Effect of sodium gluconate addition on anomalous codeposition of electroplated nickel-iron alloys

被引:1
|
作者
Ma, Ju-Lung [1 ]
Chen, Hou-Jen [1 ]
Chung, Kai-Cheng [2 ]
Wu, Yung -Fu [2 ]
Yen, Chia-Ying [3 ]
Li, Wen Jin [3 ]
Lin, Hsin-Chih [1 ]
机构
[1] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei 10617, Taiwan
[2] Ming Chi Univ Technol, Dept Chem Engn, New Taipei City 24301, Taiwan
[3] Ind Technol Res Inst, Mat & Chem Res Labs, Hsinchu 301401, Taiwan
关键词
Invar; Sodium gluconate; Anomalous codeposition; Selectivity ratio; Plastic deformation; BORIC-ACID; MECHANICAL-PROPERTIES; NI; ELECTRODEPOSITION; FE;
D O I
10.1016/j.tsf.2024.140292
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Invar nickel -iron alloy has been widely applied in the fields of electronics, sensors, communications and optics, due to its low thermal expansion coefficient, high hardness, high ductility and other characteristics according to product requirements. The application in metal stencil during the manufacturing process of active -matrix organic light -emitting diodes is mainly due to their good electrical conductivity and soft magnetic properties. In this study, sodium gluconate is used as a substitute for boric acid in the acidic electroplating of nickel -iron alloys; the concentration ratio of nickel -iron in the plating bath is 2:1. After adding sodium gluconate, the precipitation of nickel varies significantly. The iron content in the weight percentage of the deposited nickel -iron alloy is obviously larger than nickel, even up to 3 times. The whole deposition process is in the state of anomalous codeposition, and the selectivity ratio reaches 3 or more; the nickel -iron alloy deposited by adding sodium gluconate to the plating bath has a great influence on the material properties of the nickel -iron alloy plating, The nickel -iron alloy deposited at -1.4 V exhibits a hardness of approximately 3.17 GPa and a modulus of elasticity about 37.88 GPa. Notably, the resistance to plastic deformation of the alloy deposited in sodium gluconate plating solution (H 3 /U 2 =0.022) is significantly higher than that in boric acid plating solution (H 3 /U 2 =0.007). The experimental results also show that it has the best ability to resist plastic deformation.
引用
收藏
页数:7
相关论文
共 38 条
  • [31] Synergistic Effect of Mo and V Addition on Al-Si Alloys Containing High Iron Impurity
    Kishor, Modalavalasa
    Ram, Karri Yaswin Phani
    Rao, A. K. Prasada
    Nahid, Shaik Ansar Ghousiya
    Ramavajjala, Anil Kumar
    INTERNATIONAL JOURNAL OF METALCASTING, 2024, 18 (04) : 3538 - 3548
  • [32] A multiscale approach to study the effect of chromium and nickel concentration in the hardening of iron alloys
    Mastorakos, I. N.
    Zbib, H. M.
    JOURNAL OF NUCLEAR MATERIALS, 2014, 449 (1-3) : 101 - 110
  • [33] Effect of iron addition on the microstructures and properties of hypereutectic Al-20%Si alloys
    Li, Qinglin
    Zhu, Yuqian
    Li, Binqiang
    Ding, Wanwu
    Lan, Yefeng
    Xia, Tiandong
    Du, Qianbiao
    MATERIALS RESEARCH EXPRESS, 2019, 6 (01):
  • [34] Macroscopic Size Effect in the Composition and Properties of Alloys of Iron Group Metals with Tungsten Prepared by Induced Codeposition: Alloy Deposition Mechanism and Its Implications
    Dikusar, A. I.
    Belevskii, S. S.
    SURFACE ENGINEERING AND APPLIED ELECTROCHEMISTRY, 2023, 59 (06) : 699 - 711
  • [35] Effect of iron addition on Co-29Cr-6Mo alloys for biomedical applications
    Lee, Sang-Hak
    Chiba, Hisae
    Syuto, Bunei
    Nomura, Naoyuki
    Chiba, Akihiko
    PRICM 6: SIXTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-3, 2007, 561-565 : 1497 - +
  • [36] Macroscopic Size Effect in the Composition and Properties of Alloys of Iron Group Metals with Tungsten Prepared by Induced Codeposition: Alloy Deposition Mechanism and Its Implications
    A. I. Dikusar
    S. S. Belevskii
    Surface Engineering and Applied Electrochemistry, 2023, 59 : 699 - 711
  • [37] The Effect of Niobium Addition on the Microstructure and Tensile Properties of Iron-Nickel Base A286 Superalloy
    Gilakjani, Reza Soleimani
    Razavi, Seyed Hossein
    Seifollahi, Masoumeh
    IRANIAN JOURNAL OF MATERIALS SCIENCE AND ENGINEERING, 2021, 18 (01) : 61 - 70
  • [38] Effect of Deposition Current Density and Annealing Temperature on the Microstructure, Hardness and Magnetic Properties of Nanostructured Nickel-Iron-Tungsten Alloys
    Spasojevic, M.
    Cirovic, N.
    Ribic-Zelenovic, L.
    Spasojevic, P.
    Maricic, A.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2014, 161 (10) : D463 - D469