Effect of treatment conditions on the morphology of date empty fruit bunch lignocellulosic fiber for biocomposite applications

被引:0
作者
Alsuwait, Raed B. [1 ]
Bakare, Azeez Oladipupo [2 ]
Souiyah, Miloud [1 ]
Ganiyu, Saheed Adewale [3 ]
Momohjimoh, Ibrahim [4 ]
机构
[1] Univ Hafr AlBatin, Coll Engn, Dept Mech Engn, POB 1803, Hafr Albatin 39524, Saudi Arabia
[2] Univ Hafr AlBatin, Appl Coll, Dept Nondestruct Evaluat Technol, POB 1803, Hafr Albatin 39524, Saudi Arabia
[3] King Fahd Univ Petr & Minerals, Coll Chem & Mat, Dept Chem, POB 5026, Dhahran 31261, Saudi Arabia
[4] Univ Hafr AlBatin, Appl Coll, Dept Mech Engn Technol, POB 1803, Hafr Albatin 39524, Saudi Arabia
来源
CARBOHYDRATE POLYMER TECHNOLOGIES AND APPLICATIONS | 2024年 / 7卷
关键词
Fiber treatment; Characterization; Date fiber; Boiling water; Morphology; Sodium hydroxide; NATURAL FIBER; OIL PALM; MECHANICAL-PROPERTIES; COMPOSITES; EXTRACTION; CELLULOSE;
D O I
10.1016/j.carpta.2024.100519
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
The fiber of the empty date fruit is one of the waste products left after the date fruit is harvested from the date palm. Optimization of the treatment parameters as well as the economics of the treatment process are critical to the successful commercialization of the treatment of natural fibers for the production of biocomposites. Of the natural fiber treatment methods described in previous work, hot water and alkali treatments are the most costeffective, which justified the choice of these treatment methods in this work. Here, date empty fruit bunch fibers were pulverized to a particle size of 0 -500 mu m and then treated with boiling water at 100 degrees C for 3 h or with sodium hydroxide at different concentrations (2, 5, 10%) for 3 h at room temperature with constant stirring at 800 rpm. To confirm the effect of temperature on the fiber treatment, another fiber sample was treated at a 5% concentration of sodium hydroxide solution at an elevated temperature of 80 degrees C for the same period and stirring condition. The untreated and treated DEFB fibers were characterized by X-ray diffraction (XRD), Fourier transform infrared (FTIR), nuclear magnetic resonance (NMR), differential scanning calorimetry (DSC), X-ray fluorescence (XRF), and scanning electron microscopy (SEM). Chemical analysis of the fibers showed that DEFB fiber treated with 5% sodium hydroxide solution at room temperature had the highest cellulose content (52.0%), which was also confirmed by the XRD analysis. The DEFB fiber treated with boiling water exhibited higher thermal stability while the sodium hydroxide-treated fiber exhibited higher crystallinity index and cellulose content. Apparently, DEFB fiber treated with sodium hydroxide solution at 5% concentration for 3 h at room temperature for continuous stirring at 800 rpm offered the best properties. The treated fibers are expected to be viable reinforcement in the production of biocomposites with the goal of achieving energy efficiency. The developed materials could be used in industrial applications such as insulating building systems, automotive parts, and home furniture.
引用
收藏
页数:12
相关论文
共 61 条
  • [1] Extraction of oxidized nanocellulose from date palm (Phoenix Dactylifera L.) sheath fibers: Influence of CI and CII polymorphs on the properties of chitosan/bionanocomposite films
    Adel, Abeer
    El-Shafei, Amira
    Ibrahim, Atef
    Al-Shemy, Mona
    [J]. INDUSTRIAL CROPS AND PRODUCTS, 2018, 124 : 155 - 165
  • [2] Isolation and characterization of insoluble date (Phoenix dactylifera L.) fibers
    Ahmed, Jasim
    Almusallam, Abdulwahab
    Al-Hooti, Suad N.
    [J]. LWT-FOOD SCIENCE AND TECHNOLOGY, 2013, 50 (02) : 414 - 419
  • [3] The major proteins of the seed of the fruit of the date palm (Phoenix dactylifera L.): Characterisation and emulsifying properties
    Akasha, Ibrahim
    Campbell, Lydia
    Lonchamp, Julien
    Euston, Stephen R.
    [J]. FOOD CHEMISTRY, 2016, 197 : 799 - 806
  • [4] Optimisation and economic evaluation of the supercritical carbon dioxide extraction of waxes from waste date palm (Phoenix dactylifera) leaves
    Al Bulushi, Karima
    Attard, Thomas M.
    North, Michael
    Hunt, Andrew J.
    [J]. JOURNAL OF CLEANER PRODUCTION, 2018, 186 : 988 - 996
  • [5] Characterization of treated date palm tree fiber as composite reinforcement
    Alawar, Ahmad
    Hamed, Ahmad M.
    Al-Kaabi, Khalifa
    [J]. COMPOSITES PART B-ENGINEERING, 2009, 40 (07) : 601 - 606
  • [6] Microcrystalline Cellulose from Fruit Bunch Stalk of Date Palm: Isolation and Characterization
    Alotabi, Majed D.
    Alshammari, Basheer A.
    Saba, N.
    Alothman, Othman Y.
    Kian, Lau Kia
    Khan, Anish
    Jawaid, Mohammad
    [J]. JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2020, 28 (06) : 1766 - 1775
  • [7] Characterization of natural fiber obtained from different parts of date palm tree (Phoenix dactylifera L.)
    Alotaibi, Majed D.
    Alshammari, Basheer A.
    Saba, N.
    Alothman, Othman Y.
    Sanjay, M. R.
    Almutairi, Zeyad
    Jawaid, Mohammad
    [J]. INTERNATIONAL JOURNAL OF BIOLOGICAL MACROMOLECULES, 2019, 135 : 69 - 76
  • [8] Recent Development in the Processing, Properties, and Applications of Epoxy-Based Natural Fiber Polymer Biocomposites
    Alsuwait, Raed B.
    Souiyah, Miloud
    Momohjimoh, Ibrahim
    Ganiyu, Saheed Adewale
    Bakare, Azeez Oladipupo
    [J]. POLYMERS, 2023, 15 (01)
  • [9] Alkaline treatment combined with enzymatic hydrolysis for efficient cellulose nanofibrils production
    Banvillet, Gabriel
    Depres, Gael
    Belgacem, Naceur
    Bras, Julien
    [J]. CARBOHYDRATE POLYMERS, 2021, 255
  • [10] Experimental study of physical, chemical and mechanical properties of enset and sisal fibers
    Bekele, Abera E.
    Lemu, Hirpa G.
    Jiru, Moera G.
    [J]. POLYMER TESTING, 2022, 106