long-term properties evolution and life prediction of glass fiber reinforced thermoplastic bending bars exposed in concrete alkaline environment

被引:35
作者
Xian, Guijun [1 ,2 ,3 ]
Bai, Yanbo [1 ,2 ,3 ]
Zhou, Ping [1 ,2 ,3 ]
Wang, Junqi [1 ,2 ,3 ]
Li, Chenggao [1 ,2 ,3 ,4 ]
Dong, Shaoce [1 ,2 ,3 ]
Guo, Rui [1 ,2 ,3 ]
Tian, Jingwei [1 ,2 ,3 ]
Li, Jinhao [1 ,2 ,3 ]
Zhong, Jian [1 ,2 ,3 ]
He, Taipeng [1 ,2 ,3 ]
Zhang, Zhuo [1 ,2 ,3 ]
机构
[1] Harbin Inst Technol, Minist Educ, Key Lab Struct Dynam Behav & Control, Harbin 150090, Heilongjiang, Peoples R China
[2] Harbin Inst Technol, Key Lab Smart Prevent Mitigat Civil Engn Disasters, Minist Ind & Informat Technol, Harbin 150090, Peoples R China
[3] Harbin Inst Technol, Sch Civil Engn, Harbin 150090, Heilongjiang, Peoples R China
[4] 73 Huanghe Rd, Harbin 150090, Peoples R China
来源
JOURNAL OF BUILDING ENGINEERING | 2024年 / 91卷
关键词
Glass fiber reinforced polypropylene bending bars; Alkaline solution immersion; Mechanical properties; Microscopic analysis; Degradation mechanism; Prediction of service life; COMPOSITES; DURABILITY;
D O I
10.1016/j.jobe.2024.109641
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Glass fiber reinforced polypropylene (GFRPP) bending bars have many advantages, such as high toughness, high durability, repeated molding and recycling, which can be used in concrete structures to replace steel stirrup for solving the problems of corrosion and service life. However, the changes in the properties of GFRPP bending bars during long-term use in alkaline concrete environments require further investigation. In the present study, GFRPP bending bars were immersed in alkaline solution at 20 degrees C, 40 degrees C, and 60 degrees C for as long as 180 d. The water absorption, hydrolysis, mechanical properties, and microscopic properties of the bending bars were evaluated to understand the long-term performance and mechanism of degradation. The bending bars had a higher saturated water absorption percentage and time along with a lower diffusion rate than the straight bars due to the presence of pores and micro-cracks formed during the bending process. The dissolution of the glass fibers in alkaline solution led to the partial mass loss of the GFRPP bars. Compared to the control, the tensile strength retention of the bending bars was 20.6%-56.0 %. The tensile failure mode changed from fiber bursting before immersion to shear fracture after immersion due to the decreased interfacial bonding strength and increased glass fiber brittleness. The primary degradation mechanisms were the etching of glass fibers, interface debonding, and increased void volume (similar to 23.7 %). The bending bars were more seriously eroded than the straight bars due to the twisting of the fibers and imperfect interfaces. The predicted degradation times of the GFRPP bending bars ranged from 1.7 years (Haikou) to 3.9 years (Harbin), corresponding to a stable tensile strength retention of 22.13 %. The results provide a basis for evaluating the durability and service life of GFRPP bending bars and promote the application of GFRPP composite stirrups in concrete structures.
引用
收藏
页数:19
相关论文
共 52 条
[31]   Bending characterisation of a molten unidirectional carbon fibre reinforced thermoplastic composite using a Dynamic Mechanical Analysis system [J].
Margossian, A. ;
Bel, S. ;
Hinterhoelzl, R. .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2015, 77 :154-163
[32]   HYDROTHERMAL AGING OF CSM-LAMINATE DURING WATER IMMERSION - AN ACOUSTOULTRASONIC STUDY [J].
PHANI, KK ;
BOSE, NR .
JOURNAL OF MATERIALS SCIENCE, 1986, 21 (10) :3633-3637
[33]   Marine Application of Fiber Reinforced Composites: A Review [J].
Rubino, Felice ;
Nistico, Antonio ;
Tucci, Fausto ;
Carlone, Pierpaolo .
JOURNAL OF MARINE SCIENCE AND ENGINEERING, 2020, 8 (01)
[34]   Viscoelastic bending model for continuous fiber-reinforced thermoplastic composites in melt [J].
Sachs, U. ;
Akkerman, R. .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2017, 100 :333-341
[35]   Effects of hydrothermal aging on moisture absorption and property prediction of short carbon fiber reinforced polyamide 6 composites [J].
Sang, Lin ;
Wang, Chuo ;
Wang, Yingying ;
Hou, Wenbin .
COMPOSITES PART B-ENGINEERING, 2018, 153 :306-314
[36]   Synthesis and Mechanical Properties of Natural Fiber Reinforced Epoxy/Polyester/Polypropylene Composites: A Review [J].
Sathishkumar, G. K. ;
Ibrahim, Mohamed ;
Akheel, M. Mohamed ;
Rajkumar, G. ;
Gopinath, B. ;
Karpagam, R. ;
Karthik, P. ;
Charles, M. Martin ;
Gautham, G. ;
Shankar, G. Gown .
JOURNAL OF NATURAL FIBERS, 2022, 19 (10) :3718-3741
[37]  
Shenoi RA, 2011, COMPOSITE MATERIALS: A VISION FOR THE FUTURE, P69, DOI 10.1007/978-0-85729-166-0_3
[38]   Environmental durability of flax fibres and their composites based on polypropylene matrix [J].
Stamboulis, A ;
Baillie, CA ;
Garkhail, SK ;
van Melick, HGH ;
Peijs, T .
APPLIED COMPOSITE MATERIALS, 2000, 7 (5-6) :273-294
[39]   Additive manufacturing of PEEK-based continuous fiber reinforced thermoplastic composites with high mechanical properties [J].
Vatandas, Bahri Baris ;
Usun, Altug ;
Yildiz, Nuri ;
Simsek, Cemaleddin ;
Cora, Omer Necati ;
Aslan, Mustafa ;
Gumruk, Recep .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2023, 167
[40]  
Wang C., 2010, J. Disaster Prev. Mitig. Eng., V30, P373