CMAS corrosion resistance of Y 2 O 3-Al 2 O 3 binary ceramic materials

被引:1
|
作者
Li, Chenguang [1 ]
Lai, Chenbiao [1 ]
Wu, Yaoyan [2 ]
Ouyang, Hanxiang [2 ]
Sun, Junbin [1 ,3 ,4 ,5 ]
Lu, Weihong [1 ,3 ,4 ,5 ]
机构
[1] Hengyang Normal Univ, Coll Chem & Mat Sci, Hengyang 421008, Peoples R China
[2] Hengyang Normal Univ, Coll Nanyue, Hengyang 421008, Peoples R China
[3] Hengyang Normal Univ, Hunan Prov Key Lab Funct Met Organ Cpds, Hengyang 421008, Peoples R China
[4] Hengyang Normal Univ, Coll Hunan Prov, Key Lab Organometall New Mat, Hengyang 421008, Peoples R China
[5] Hengyang Normal Univ, Hunan Engn Res Ctr Monitoring & Treatment Heavy Me, Hengyang 421008, Peoples R China
基金
中国国家自然科学基金;
关键词
CMAS corrosion; Alumina based compounds; THERMAL BARRIER COATINGS; MAGNESIUM-ALUMINA-SILICATE; HOT CORROSION; OPTICAL BASICITY; CYCLING BEHAVIOR; DEGREES-C; PART I; DELAMINATION; TEMPERATURE; EVOLUTION;
D O I
10.1016/j.ceramint.2024.01.286
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Alumina based rare earth oxides ceramic materials, with the good performance against the CMAS corrosion, were widely used as the thermal/environmental barrier coatings. In this work, three Y 2 O 3 - Al 2 O 3 binary ceramic bulks, which were the Y 3 Al 5 O 12 , YAlO 3 and Y 4 Al 2 O 9 , were prepared by high temperature solid state reaction using the Y 2 O 3 and Al 2 O 3 as the raw materials. The resistances to CMAS corrosion of these materials at 1250 degrees C and 1350 degrees C were compared fully. The compositions and structures of the samples before and after corrosion were analysed by X-ray diffraction (XRD) and scanning electron microscopy (SEM). Results showed that the different chemical compositions of the materials resulted in the different optical basicity (OB) values which can decide the reactivity of the material with the CMAS melts. The Y 3 Al 5 O 12 ceramic material was inert to the CMAS for its low OB value of 0.75 and damaged seriously by the CMAS through physical penetration. The YAlO 3 and Y 4 Al 2 O 9 with the high OB values of 0.80 and 0.87 reacted with the CMAS to form the Ca 4 Y 6 (SiO 4 ) 6 O. The YAlO 3 ceramic bulk exhibited the good performance against the CMAS corrosion benefitting from the formation of the Ca 4 Y 6 (SiO 4 ) 6 O and the CaAl 2 Si 2 O 8 .
引用
收藏
页码:13721 / 13731
页数:11
相关论文
共 50 条
  • [1] Investigation of CMAS corrosion resistance for gradient Y 2 O 3 stabilized ZrO 2
    Wang, Wei
    Wen, Jiao
    He, Jian
    Cao, Pin
    Li, Chun
    Guo, Hongbo
    Peng, Hui
    SURFACE & COATINGS TECHNOLOGY, 2024, 487
  • [2] CMAS corrosion resistance of YSZ thermal barrier coatings with Al2O3 and YSZ-Al2O3 protective layers
    Ru, Pei-wen
    Hu, Yi
    Yang, Yong
    Zhao, Hong-jian
    Shao, Yu-xuan
    Wang, Yan-wei
    Li, Wei
    Wang, Xing-yu
    Sun, Wen-wei
    Ma, Yu-duo
    CERAMICS INTERNATIONAL, 2024, 50 (21) : 44401 - 44416
  • [3] Hot corrosion behavior of ZrO29.5Y2O35.6Yb2O35.2Gd2O3TBCs in CMAS: CaO-MgO-Al2O3-SiO2
    Bahamirian, M.
    Hadavi, S. M. M.
    Farvizi, M.
    Keyvani, A.
    Rahimipour, M. R.
    JOURNAL OF THE AUSTRALIAN CERAMIC SOCIETY, 2021, 57 (01) : 215 - 224
  • [4] CMAS corrosion behavior of LaMgAl11O19/CeO2 ceramic materials
    Ou, Jiani
    Bin, Xing
    Liu, Zhihua
    Sun, Junbin
    Lu, Weihong
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (06) : 3747 - 3759
  • [5] Outstanding molten calcium-magnesium-aluminosilicate (CMAS) corrosion resistance of directionally solidified Al2O3/Y3Al5O12 eutectic ceramic at 1500 °C
    Sun, Haofei
    Sun, Luchao
    Ren, Xiaomin
    Zhou, Cui
    Li, Jie
    Du, Tiefeng
    Liu, Jing
    Wang, Jingyang
    CORROSION SCIENCE, 2023, 220
  • [6] Influence of Ti3AlC2 additions on CMAS corrosion resistance of porous LaMg Al11O19 abradables
    Huang, Jingqi
    Chen, Wenbo
    Xu, Mingyi
    Deng, Longhui
    Jiang, Jianing
    Dong, Shujuan
    Chen, Meizhu
    Cao, Xueqiang
    CERAMICS INTERNATIONAL, 2024, 50 (24) : 54134 - 54144
  • [7] Effect of P 2 O 5 on nucleation, crystallization and mechanical properties of Y 2 O 3-Al 2 O 3-SiO 2 glasses
    Zheng, Weihong
    Zhang, Hao
    Wang, Qidong
    Yuan, Jian
    Tian, Peijing
    CERAMICS INTERNATIONAL, 2024, 50 (08) : 13467 - 13477
  • [8] Investigation on CMAS corrosion resistance of Sc2O3-Y2O3 co-stabilized ZrO2 thermal barrier coating material by tunable design with Gd-doping
    Zu, J. H.
    Feng, Z.
    Liu, D.
    Gao, Y.
    Luo, W. F.
    Fan, W.
    Lin, M. T.
    Wang, Y.
    Bai, Y.
    CORROSION SCIENCE, 2025, 244
  • [9] Improvement on corrosion resistance of molten calcium-magnesium-alumina-silicate (CMAS) by Yb2O3-Y2O3 co-stabilized ZrO2 ceramic pellets
    Liu, Yangguang
    Liu, Wei
    Wang, Weize
    Zhang, Wenkang
    Yang, Ting
    Li, Kaibin
    Tang, Zhongxiang
    Liu, Chen
    Zhang, Chengcheng
    CORROSION SCIENCE, 2024, 227
  • [10] A New Al2O3-Protected EB-PVD TBC with Superior CMAS Resistance
    Qin, Shiying
    Cao, Huatang
    Gao, Zhaohe
    Brewster, Gyn
    Martin, Joao P.
    Chen, Ying
    Xiao, Ping
    ADVANCED SCIENCE, 2024, 11 (05)