A Study of Directionality Effects in Three-Beam Coaxial Titanium Wire-Based Laser Metal Deposition

被引:0
作者
Mathenia, Remy [1 ]
McLain, Braden [1 ]
Sparks, Todd [2 ]
Liou, Frank [1 ]
机构
[1] Missouri Univ Sci & Technol, Dept Mech & Aerosp Engn, Rolla, MO 65409 USA
[2] Prod Innovat & Engn, St James, MO 65559 USA
关键词
three-beam coaxial laser; wire deposition; bead geometry; defocusing;
D O I
10.3390/ma17133201
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Coaxial wire-based laser metal deposition is a versatile and efficient additive process that can achieve a high deposition rate in the manufacturing of complex structures. In this paper, a three-beam coaxial wire system is studied, with particular attention given to the effects of the deposition direction and laser beam orientation on the resulting bead geometry symmetry. With the three-beam laser delivery, the laser spot pattern is not always symmetric with respect to the deposition direction. Single titanium beads are deposited in different directions and at varying deposition rates, and the bead profile is quantitatively scored for multiple symmetry measures. Through an analysis of variance, the deposition direction and deposition rate were found to be insignificant with respect to the resulting bead symmetry for the developed measures. The bead symmetry and geometry are important factors in determining if a build is free of critical defects, and in this study, it is shown that the three-beam coaxial wire deposition setup is a directionally independent process.
引用
收藏
页数:15
相关论文
共 26 条
  • [1] Laser metal deposition technique: sustainability and environmental impact
    Abdulrahman, Kamardeen O.
    Akinlabi, Esther T.
    Mahamood, Rasheedat M.
    [J]. 15TH GLOBAL CONFERENCE ON SUSTAINABLE MANUFACTURING, 2018, 21 : 109 - 116
  • [2] State of the Art in Directed Energy Deposition: From Additive Manufacturing to Materials Design
    Dass, Adrita
    Moridi, Atieh
    [J]. COATINGS, 2019, 9 (07):
  • [3] Wire-feed additive manufacturing of metal components: technologies, developments and future interests
    Ding, Donghong
    Pan, Zengxi
    Cuiuri, Dominic
    Li, Huijun
    [J]. INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2015, 81 (1-4) : 465 - 481
  • [4] Influence of Build Orientation, Chamber Temperature and Infill Pattern on Mechanical Properties of 316L Parts Manufactured by Bound Metal Deposition
    Gabilondo, Maitane
    Cearsolo, Xabier
    Arrue, Mario
    Castro, Francisco
    [J]. MATERIALS, 2022, 15 (03)
  • [5] Annular laser beam based direct metal deposition
    Govekar, Edvard
    Jeromen, Andrej
    Kuznetsov, Alexander
    Kotar, Matjaz
    Kondo, Masaki
    [J]. 10TH CIRP CONFERENCE ON PHOTONIC TECHNOLOGIES [LANE 2018], 2018, 74 : 222 - 227
  • [6] ipt, Wire-Based Laser Metal Deposition (LMD-w)
  • [7] Effects of Defocus Distance on Three-Beam Laser Internal Coaxial Wire Cladding
    Ji, Shaoshan
    Liu, Fan
    Shi, Tuo
    Fu, Geyan
    Shi, Shihong
    [J]. CHINESE JOURNAL OF MECHANICAL ENGINEERING, 2021, 34 (01)
  • [8] Advances in the understanding of the annular laser beam wire cladding process
    Kotar, Matjaz
    Fujishima, Makoto
    Levy, Gideon N.
    Govekar, Edvard
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2021, 294
  • [9] Initial transient phase and stability of annular laser beam direct wire deposition
    Kotar, Matjaz
    Fujishima, Makoto
    Levy, Gideon
    Govekar, Edvard
    [J]. CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2019, 68 (01) : 233 - 236
  • [10] The influence of the workpiece illumination proportion in annular laser beam wire deposition process
    Kotar, Matjaz
    Govekar, Edvard
    [J]. 10TH CIRP CONFERENCE ON PHOTONIC TECHNOLOGIES [LANE 2018], 2018, 74 : 228 - 232