Brazing of high-nitrogen steel to Al0.3CoCrFeNi using a BNi-2 filler: Microstructure, mechanical properties, and corrosion resistance

被引:1
作者
Sun, Hao [1 ,2 ]
Fu, Wei [1 ,2 ]
Song, Xiaoguo [1 ,2 ]
Tian, Xiaoyu [3 ]
Wu, Guangdong [3 ]
Chen, Xiukai [1 ,2 ]
Wang, Huaijin [1 ,2 ]
机构
[1] Harbin Inst Technol, Natl Key Lab Precis Welding & Joining Mat & Struct, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Shandong Prov Key Lab Special Welding Technol, Weihai 264209, Peoples R China
[3] Beijing Inst Control Engn, Beijing 100190, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 31卷
基金
中国国家自然科学基金;
关键词
Al; 0.3; CoCrFeNi; High-nitrogen steel; Brazing; Corrosion; BNi-2; filler; AUSTENITIC STAINLESS-STEEL; ALLOY;
D O I
10.1016/j.jmrt.2024.06.140
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Studies that focus on brazing high-nitrogen steel (HNS) to high-entropy alloys (HEAs) are currently limited. In this study, the HEA Al0.3CoCrFeNi was successfully brazed to HNS using a commercial BNi-2 filler at 1080-1140 degrees C. The microstructure and shear strength of the Al0.3CoCrFeNi/HNS brazed joints were observed and evaluated. The typical microstructure of the brazed joint was HNS/infiltration layer/reaction layer/Ni(s,s) (containing NiAl3)/reaction layer/infiltration layer/Al0.3CoCrFeNi. The higher brazing temperature and longer holding time promoted the diffusion of B as a brazing seam with homogeneous Ni(s,s), and more intergranular Cr-rich borides formed in the base materials. The optimized shear strength attained 549.2 MPa after the joint brazed at 1120 degrees C for 15 min, and ductile fracture occurred in the reaction zone. The insufficient and excessive diffusion of B resulted in residual Cr-B compounds in the brazing seam and excess borides in the HNS, respectively, which negatively affected shear strength. All the joints showed poor corrosion resistance following immersion in a 3.5 wt% NaCl solution because the excess Cr-rich compounds resulted in decreased Cr content in the surrounding matrix. Therefore, Ni-based fillers without B were more suitable for obtaining Al0.3CoCrFeNi/ HNS joints with a favorable corrosion resistance.
引用
收藏
页码:1304 / 1312
页数:9
相关论文
共 50 条
  • [41] Influence of Partial Er Substitution for Sc on the Microstructure, Mechanical Properties and Corrosion Resistance of Short-Processed Al-4.7Mg-0.6Mn-0.3Zr-0.3Sc Sheets
    Lu, Guangxi
    Liang, Yabo
    Xu, Cong
    Rao, Wenfei
    Xue, Yaodong
    Li, Longfei
    Zhang, Li
    Guan, Shaokang
    METALS, 2024, 14 (09)
  • [42] Influence of TiO2 on the Microstructure, Mechanical Properties and Corrosion Resistance of Hydroxyapatite HaP + TiO2 Nanocomposites Deposited Using Spray Pyrolysis
    Dhiflaoui, Hafedh
    Ben Salem, Sarra
    Salah, Mohamed
    Dabaki, Youssef
    Chayoukhi, Slah
    Gassoumi, Bilel
    Hajjaji, Anouar
    Larbi, Ahmed Ben Cheikh
    Amlouk, Mosbah
    Benhayoune, Hicham
    COATINGS, 2023, 13 (07)
  • [43] Microstructure, mechanical, and corrosion resistance properties of Al0.8CrFeCoNiCux high-entropy alloy coatings on aluminum by laser cladding
    Li, Yanzhou
    Shi, Yan
    Olugbade, Emmanuel
    MATERIALS RESEARCH EXPRESS, 2020, 7 (02)
  • [44] Improvement of biocompatible TA9/ZrO2 joint by AuSn20 filler: Interfacial microstructure, mechanical properties, and corrosion resistance
    Chen, Xiukai
    Shi, Bin
    Zhao, Zhenhua
    Long, Fei
    Bian, Hong
    Song, Xiaoguo
    Wang, Zhendong
    Lin, Danyang
    Dai, Jianhong
    CORROSION SCIENCE, 2025, 243
  • [45] Microstructure and mechanical properties of Al0.3FeCoCrNi high entropy alloy processed by laser powder bed fusion using FeCoCrNi and Al powder mixture
    Zhu, Xiangjian
    Wang, Guangchun
    Wang, Xiebin
    Zhao, Guoqun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 848
  • [46] Brazing ZrO2 ceramic to Ti-6Al-4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties
    Cao, J.
    Song, X. G.
    Li, C.
    Zhao, L. Y.
    Feng, J. C.
    MATERIALS CHARACTERIZATION, 2013, 81 : 85 - 91
  • [47] Microstructure and mechanical properties of resistance spot welded dissimilar aluminum/steel joints fabricated using high entropy alloy as interlayer
    Zhou, Kang
    Yu, Wenxiao
    Ren, Baokai
    Wang, Gang
    Yao, Ping
    MATERIALS CHARACTERIZATION, 2024, 216
  • [48] Microstructure and mechanical properties of 17-4 PH stainless steel and Al2O30 ceramic joints brazed with graphene reinforced Ag-Cu-Ti brazing alloy
    Yang, Z. W.
    Yang, J. H.
    Han, Y. J.
    Wang, Y.
    Wang, D. P.
    VACUUM, 2020, 181
  • [49] Influence of cold deformation on microstructure,mechanical properties,and corrosion resistance of high-sulfur free-cutting 316LS stainless steel
    QIANG Shaoming
    WANG Zhiyu
    BaosteelTechnicalResearch, 2018, 12 (03) : 37 - 43
  • [50] The Effect of Ti Content in the Filler Powder on Interfacial Microstructure and Mechanical Properties of C/C Composites/T2-Copper Joints via Thermo-Compensated Resistance Brazing Welding
    Yu, Jiang
    Miao, Xinglin
    Zhang, Hongtao
    Wang, Bo
    Qu, Changming
    METALS, 2022, 12 (05)