Comparison of the Mechanical Properties of Hardfacings Made by Standard Coated Stick Electrodes and a Newly Developed Rectangular Stick Electrode

被引:1
作者
Bjelajac, Edvard [1 ]
Skumavc, Andrej [2 ]
Lojen, Gorazd [3 ]
Manjgo, Mirza [3 ]
Vuherer, Tomaz [3 ]
机构
[1] Messer Slovenija Doo, Jugova Ulica 20, Ruse 2342, Slovenia
[2] SIJ Acroni Doo, Cesta Borisa Kidr 44, Jesenice 4270, Slovenia
[3] Univ Maribor, Fac Mech Engn, Smetanova Ulica 17, Maribor 2000, Slovenia
关键词
hardfacing; dilution rate; hardness; Charpy impact toughness; residual stress; fracture toughness; CARBON-STEEL; WEAR; BEHAVIOR; MICROSTRUCTURE; SMAW;
D O I
10.3390/ma17092051
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cladding with a stick electrode is one of the oldest arc processes for adding a deposit on a base material. The process is suitable for outdoor working, but the disadvantages are low productivity and large dilution rates. In this work, a simple solution is proposed, which would enable cladding of a larger area with one pass and decrease the dilution rate at the same time-a new type of electrode was developed, exhibiting a rectangular cross-section instead of a round one. Hardfacings, welded with E Fe8 electrodes according to EN 14 700 Standard were welded on mild steel S355 J2 base material with three different coated stick electrodes. The first one was a commercially available, standard, round hardfacing electrode, the second was the same, but with a thinner coating, and the third one was a newly developed rectangular electrode. All three types had equal cross-sections of the metallic core and the same type of coating. Manufacturing of the rectangular electrodes in the laboratory is explained briefly. One- and multi-layer deposits were welded with all three types. Differences were observed in the arc behavior between the round and rectangular electrodes. With the rectangular electrode, the microstructure of the deposit was finer, penetration was shallower, and dilution rates were lower, while the hardness was higher, residual stresses predominantly compressive, and the results of instrumented Charpy impact tests and fracture mechanics tests were better.
引用
收藏
页数:22
相关论文
共 56 条
  • [21] Investigation on the impact wear behavior of 2.25Cr-1Mo steel at elevated temperature
    Chen, Xu-dong
    Wang, Li-wen
    Yang, Ling-yun
    Tang, Rui
    Yu, Yan-qing
    Cai, Zhen-bing
    [J]. WEAR, 2021, 476
  • [22] Operational behavior assesment of coated tubular electrodes for SMAW hardfacing
    Crespo, Amado Cruz
    Scotti, Americo
    Perez, Manuel Rodriquez
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2008, 199 (1-3) : 265 - 273
  • [23] Wear and diffusive processes
    D'Acunto, M
    [J]. TRIBOLOGY INTERNATIONAL, 2003, 36 (07) : 553 - 558
  • [24] Dasgupta R., 1997, Surf. Eng, V13, P123, DOI [10.1179/sur.1997.13.2.123, DOI 10.1179/SUR.1997.13.2.123]
  • [25] Method for conducting micro-abrasion wear testing of materials in oscillating sliding
    David Resendiz-Calderon, Cesar
    Cazares-Ramirez, Irving
    Laura Samperio-Galicia, Diana
    Israel Farfan-Cabrera, Leonardo
    [J]. METHODSX, 2022, 9
  • [26] Fretting wear behavior of the high-carbon high-chromium X210CrW12 steel: Influence of counterbody material
    Duan, Yong
    Qu, Shengguan
    Jia, Siyu
    Li, Xiaoqiang
    [J]. WEAR, 2021, 486
  • [27] Elektrode Jesenice d.o.o., 2009, Welding Consumable, pK7
  • [28] Garbade R. R., 2021, IOP Conference Series: Materials Science and Engineering, V1017, DOI 10.1088/1757-899X/1017/1/012033
  • [29] Modification of TiB2/Fe coating by SMAW with high carbon ferrochrome
    Guo, L. J.
    Wang, X. B.
    Wang, F. H.
    Wang, H. B.
    [J]. SURFACE ENGINEERING, 2013, 29 (08) : 642 - 646
  • [30] Gwidon W.W.S., 2005, WearMaterials, Mechanisms and Practice