Indentation Behavior Assessment of As-Built, Solution, and Artificial Aged Heat-Treated Selective Laser Melting Specimens of AlSi10Mg

被引:0
|
作者
Kamil, Abubakr Shahnawaz [1 ]
Muzamil, Muhammad [1 ]
Akhtar, Maaz [2 ]
Alsaleh, Naser [2 ]
Khan, Rashid [2 ]
Samiuddin, Muhammad [3 ]
Siddiqui, Ali Khursheed [2 ]
Yang, Junzhou [4 ]
Djuansjah, Joy [2 ]
机构
[1] NED Univ Engn & Technol, Dept Mech Engn, Karachi 75270, Pakistan
[2] Imam Mohammad Ibn Saud Islamic Univ, Coll Engn, Mech & Ind Engn Dept, Riyadh 11432, Saudi Arabia
[3] NED Univ Engn & Technol, Dept Met Engn, Karachi 75270, Pakistan
[4] Xian Univ Architecture & Technol, Sch Met Engn, Xian 710075, Peoples R China
关键词
SLM; AlSi10Mg; solution treatment; artificial aging; indentation; Finite Element Analysis; Rockwell Indentation; hardness; PARTS;
D O I
10.3390/cryst14070610
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
This study was conducted to determine the indentation behavior of thin AlSi10Mg specimens manufactured using Selective Laser Melting (SLM) in the as-built condition along with two post-treatments, namely solution heat treatment and artificial aging. Four different thicknesses of 1.0 mm, 1.5 mm, 2 mm, and 2.5 mm of SLM specimens, with the different post-treatments, underwent standardized Rockwell hardness tests using a spherical indenter to determine their hardness values and assess the impression using a stereo microscope and scanning electron microscope (SEM). The as-built specimens showed a trend of smaller indentation depths with increasing specimen thickness, and finally creased with 0.1547 mm depth at 2.5 mm. However, the post-treatments altered the behavior of the specimens to a certain degree, giving larger experimental indentation depths of 0.2204 mm, 0.1962 mm, and 0.1798 mm at 1.0 mm, 1.5 mm, and 2.5 mm thickness, respectively, after solution heat treatment. Artificial aging showed a general decrease in indentation depth with increasing specimen thickness in contrast to solution treatment, and resulted in depths of 0.1888 mm and 0.1596 mm at 1.0 mm and 2.5 mm thickness. Furthermore, a material numerical model was made using stress-strain data on ANSYS Workbench to develop a predictive model for the indentation behavior of the specimens in contrast to experimentation. Under multi-linear isotropic hardening, the Finite Element Analysis (FEA) simulation produced indentation geometry with an average accuracy of 95.4% for the artificial aging series.
引用
收藏
页数:24
相关论文
共 50 条
  • [31] High cycle fatigue performance of AlSi10mg alloy produced by selective laser melting
    Xu, Z. W.
    Wang, Q.
    Wang, X. S.
    Tan, C. H.
    Guo, M. H.
    Gao, P. B.
    MECHANICS OF MATERIALS, 2020, 148
  • [32] Influence of as-built surface and heat treatment on the fatigue resistance of Additively Layer Manufacturing (ALM) AlSi10Mg alloy
    Ngnekou, Julius Noel Domfang
    Nicolai, Julien
    Nadot, Yves
    Henaff, Gilbert
    Ridosz, Lionel
    12TH INTERNATIONAL FATIGUE CONGRESS (FATIGUE 2018), 2018, 165
  • [33] Effect of laser remelting on surface roughness and microstructure of AlSi10Mg selective laser melting manufactured parts
    Boschetto, Alberto
    Bottini, Luana
    Pilone, Daniela
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 113 (9-10): : 2739 - 2759
  • [34] Improving the comprehensive mechanical property of the AlSi10Mg alloy via parameter adaptation of selective laser melting and heat treatment
    Mei, Jiahe
    Han, Ying
    Sun, Jiapeng
    Jiang, Mingkun
    Zu, Guoqing
    Song, Xiaolei
    Zhu, Weiwei
    Ran, Xu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 981
  • [35] Effect of heat treatment patterns on microstructure and mechanical properties of selective laser melting fabricated SiC/AlSi10Mg composite
    Wang, Xingyao
    Lu, Qinghua
    Xu, Shijun
    Zhang, Peilei
    Yan, Hua
    Shi, Haichuan
    Qin, Jianing
    Zhou, Kai
    Chen, Kaiyuan
    Sun, Tianzhu
    OPTICS AND LASER TECHNOLOGY, 2025, 181
  • [36] Influence of processing parameters on AlSi10Mg lattice structure during selective laser melting: Manufacturing defects, thermal behavior and compression properties
    Li, Dongming
    Zhang, Xu
    Qin, Ruixian
    Xu, Jianxin
    Yue, Deyu
    Chen, Bingzhi
    OPTICS AND LASER TECHNOLOGY, 2023, 161
  • [37] EFFECT OF BUILD ATMOSPHERE ON THE SURFACE ROUGHNESS OF AlSi10Mg SAMPLES PRODUCED BY SELECTIVE LASER MELTING
    Hein, Thant Zin
    Babaytsev, A., V
    Ripetskiy, A., V
    NANOSCIENCE AND TECHNOLOGY-AN INTERNATIONAL JOURNAL, 2022, 13 (01) : 1 - 9
  • [38] Influence of wall thickness on the hardness of AlSi10Mg alloy parts manufactured by selective laser melting
    Majeed, Arfan
    Ahmed, Altaf
    Liu, Bufan
    Ren, Shan
    Yang, Jiahao
    52ND CIRP CONFERENCE ON MANUFACTURING SYSTEMS (CMS), 2019, 81 : 459 - 463
  • [39] Effect of the strut size and tilt angle on the geometric characteristics of selective laser melting AlSi10Mg
    Zhang, Baopeng
    Han, Xuesong
    Chen, Changpeng
    Zhang, Wenqi
    Liao, Hailong
    Chen, Baijin
    RAPID PROTOTYPING JOURNAL, 2021, 27 (05) : 879 - 889
  • [40] An approach to predict the residual stress and distortion during the selective laser melting of AlSi10Mg parts
    Lianfeng Wang
    Xiaohui Jiang
    Yihong Zhu
    Xiaogang Zhu
    Jing Sun
    Biao Yan
    The International Journal of Advanced Manufacturing Technology, 2018, 97 : 3535 - 3546