Impact of zinc concentration and annealing temperature on the structural, optical, and photoelectrochemical properties of nickel oxide thin films synthesized by electrodeposition method

被引:0
作者
Ismail, Walid [1 ]
Samir, Sanya [1 ]
Habib, Mohamed. A. [2 ,3 ]
El-Shaer, Abdelhamid [1 ]
机构
[1] Kafrelsheikh Univ, Fac Sci, Phys Dept, Kafrelsheikh 33516, Egypt
[2] Imam Mohammad Ibn Saud Islamic Univ IMSIU, Coll Sci, Dept Chem, Riyadh 11623, Saudi Arabia
[3] Natl Res Ctr, Chem Ind Inst, Chem Tanning Mat & Leather Technol Dept, PO 12622, Giza, Egypt
关键词
Nickel Oxide; Thin films; Zinc doping; Electrodeposition; PL; Optoelectronic applications; NANOSTRUCTURED NIO; PHYSICAL-PROPERTIES; DEPOSITION; NANOPARTICLES;
D O I
10.1016/j.jallcom.2024.175343
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, Zinc (Zn)- doped nickel oxide (NiO) thin films were fabricated via the electrodeposition method. The synthesized films were created with different concentrations of Zn (2 %, 4 %, 6 %, and 8 %) after that annealed at two different temperatures (300 degrees C and 500 degrees C). The prepared samples were analyzed using X-ray diffraction (XRD), scanning electron microscopy (SEM), Raman spectroscopy (RAM), UV-vis spectrophotometry, photocurrent (PC), photoluminescence (PL), electrochemical impedance spectroscopy (EIS), Energy-Dispersive X-ray spectroscopy (EDX), photocurrent (PC), and Mott-Schottky (MS) analysis. XRD patterns indicate that Zn: NiO thin films have a cubic phase, with the (111) direction as the preferred orientation. Various structural parameters such as dislocation density, stacking fault, lattice strain, and crystallite size have been determined. The presence of Zn doping in NiO has been confirmed by EDX analysis. The EDX mapping of elements revealed the uniform distribution of Ni, Zn, and O in the sample. The optical transmittance and absorbance were analyzed using a UV-vis spectrophotometer. The lowest transmittance values were found for 8 % Zn: NiO thin films annealed at 300 degrees C and 500 degrees C. The absorption edge corresponding to pure NiO-300 degrees C and NiO-500 degrees C has been observed at 300 and 320 nm, respectively. The band gap energy (Eg) decreased to 3.88 eV for 8 %Zn: NiO (300 degrees C) and 3.71 eV for 8 %Zn: NiO (500 degrees C). The Raman analysis showed three distinct peaks at 590 cm-1, 705 cm-1, and 1172 cm-1, which correspond to the vibration of Ni-O bonds. The SEM results indicated that increasing the doping concentration and annealing temperature resulted in larger grain sizes in the manufactured samples. Furthermore, the PL spectra analysis of the synthesized films revealed two distinct emission peaks at around 400 and 490 nm. PC analysis confirmed the p-type conductivity of manufactured arrays. From MS measurements, the highest carrier concentration (NA) values of 8.81x1018 cm-3 and 9.41x1019 cm-3 were obtained for 8 %Zn: NiO (300 degrees C) and 8 %Zn: NiO (500 degrees C), respectively. EIS analysis confirmed the highest conductivity and enhanced electrochemical activity for 6 % Zn: NiO (500 degrees C) and 8 % Zn: NiO (300 degrees C). These results suggest that Zn-doped NiO is suitable for optoelectronic applications.
引用
收藏
页数:12
相关论文
共 50 条
[31]   Annealing Temperature Dependent Structural and Optical Properties of RF Sputtered ZnO Thin Films [J].
Sharma, Shashikant ;
Varma, Tarun ;
Asokan, K. ;
Periasamy, C. ;
Boolchandani, Dharmendar .
JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2017, 17 (01) :300-305
[32]   The effect of copper doping on the structural, optical, and electrical properties of nickel oxide thin films for optoelectronic applications [J].
Mohammed, Ban K. ;
Mohammed, Mustafa K. A. ;
Ahmed, Duha S. .
JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 2021, 99 (01) :1-12
[33]   Effect of Al dopant concentration on structural, optical and photoconducting properties in nanostructured zinc oxide thin films [J].
Ganesh, T. ;
Rajesh, S. ;
Xavier, Francis P. .
MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING, 2013, 16 (02) :295-302
[34]   The effect of annealing temperature on the structural, optical, and electrical properties of CdS films [J].
Metin, Hulya ;
Ari, Mehmet ;
Erat, Selma ;
Durmus, Semra ;
Bozoklu, Mehmet ;
Braun, Artur .
JOURNAL OF MATERIALS RESEARCH, 2010, 25 (01) :189-196
[35]   Effect of annealing on microstructural, compositional, optical, and photoelectrochemical properties of CdSe thin films [J].
Thanikaikarasan, Sethuramachandran .
IONICS, 2018, 24 (05) :1529-1536
[36]   Effect of annealing on microstructural, compositional, optical, and photoelectrochemical properties of CdSe thin films [J].
Sethuramachandran Thanikaikarasan .
Ionics, 2018, 24 :1529-1536
[37]   Impact of annealing temperature on structural, optical, and morphological properties of zno nanoparticles synthesized by a simple precipitation method [J].
Deshmukh L.D. ;
Chavan K.B. .
Nanoscience and Nanotechnology - Asia, 2021, 11 (02) :204-210
[38]   Annealing temperature dependent on structural, optical and electrical properties of indium oxide thin films deposited by electron beam evaporation method [J].
Senthilkumar, V. ;
Vickraman, P. .
CURRENT APPLIED PHYSICS, 2010, 10 (03) :880-885
[39]   Effect of concentration on the properties of nitrogen-doped zinc oxide thin films grown by electrodeposition [J].
K. A. Musiliyu ;
E. D. Ogunmola ;
A. A. Ajayi ;
O. W. Abodunrin .
Materials for Renewable and Sustainable Energy, 2023, 12 :23-29
[40]   Effect of annealing temperature on structural, optical and electrical properties of hydrothermal assisted zinc oxide nanorods [J].
Narayanan, Guru Nisha ;
Ganesh, R. Sankar ;
Karthigeyan, A. .
THIN SOLID FILMS, 2016, 598 :39-45