Comparative study of Ti-6.5Al-2Zr-1Mo-1V (TA15) alloy fabricated by selective laser melting and laser metal deposition

被引:5
|
作者
Xu, Wei [1 ,2 ]
Zhu, Xiangyu [1 ,2 ]
Wang, Zhe [3 ]
Ran, Xing [4 ]
Li, Zhiyong [5 ]
Chen, Rong [5 ]
Du, Zhiheng [1 ,2 ]
Zhang, Xiaohang [1 ,2 ]
Singh, Harshpreet [6 ]
Zhang, Jiazhen [1 ]
Lu, Xin [1 ,2 ]
机构
[1] Univ Sci & Technol Beijing, Inst Engn Technol, Natl Engn Res Ctr Adv Rolling & Intelligent Mfg, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, Shunde Innovat Sch, Foshan 528399, Peoples R China
[3] AVIC Heavy Machinery Res Inst, Xian Branch, Xian 710200, Peoples R China
[4] AVIC Heavy Machinery Co Ltd, Guiyang 550005, Peoples R China
[5] Aerosp Addit Technol Beijing Co Ltd, Beijing 100074, Peoples R China
[6] Univ Auckland, Dept Chem & Mat Engn, Auckland 1142, New Zealand
来源
基金
中国国家自然科学基金;
关键词
Selective laser melting; Laser metal deposition; Ti-6.5Al-2Zr-1Mo-1V alloy; Microstructure; Mechanical property; Forming cost; MECHANICAL-PROPERTIES; POWDER-METALLURGY; PURE TI; TITANIUM; BEHAVIOR; DESIGN;
D O I
10.1016/j.optlastec.2024.111052
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
In the present study, Ti-6.5Al-2Zr-1Mo-1V (TA15) alloy, one of the widely used near-alpha titanium alloys in the field of aeronautical and astronautical, was fabricated by two lasers additive manufacturing technologies, namely selective laser melting (SLM) and laser metal deposition (LMD). Microstructure, mechanical property, productivity, and forming cost of fabricated TA15 samples by these two processes were compared systematically. The results showed that the microstructure of the SLM-ed and LMD-ed samples exhibited differences in terms of crystallographic orientations, grain boundaries, and grain sizes, which was mainly attributed to the distinct thermal histories associated with each process. Such differences resulted in the LMD-ed sample presenting anisotropy, lower tensile strength, and higher elongation compared to the SLM-ed sample. Cost analysis indicated that the forming cost per unit volume of the LMD-ed sample was about half that of the SLM-ed sample. This difference was primally due to the higher productivity of the LMD process (226.1 cm3/h) compared to the SLM process (8.8 cm3/h), as well as the lower power cost of the powder materials (60 vs. 100 $/kg). Furthermore, the forming maximum volume of the LMD process (-30.38 m3) was about 28 times than that of the SLM process (-1.08 m3). In conclusion, this study provides a detailed comparison between SLM-ed and LMD-ed TA15 samples. The findings can act as a reference for selecting optimized fabrication methods for practical industrial applications, taking into consideration specific mechanical properties, forming size, and cost requirements.
引用
收藏
页数:9
相关论文
共 50 条
  • [41] Microstructure and property evaluation of TA15 titanium alloy fabricated by selective laser melting after heat treatment
    Huang, Shuai
    Sun, Bingbing
    Guo, Shaoqing
    OPTICS AND LASER TECHNOLOGY, 2021, 144
  • [42] Microstructure and property evaluation of TA15 titanium alloy fabricated by selective laser melting after heat treatment
    Huang, Shuai
    Sun, Bingbing
    Guo, Shaoqing
    Optics and Laser Technology, 2021, 144
  • [43] Microstructure and Mechanical Property of Ti-5Al-5Mo-5V-3Cr-1Zr Alloy Fabricated by Selective Laser Melting with a Preheated Substrate
    Deng, Hao
    Qiu, Wenbin
    Chen, Longqing
    Cao, Sheng
    Wei, Yongqiang
    Hu, Zhendong
    Cui, Xuidong
    Tang, Jun
    ADVANCED ENGINEERING MATERIALS, 2021, 23 (09)
  • [44] Effect of α texture on the anisotropy of yield strength in Ti-6Al-2Zr-1Mo-1V alloy fabricated by laser directed energy deposition technique
    Li, Renkai
    Wang, Huaming
    He, Bei
    Li, Zhuo
    Zhu, Yanyan
    Zheng, Dongdong
    Tian, Xiangjun
    Zhang, Shuquan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 824
  • [45] Thermal expansion properties of laser melting deposited Ti-6.5Al-2Zr-1Mo-1W alloy during α plus β zone annealing
    Li, Zhuo
    Cheng, Xu
    Li, Jia
    Wang, Huaming
    MATERIALS CHARACTERIZATION, 2017, 128 : 115 - 122
  • [46] Deformation Behavior and Microstructure Evolution of a TiB-Reinforced Ti-6.5Al-2Zr-1Mo-1V Matrix Composite
    Ozerov, Maxim
    Stepanov, Nikita
    Sokolovsky, Vitaly
    Astakhov, Ilya
    Klimova, Margarita
    Galtsev, Alexander
    Huang, Lujun
    Zherebtsov, Sergey
    METALS, 2023, 13 (11)
  • [47] Enhanced mechanical properties of Ti-6Al-2Zr-1Mo-1V with ultrafine crystallites and nano-scale twins fabricated by selective laser melting
    Wu, Xu
    Cai, Chao
    Yang, Lei
    Liu, Wan
    Li, Wei
    Li, Ming
    Liu, Jie
    Zhou, Kun
    Shi, Yusheng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 738 : 10 - 14
  • [48] Anisotropy of Ti6Al4V Alloy Fabricated by Selective Laser Melting
    Diao W.
    Du L.
    Wang Y.
    Zhou H.
    Sun J.
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2022, 36 (03): : 231 - 240
  • [49] The anisotropic of corrosion and tribocorrosion behaviors of Ti-15Mo alloy fabricated by selective laser melting
    Chen, Jian
    Li, Chaoying
    Zhou, Libo
    Ren, Yanjie
    Li, Cong
    Liao, Xingyu
    Wang, Yuanjing
    Niu, Yan
    MATERIALS CHARACTERIZATION, 2022, 190
  • [50] Ti-6.5Al-2Zr-1Mo-1V钛合金低温应力松弛及组织演变(英文)
    黄镇
    袁武华
    朱佳佳
    稀有金属材料与工程, 2022, 51 (01) : 83 - 91