Fatigue crack growth study on rolled and cryogenically treated AZ31B Mg alloy plate

被引:3
作者
Ganesan, Karthick [1 ]
Selvan, Dharani Kumar [2 ]
Marimuthu, Ganesan Somasundaram [3 ]
机构
[1] Sri Sivasubramaniya Nadar Coll Engn, Dept Mech Engn, Chennai 603110, Tamil Nadu, India
[2] KPR Inst Engn & Technol, Ctr Machining & Mat Testing, Coimbatore 641407, Tamil Nadu, India
[3] CSIR Cent Electrochem Res Inst CECRI, Corros & Mat Protect Div, Karaikkudi 630003, Tamil Nadu, India
关键词
AZ31B; Cryogenic treatment; Fatigue crack growth rate; Cleavage failure; MECHANICAL-PROPERTIES; PARIS EQUATION; MICROSTRUCTURE; PROPAGATION; STRENGTH; BEHAVIOR;
D O I
10.1016/j.tafmec.2024.104530
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper investigates the fatigue crack growth rate (FCGR) of AZ31B Mg alloy after cryogenic treatments. Shallow and deep cryogenic treatments were carried out separately at - 80 omicron C and - 196 omicron C for 12 and 72 hrs, respectively. The microstructural characterization of the cryogenically treated AZ31B specimens was carried out by optical microscope (OM) and X -Ray diffraction (XRD). The small crystalline size structure generated in AZ31B alloy due to the cryogenic treatment further promoted the nucleation of Mg 17 Al 12 phase. Accumulation of dislocation density was also observed in the cryogenically treated specimens. CT specimens were prepared for all three conditions to estimate the FCGR. The as -rolled specimen (R) had higher fatigue resistance than the cryogenically treated specimens. The R specimen ' s threshold intensity factor ( Delta K th ) was higher than the cryogenically treated specimens. The exponent (m) value of the R specimen was lower than the shallow and deep cryogenic treated specimens. Hence, the crack growth resistance was marginally higher in the R specimen compared to the cryogenically treated specimens. However, the critical stress intensity factor ( Delta K cr ) of cryogenically treated specimens was slightly higher than the R specimen. The post -fracture characterization of the specimens was carried out at three different regions by SEM. The cleavage faces, tear ridges, and voids were noticed in all specimens. The fatigue failure of the R specimen was due to ductile and brittle mode, whereas the cryogenically treated specimen was dominated entirely by brittle fracture.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Anisotropy of flow during isothermal forging of rolled AZ31B magnesium alloy rolled plate in three orthogonal directions: Correlation with processing maps
    Rao, K. P.
    Prasad, Y. V. R. K.
    Suresh, K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 558 : 30 - 38
  • [22] Effect of laser bionic treatment on fatigue crack growth behavior of TIG welded AZ31B magnesium alloy joint
    Meng, Chao
    Zhang, Zhengqiang
    Yang, Juntao
    Zhuang, Weibin
    Shi, Haifang
    MATERIALS LETTERS, 2022, 320
  • [23] Investigation on ballistic behaviour of friction stir welded rolled AZ31B magnesium alloy
    Dharani Kumar, S.
    Magarajan, U.
    Kumar, Saurabh S.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2022, 236 (10) : 2058 - 2065
  • [24] Microstructures and Properties of FSW Joints of AZ31B Mg Alloy
    Yu, Sirong
    Chen, Xianjun
    MATERIALS PROCESSING TECHNOLOGY, PTS 1-4, 2011, 291-294 : 855 - +
  • [25] Influence of Low Temperature Forging on Microstructure and Low Cycle Fatigue Behavior of Cast AZ31B Mg Alloy
    Toscano, D.
    Shaha, S. K.
    Behravesh, B.
    Jahed, H.
    Williams, B.
    Su, X.
    MAGNESIUM TECHNOLOGY 2018, 2018, : 267 - 273
  • [26] Effects of welding parameters and surface pretreatments on resistance spot welding of AZ31B Mg alloy
    Zhou, Shiquan
    Liu, Lei
    Jung, Jae Pil
    Lee, Mok-Young
    Zhou, Y. Norman
    METALS AND MATERIALS INTERNATIONAL, 2010, 16 (06) : 967 - 974
  • [27] Effect of forging on the low cycle fatigue behavior of cast AZ31B alloy
    Toscano, D.
    Shaha, S. K.
    Behravesh, B.
    Jahed, H.
    Williams, B.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 706 : 342 - 356
  • [28] The influence of surface pre-twinning on the friction and wear performance of an AZ31B Mg alloy
    Mao, Bo
    Siddaiah, Arpith
    Zhang, Xing
    Li, Bin
    Menezes, Pradeep L.
    Liao, Yiliang
    APPLIED SURFACE SCIENCE, 2019, 480 : 998 - 1007
  • [29] Influence of laser shock peening on the surface energy and tribocorrosion properties of an AZ31B Mg alloy
    Siddaiah, Arpith
    Mao, Bo
    Kasar, Ashish K.
    Liao, Yiliang
    Menezes, Pradeep L.
    WEAR, 2020, 462
  • [30] Texture enhancement during grain growth of magnesium alloy AZ31B
    Bhattacharyya, J. J.
    Agnew, S. R.
    Muralidharan, G.
    ACTA MATERIALIA, 2015, 86 : 80 - 94