Examining Sigma Phase in Super Duplex Stainless Steels (UNS S32750) after Isothermal Aging, Focusing on Its Influence on Etching and Pitting Corrosion with Optical Microscopy

被引:2
|
作者
Shrivastava, Rahul [1 ]
Maurya, Rita [2 ]
Katiyar, Prvan Kumar [1 ]
机构
[1] Natl Inst Technol Srinagar, Dept Met & Mat Engn, Srinagar 190006, India
[2] Natl Inst Technol Hamirpur, Dept Mat Sci & Engn, Hamirpur 177005, India
关键词
Super duplex stainless steel; Sigma phase; Electrochemical etching; Optical microscope; XRD; Pitting corrosion; MECHANICAL-PROPERTIES; INTERGRANULAR CORROSION; CHI PHASES; BEHAVIOR; PRECIPITATION; MICROSTRUCTURE; RESISTANCE; EVOLUTION;
D O I
10.1007/s13632-024-01120-y
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Super duplex stainless steel (SDSS), known for its ferritic-austenitic microstructure and exceptional corrosion resistance, is widely used in petrochemical and marine industries. The impact of sigma (sigma) phase formation on the pitting corrosion behavior of isothermally aged SDSS across varying aging times (15, 30, 45, 120, 420 min) at 1000 degrees C has been investigated in this study. Phase sizes and morphologies, which have evolved over aging time, have been measured after electrochemical etching. Optical microscopy and XRD analysis revealed the evolution of ferrite (alpha), austenite (gamma), and secondary phases (sigma and gamma 2). As aging time increased, the fractions of gamma 2 and sigma phases rose at the expense of the alpha phase. Pitting corrosion tests, conducted according to ASTM-G48 standards, indicated a decline in corrosion resistance with increased secondary phase fraction due to compositional variances, leading to electrochemical potential changes and micro-galvanic cell formation. Prolonged aging resulted in more pronounced Cr- and Mo-depleted areas, increasing the corroded surface fraction and pits volume-to-depth ratio. Correspondingly, the overall corrosion performance was assessed based on pit volume, calculated using optical microscopy, and escalated with aging time, indicating progressive corrosion damage. The study concludes that the sigma phase negatively impacts pitting corrosion resistance, requiring careful management of high-temperature applications, welding, and heat treatments to control sigma phase formation in SDSS. These insights are crucial for optimizing SDSS in petrochemical and marine industries, enhancing service life and reliability in corrosive environments.
引用
收藏
页码:741 / 763
页数:23
相关论文
共 40 条
  • [21] Influence of machining parameters on tool wear, residual stresses, and corrosion resistance after milling super duplex stainless steel UNS S32750
    Marques, Daniel Cirillo
    Suyama, Daniel Iwao
    Antunes, Renato Altobelli
    Hassui, Amauri
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 129 (1-2) : 801 - 814
  • [22] Influence of Sigma Phase Formation on Pitting Corrosion of an Aged UNS S31803 Duplex Stainless Steel
    dos Santos, Daniella Caluscio
    Magnabosco, Rodrigo
    de Moura-Neto, Carlos
    CORROSION, 2013, 69 (09) : 900 - 911
  • [23] Effects of the Volume Fraction of the Secondary Phase after Solution Annealing on Electrochemical Properties of Super Duplex Stainless Steel UNS S32750
    Kim, Dohyung
    Chung, Wonsub
    Shin, Byung-Hyun
    METALS, 2023, 13 (05)
  • [24] Role of microstructure on the varying corrosion behavior across the UNS S32750 super duplex stainless steel friction stir weld
    Ajay, E.
    Prasad, A. D. V.
    Rao, A. G.
    Raja, V. S.
    JOURNAL OF MATERIALS SCIENCE, 2025, 60 (03) : 1628 - 1646
  • [25] Microstructure, Corrosion Resistance, and Hardness of Simulated Heat-Affected Zone of Duplex UNS S32205 and Superduplex UNS S32750 Stainless Steels
    Pecly, P. H. R.
    Almeida, B. B.
    Perez, G.
    Pimenta, A. R.
    Tavares, S. S. M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (20) : 9019 - 9028
  • [26] Premature failure in UNS S32750 duplex stainless steel laying head pipes: The role of sigma phase precipitation
    Moreira, Guilherme Duarte
    Maia, Juliana de Fatima
    de Faria, Geraldo Lucio
    ENGINEERING FAILURE ANALYSIS, 2025, 169
  • [27] Effect of Aging Treatment on Corrosion Resistance of S32750 Super Duplex Stainless Steel in Simulated Seawater at Low Temperature
    Jin, Lan
    Liang, Ping
    Shi, Yanhua
    Guo, Yier
    Zhao, Yan
    Li, Fei
    Hou, Guanyu
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (04): : 3651 - 3662
  • [28] Effect of isothermal aging on the pitting corrosion resistance of UNS S82441 duplex stainless steel based on electrochemical detection
    Zhang, Ziying
    Zhao, Hui
    Zhang, Huizhen
    Yu, Zhishui
    Hu, Jun
    He, Liang
    Li, Jing
    CORROSION SCIENCE, 2015, 93 : 120 - 125
  • [29] Effect of Aging Temperature on the Microstructure, Local Mechanical Properties, and Wear Behavior of a UNS S32750 Super Duplex Stainless Steel
    Bouzid Maamache
    Billel Cheniti
    Brahim Belkessa
    Karima Tahar-chaouch
    Ramdhane Kouba
    Journal of Materials Engineering and Performance, 2021, 30 : 546 - 555
  • [30] Influence of Solution Treatment Duration on Microstructural Features of an Industrial Forged UNS S32750/1.4410/F53 Super Duplex Stainless Steel (SDSS) Alloy
    Cojocaru, Vasile Danut
    Raducanu, Doina
    Angelescu, Mariana Lucia
    Vintila, Adrian Nicolae
    Serban, Nicolae
    Dan, Ioan
    Cojocaru, Elisabeta Mirela
    Cinca, Ion
    JOM, 2017, 69 (08) : 1439 - 1445