Study on microstructure, mechanical and corrosion behavior of Ti-6Al-4V titanium alloy by Keyhole gas tungsten arc welding

被引:2
|
作者
Zhang, Luxia [1 ]
Wu, Zhisheng [1 ]
Li, Yan [1 ,2 ]
Feng, Yulan [1 ]
Zhao, Fei [1 ]
机构
[1] Taiyuan Univ Sci & Technol, Coll Mat Sci & Engn, Taiyuan 030024, Peoples R China
[2] Shanxi Elect Sci & Technol Inst, Linfen 041000, Peoples R China
来源
MATERIALS TODAY COMMUNICATIONS | 2024年 / 40卷
基金
中国国家自然科学基金;
关键词
Ti-6Al-4V; K-TIG welding; Microstructure; Mechanical properties; Electrochemical corrosion; EVOLUTION; TEXTURE; RESISTANCE; JOINT; BETA; NB;
D O I
10.1016/j.mtcomm.2024.109530
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, 8 mm thick Ti6Al4V titanium alloy was successfully welded by keyhole gas tungsten electrode arc welding (K-TIG) technology without special edge preparation. The microstructure, mechanical properties and corrosion resistance of the joint were studied. The experimental results show that the overall weld is nail -shaped, and there are no welding defects such as porosity, cracks, and unfused sidewalls. The weld area is mainly composed of many fine acicular -like alpha, coarse acicular -like alpha and massive alpha intertwined with each other, and the distribution ratio of high -angle grain boundaries in the heat -affected zone and weld metal area is higher than that of the base metal. The microhardness fluctuation of each region in the welded joints is not large, and the tensile strength of the welded joints reaches 96.7 % of the base metal, and the post -weld mechanical properties are good. The K-TIG welded joints and the base metal were electrochemically analyzed, and the welded joints showed good corrosion resistance.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] Corrosion Behavior of Additive Manufactured Ti-6Al-4V Alloy in NaCl Solution
    Yang, Jingjing
    Yang, Huihui
    Yu, Hanchen
    Wang, Zemin
    Zeng, Xiaoyan
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2017, 48A (07): : 3583 - 3593
  • [32] Corrosion Behavior of Friction Stir-Processed and Gas Tungsten Arc-Welded Ti-6Al-4V
    Atapour, Masoud
    Pilchak, Adam L.
    Frankel, G. S.
    Williams, James C.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (09): : 2318 - 2327
  • [33] An Exploratory Study on Resistance Spot Welding of Titanium Alloy Ti-6Al-4V
    Fatmahardi, Ichwan
    Mustapha, Mazli
    Ahmad, Azlan
    Derman, Mohd Nazree
    Lenggo Ginta, Turnad
    Taufiqurrahman, Iqbal
    MATERIALS, 2021, 14 (09)
  • [34] Friction stir welding of additively manufactured Ti-6Al-4V: Microstructure and mechanical properties
    Singh, Amit Kumar
    Kumar, Bhoopendra
    Jha, Kaushal
    Astarita, Antonello
    Squillace, Antonino
    Franchitti, Stefania
    Arora, Amit
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2020, 277
  • [35] Effect of cryogenic coupled magnetic field treatment on the microstructure and mechanical properties on Ti-6Al-4V titanium alloy
    Song, Xin
    Qi, Huiping
    Li, Shuang
    Hu, Yong
    Yang, Wen
    Li, Zhenjiang
    MATERIALS TODAY COMMUNICATIONS, 2024, 40
  • [36] Study on the warm deformation behavior and microstructure evolution of the MDIFed Ti-6Al-4V titanium alloy
    Yang, Yingxiang
    Wang, He
    Feng, Zhongxue
    Shi, Qingnan
    Yang, Bin
    Chen, Min
    Qi, Huarong
    Wang, Xiaoqi
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 8929 - 8943
  • [37] Experimental and numerical studies on gas tungsten arc welding of Ti-6Al-4V tailor-welded blank
    Karpagaraj, A.
    Rajesh Kumar, N.
    Thiyaneshwaran, N.
    Siva Shanmugam, N.
    Cheepu, MuraliMohan
    Sarala, R.
    JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2020, 42 (10)
  • [38] Effect of the welding parameters on microstructure and mechanical properties of linear friction welded Ti-6Al-4V alloy
    Choi, Jeong-Won
    Aoki, Yasuhiro
    Ushioda, Kohsaku
    Fujii, Hidetoshi
    JOURNAL OF MANUFACTURING PROCESSES, 2022, 75 : 651 - 663
  • [39] Microstructure Evolution and Abrasive Wear Behavior of Ti-6Al-4V Alloy
    Hadke, Shreyash
    Khatirkar, Rajesh K.
    Shekhawat, Satish K.
    Jain, Shreyans
    Sapate, Sanjay G.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (10) : 3969 - 3981
  • [40] Microstructure and Mechanical Properties of Keyhole Gas Tungsten Arc Welds in Titanium and Titanium Alloys
    Lathabai, S.
    Barton, K. J.
    Green, L. K.
    Tyagi, V. K.
    TRENDS IN WELDING RESEARCH, PROCEEDINGS, 2006, : 711 - 716