Effects of elevated temperatures and cooling regimes on the waste andesite dust-based geopolymer mortars

被引:9
作者
Celikten, Serhat [1 ]
Saridemir, Mustafa [2 ]
Sologlu, Mustafa [3 ]
机构
[1] Nevsehir Haci Bektas Veli Univ, Dept Civil Engn, Nevsehir, Turkiye
[2] Nigde Omer Halisdemir Univ, Dept Civil Engn, Nigde, Turkiye
[3] Nevsehir Haci Bektas Veli Univ, Inst Sci, Nevsehir, Turkiye
关键词
Waste andesite dust; Geopolymer; High temperature; Cooling conditions; MECHANICAL-PROPERTIES; MICROSTRUCTURAL PROPERTIES; STRENGTH; SILICATE; BEHAVIOR; POWDER; RESISTANCE; EVOLUTION; CEMENT; RATIOS;
D O I
10.1016/j.conbuildmat.2024.135857
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this study, the geopolymer mortar mixtures were manufactured by activating andesite stone cutting waste dust with sodium silicate. The sodium silicate content in the mixtures was determined to contain 6%, 8% and 10% Na2O by weight of waste andesite dust (WAD). The produced mixtures were subjected to thermal curing at three different temperatures (60 degrees C, 75 degrees C and 90 degrees C), and in two different periods (8 hours and 24 hours). Flexural strength (fs) and compressive strength (fc) tests of 1, 28 and 56 days were carried out on the specimens obtained from the geopolymer mortar mixtures. The effects of Na2O content, thermal curing temperature and time on the strength values of the geopolymer mortars were investigated. Moreover, the geopolymer mortar samples produced with 8 hours of thermal curing were exposed separately to 400 degrees C, 600 degrees C and 800 degrees C. The specimens, which were kept for 1 hour at 400 degrees C, 600 degrees C and 800 degrees C, were exposed to three different cooling conditions (slow-cooled in air, fast-cooled in air and water-cooled). The fs and fc tests were carried out on the cooled geopolymer mortars, and the effects of high temperatures and cooling conditions on the strength properties of the geopolymer mortars were evaluated. In addition, the changes in the microstructures were examined by performing XRD and SEM/EDAX analyses on the selected geopolymer mortars. The fs and fc values of the watercooled geopolymer mortars significantly decreased.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] The effects on mechanical properties of sustainable use of waste andesite dust as a partial substitution of cement in cementitious composites
    Ozkan, Sukru
    Ceylan, Hakan
    [J]. JOURNAL OF BUILDING ENGINEERING, 2022, 58
  • [32] Performance of eco-friendly fly ash-based geopolymer mortars with stone-cutting waste
    Ozturk, Zahide Bayer
    Cam, Tugrul
    [J]. MATERIALS CHEMISTRY AND PHYSICS, 2023, 307
  • [33] Compressive strength and microstructure of alkali-activated fly ash/slag binders at high temperature
    Pan, Z.
    Tao, Z.
    Cao, Y. F.
    Wuhrer, R.
    Murphy, T.
    [J]. CEMENT & CONCRETE COMPOSITES, 2018, 86 : 9 - 18
  • [34] Reaction mechanism, kinetics and high temperature transformations of geopolymers
    Rahier, H.
    Wastiels, J.
    Biesemans, M.
    Willlem, R.
    Van Assche, G.
    Van Mele, B.
    [J]. JOURNAL OF MATERIALS SCIENCE, 2007, 42 (09) : 2982 - 2996
  • [35] Development of high volume rice husk ash alumino silicate composites
    Rattanasak, Ubolluk
    Chindaprasirt, Prinya
    Suwanvitaya, Prasert
    [J]. INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2010, 17 (05) : 654 - 659
  • [36] Fire performance of fly-ash-based geopolymer concrete: Effect of burning temperature on mechanical and microstructural properties
    Razak, Siti Nooriza Abd
    Shafiq, Nasir
    Nikbakht, Ehsan Hasan
    Mohammed, Bashar S.
    Guillaumat, Laurent
    Farhan, Syed Ahmad
    [J]. MATERIALS TODAY-PROCEEDINGS, 2022, 66 : 2665 - 2669
  • [37] Strength and Ultrasonic Characteristics of Alkali-Activated Fly Ash-Slag Geopolymer Concrete after Exposure to Elevated Temperatures
    Ren, Weibo
    Xu, Jinyu
    Bai, Erlei
    [J]. JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2016, 28 (02)
  • [38] Effect of high temperature on the microstructural evolution of fiber reinforced geopolymer composite
    Samal, Sneha
    [J]. HELIYON, 2019, 5 (05)
  • [39] Applications of glaze and decor on dimensioned andesites used in construction sector
    Sariisik, Ali
    Sariisik, Gencay
    Senturk, Ahmet
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2011, 25 (09) : 3694 - 3702
  • [40] Effect of fire exposure on cracking, spalling and residual strength of fly ash geopolymer concrete
    Sarker, Prabir Kumar
    Kelly, Sean
    Yao, Zhitong
    [J]. MATERIALS & DESIGN, 2014, 63 : 584 - 592