Corrosion resistance and microstructural evolution of Yb-Al-Si-O glass-ceramics under molten Ca-Mg-Al-Si environment at 1350 ° C

被引:0
|
作者
Meng, Xinyu [1 ]
Ma, Yujie [1 ]
Guo, Chun [1 ]
Chen, Bo [1 ]
Yang, Shaobo [1 ]
Deng, Juanli [2 ]
Fan, Shangwu [1 ]
机构
[1] Northwestern Polytech Univ, Sci & Technol Thermostruct Composites Mat Lab, Xian 710072, Shaanxi, Peoples R China
[2] Changan Univ, Sch Mat Sci & Engn, Xian 710064, Shaanxi, Peoples R China
关键词
Yb-Al-Si-O; Glass-ceramics; CMAS corrosion; Crystallization; RARE-EARTH DISILICATES; BARRIER COATINGS; WATER-VAPOR; MATRIX COMPOSITES; OXIDATION; BEHAVIOR; SILICA;
D O I
10.1016/j.jeurceramsoc.2024.05.043
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The intrinsic characteristics of Yb 2 O 3 -Al 2 O 3 -SiO 2 (YbAS) glass-ceramics and their resistance to corrosion by molten calcium magnesium aluminosilicate (CMAS) at 1350 degrees C were systematically investigated. YbAS glassceramics, characterized by diverse compositions, maintaining phase stability over extended durations at elevated temperatures. After CMAS corrosion for 50 h, the main reaction phases were CaAl 2 Si 2 O 8 and Ca 2 Yb 8 (SiO 4 ) 6 O 2 , accompanied by multiple ion solid solution garnet in certain components. The glass component positioned along the eutectic line of Yb 2 Si 2 O 7 and mullite, with an OB value marginally exceeding that of CMAS, exhibits superior corrosion resistance to CMAS. This finding offers valuable insights for the subsequent design of environmental barrier coatings (EBCs).
引用
收藏
页码:7891 / 7903
页数:13
相关论文
共 47 条
  • [41] Optimizing damage resistance and structural evolution in CaO-modified Li2O-Al2O3-B2O3-TiO2-P2O5 glass-ceramics
    Hu, Sijia
    Zhou, Kun
    Huang, Zuzhi
    Zhang, Hao
    Xie, Hailei
    He, Feng
    Duo, Shuwang
    Shi, Jiang
    CERAMICS INTERNATIONAL, 2024, 50 (23) : 50635 - 50647
  • [42] The effect of Al2O3 on the high-temperature oxidation resistance of Si-B-C ceramic under air atmosphere
    Shan, Qingliang
    Hu, Jianbao
    Kan, Yanmei
    Ni, Dewei
    Gao, Le
    Chen, Xiaowu
    Dong, Shaoming
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2018, 15 (05) : 1146 - 1156
  • [43] Mineral-phase evolution and sintering behavior of MO-SiO2-Al2O3-B2O3 (M = Ca, Ba) glass-ceramics by low-temperature liquid-phase sintering
    Chen, Song
    Sun, Zhen
    Zhu, De-gui
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2018, 25 (09) : 1042 - 1054
  • [44] Microstructural Evolution and Mechanical Properties of Semi-Solid Al15Mg45Li39Ca0.5Si0.5 Light-Weight High Entropy Alloys Fabricated by Isothermal Heat Treatment
    Hu, Yong
    Liu, Fei
    Zhao, Longzhi
    Tang, Yanchuan
    Jiao, Haitao
    METALS AND MATERIALS INTERNATIONAL, 2023, 29 (05) : 1489 - 1497
  • [45] Mineral-phase evolution and sintering behavior of MO–SiO2–Al2O3–B2O3 (M = Ca, Ba) glass-ceramics by low-temperature liquid-phase sintering
    Song Chen
    Zhen Sun
    De-gui Zhu
    International Journal of Minerals, Metallurgy, and Materials, 2018, 25 : 1042 - 1054
  • [46] Mineral-phase evolution and sintering behavior of MO–SiO2–Al2O3–B2O3 (M = Ca,Ba) glass-ceramics by low-temperature liquid-phase sintering
    Song Chen
    Zhen Sun
    De-gui Zhu
    InternationalJournalofMineralsMetallurgyandMaterials, 2018, 25 (09) : 1042 - 1054
  • [47] Effects of alkali/alkaline-earth ions on the preparation, crystallization behavior and photocatalytic activity of R2O/MO-ZnO-Al2O3-TiO2-P2O5 (R=Li, Na, K; M=Mg, Ca, Sr) glass and glass-ceramics
    Liu, Xinzhu
    Luo, Zhiwei
    Tong, Juxia
    Liu, Xinyu
    Liang, Haozhang
    Wang, Yiren
    Lu, Anxian
    CERAMICS INTERNATIONAL, 2024, 50 (22) : 47118 - 47127