Understanding the deterioration of hydration products in alkali-activated slag/Portland cement exposure to sulfate attack

被引:1
|
作者
Jia, Zijian [1 ]
Cao, Ruilin [2 ]
Xiong, Yuanliang [3 ]
Zhang, Shunquan [4 ]
Jia, Lutao [1 ]
Zhang, Yamei [1 ]
Gao, Yueyi [5 ]
机构
[1] Southeast Univ, Sch Mat Sci & Engn, Jiangsu Key Lab Construct Mat, Nanjing 211189, Peoples R China
[2] Nanjing Tech Univ, Coll Mat Sci & Engn, Nanjing 211816, Peoples R China
[3] Yantai Univ, Sch Civil Engn, Yantai 264005, Peoples R China
[4] Anhui Univ Technol, Sch Civil Engn & Architecture, Maanshan 243002, Peoples R China
[5] Jiangsu Acad Safety Sci & Technol, Nanjing, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
Portland cement; Alkali-activated slag; Sulfate attack; Hydration products; In-situ observation; C-S-H; PART II; SLAG; MAGNESIUM; CONCRETE; PASTE; DEGRADATION; TEMPERATURE; RESISTANCE; MORTARS;
D O I
10.1016/j.jobe.2024.110292
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The deterioration of different phases under sulfate attack is a critical durability problem for cementitious materials. Alkali-activated slag (AAS) is a kind of low carbon footprint cementitious material, whose hydration products are quite different from that of Portland cement (PC). The specific variations in the behavior of different hydration products under sulfate attack in PC and AAS have not been comprehensively explored. In this paper, a combination of BSE and EDS techniques was applied to investigate the change of various hydration products in PC and AAS before and after exposure to sulfate solutions. The results indicate that the unhydrated slag in AAS is more stable than the unhydrated C2S and C3S in PC paste after exposure to deionized water and sulfate solutions, and obvious substitution of Ca by Mg can be found for C2S and C3S after exposure to MgSO4 solution. In PC sample, the Ca/Si reduction of outer product after deterioration in different solutions is less significant than that of inner product, mainly due to the existing of Ca rich phases intermixed in Op. While in AAS, the change of Ca/Si in dark rims in different solutions is consistent with that of C-A-S-H presented in the matrix. After exposure to sulfate solutions, no significant sulfate rich area can be observed for AAS, which should mainly be attributed to the relatively slower formation of gypsum in AAS due to the absence of highly soluble calciumrich phases like portlandite in PC.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Influence of slag composition on the hydration of alkali-activated slags
    Winnefeld, Frank
    Ben Haha, Mohsen
    Le Saout, Gwenn
    Costoya, Mercedes
    Ko, Suz-Chung
    Lothenbach, Barbara
    JOURNAL OF SUSTAINABLE CEMENT-BASED MATERIALS, 2015, 4 (02) : 85 - 100
  • [42] KINETIC-STUDY ON HYDRATION OF ALKALI-ACTIVATED SLAG
    ZHOU, HH
    WU, XQ
    XU, ZZ
    TANG, MH
    CEMENT AND CONCRETE RESEARCH, 1993, 23 (06) : 1253 - 1258
  • [43] Individual and combined effects Of Portland cement-based hydrated mortar components on alkali-activated slag cement
    Rakhimova, N. R.
    Rakhimov, R. Z.
    CONSTRUCTION AND BUILDING MATERIALS, 2014, 73 : 515 - 522
  • [44] The role of sodium during the hydration of alkali-activated slag
    Wang, SD
    ADVANCES IN CEMENT RESEARCH, 2000, 12 (02) : 65 - 69
  • [45] Advances in Understanding the Alkali-Activated Metallurgical Slag
    Liu, Kuisheng
    Zhang, Zengqi
    Sun, Jianwei
    ADVANCES IN CIVIL ENGINEERING, 2021, 2021
  • [46] The hydration of slag, part 1: reaction models for alkali-activated slag
    W. Chen
    H. J. H. Brouwers
    Journal of Materials Science, 2007, 42 : 428 - 443
  • [47] The hydration of slag, part 1: reaction models for alkali-activated slag
    Chen, W.
    Brouwers, H. J. H.
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (02) : 428 - 443
  • [48] MAGNESIUM SULPHATE ATTACK ON ALKALI-ACTIVATED SLAG MORTAR
    Allahverdi, Ali
    Hashemi, Hamideh
    NON-TRADITIONAL CEMENT & CONCRETE IV, 2011, : 590 - 598
  • [49] SODIUM SULPHATE ATTACK ON ALKALI-ACTIVATED SLAG MORTAR
    Allahverdi, Ali
    Hashemi, Hamideh
    NON-TRADITIONAL CEMENT & CONCRETE IV, 2011, : 581 - 589
  • [50] Resistance of alkali-activated slag concrete to acid attack
    Bakharev, T
    Sanjayan, JG
    Cheng, YB
    CEMENT AND CONCRETE RESEARCH, 2003, 33 (10) : 1607 - 1611