CMAS corrosion resistance of Y 2 O 3-Al 2 O 3 binary ceramic materials

被引:1
作者
Li, Chenguang [1 ]
Lai, Chenbiao [1 ]
Wu, Yaoyan [2 ]
Ouyang, Hanxiang [2 ]
Sun, Junbin [1 ,3 ,4 ,5 ]
Lu, Weihong [1 ,3 ,4 ,5 ]
机构
[1] Hengyang Normal Univ, Coll Chem & Mat Sci, Hengyang 421008, Peoples R China
[2] Hengyang Normal Univ, Coll Nanyue, Hengyang 421008, Peoples R China
[3] Hengyang Normal Univ, Hunan Prov Key Lab Funct Met Organ Cpds, Hengyang 421008, Peoples R China
[4] Hengyang Normal Univ, Coll Hunan Prov, Key Lab Organometall New Mat, Hengyang 421008, Peoples R China
[5] Hengyang Normal Univ, Hunan Engn Res Ctr Monitoring & Treatment Heavy Me, Hengyang 421008, Peoples R China
基金
中国国家自然科学基金;
关键词
CMAS corrosion; Alumina based compounds; THERMAL BARRIER COATINGS; MAGNESIUM-ALUMINA-SILICATE; HOT CORROSION; OPTICAL BASICITY; CYCLING BEHAVIOR; DEGREES-C; PART I; DELAMINATION; TEMPERATURE; EVOLUTION;
D O I
10.1016/j.ceramint.2024.01.286
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Alumina based rare earth oxides ceramic materials, with the good performance against the CMAS corrosion, were widely used as the thermal/environmental barrier coatings. In this work, three Y 2 O 3 - Al 2 O 3 binary ceramic bulks, which were the Y 3 Al 5 O 12 , YAlO 3 and Y 4 Al 2 O 9 , were prepared by high temperature solid state reaction using the Y 2 O 3 and Al 2 O 3 as the raw materials. The resistances to CMAS corrosion of these materials at 1250 degrees C and 1350 degrees C were compared fully. The compositions and structures of the samples before and after corrosion were analysed by X-ray diffraction (XRD) and scanning electron microscopy (SEM). Results showed that the different chemical compositions of the materials resulted in the different optical basicity (OB) values which can decide the reactivity of the material with the CMAS melts. The Y 3 Al 5 O 12 ceramic material was inert to the CMAS for its low OB value of 0.75 and damaged seriously by the CMAS through physical penetration. The YAlO 3 and Y 4 Al 2 O 9 with the high OB values of 0.80 and 0.87 reacted with the CMAS to form the Ca 4 Y 6 (SiO 4 ) 6 O. The YAlO 3 ceramic bulk exhibited the good performance against the CMAS corrosion benefitting from the formation of the Ca 4 Y 6 (SiO 4 ) 6 O and the CaAl 2 Si 2 O 8 .
引用
收藏
页码:13721 / 13731
页数:11
相关论文
共 50 条
  • [41] Erosion mechanism of the postmortem Al2O3-Ti2O3-Al sliding gate containing novel Al2O3-Ti2O3 raw materials
    Zheng, Qingyao
    Li, Yong
    Ma, Chenhong
    Sun, Jialin
    Gao, Yuan
    Li, Hongxia
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (08) : 3788 - 3793
  • [42] Effect of Y2O3 contents on microstructural, mechanical, and antioxidative characteristics of Al2O3-ZrO2-Y2O3 coatings
    Yu, Yongdong
    Pan, Jiayu
    Yuan, Yuchen
    Liu, Xudong
    Yu, Wanjun
    Yin, Hang
    Zheng, Yongting
    He, Xiaodong
    APPLIED SURFACE SCIENCE, 2022, 590
  • [43] Reactive Sintering of Al2O3-Y3Al5O12 Ceramic Composites Obtained by Direct Ink Writing
    Baltazar, Joana
    Alves, Manuel Fellipe Rodrigues Pais
    dos Santos, Claudinei
    Olhero, Susana
    CERAMICS-SWITZERLAND, 2022, 5 (01): : 1 - 12
  • [44] Equiaxed colony growth in the small undercooled Y2O3-doped Al2O3-ZrO2 eutectic ceramic melt
    Fu, Lian-sheng
    Fu, Ying
    Yu, Zhan-dong
    Ma, Zheng
    Fu, Xue-song
    Chen, Guo-qing
    CERAMICS INTERNATIONAL, 2024, 50 (06) : 8625 - 8633
  • [45] Corrosion behavior of CMAS coupling NaVO3 salt for plasma-sprayed Al2O3/YSZ thermal barrier coatings
    Zhang, Yongang
    Han, Jiasen
    Wu, Dongting
    Zou, Yong
    CORROSION SCIENCE, 2023, 221
  • [46] Robust corrosion resistance of Yb4Hf3O12 coating against CMAS attack at 1300-1500 °C
    Wu, Yiming
    Zhong, Xin
    Hong, Du
    Chen, Xiaowu
    Shi, Minhao
    Huang, Liping
    Niu, Yaran
    Zeng, Yi
    Zheng, Xuebin
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (04)
  • [47] Microstructure and mechanical properties of Y2O3-doped melt-grown Al2O3-ZrO2 eutectic ceramic
    Fu, Lian-sheng
    Wang, Zhen
    Fu, Xue-song
    Chen, Guo-qing
    Zhou, Wen-long
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 703 : 372 - 379
  • [48] Study of Gd2O3-Doped La2(Zr0.7Ce0.3)2O7 Thermal Barriers for Coating Ceramic Materials for CMAS Resistance
    Song, Xiaowei
    Xie, Min
    Qu, Xiaofu
    Song, Xiwen
    Zhang, Yonghe
    Mu, Rende
    COATINGS, 2025, 15 (04):
  • [49] Ruby micro-piezospectroscopy in GdAlO3/Al2O3(/ZrO2), Er3Al5O12/Al2O3(/ZrO2) and Y3Al5O12/Al2O3(/ZrO2) binary and ternary directionally solidified eutectics
    Gouadec, Gwenael
    Makaoui, Karim
    Perriere, Loic
    Colomban, Philippe
    Mazerolles, Leo
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (10) : 2145 - 2151
  • [50] Corrosion Resistance of Al2O3 Coating Prepared by Filtered Cathodic Vacuum Arc for Thermal Barrier Coatings Against CMAS Degradation
    Tao, Liu
    Qing, He
    Dan, Li
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (11) : 3981 - 3988