Synthesis and Characterization of Poly(butylene glycol adipate-co-terephthalate/diphenylsilanediol adipate-co-terephthalate) Copolyester

被引:3
|
作者
Ge, Tiejun [1 ,2 ]
Wang, Meiyuan [1 ,2 ]
He, Xiaofeng [1 ,2 ]
Yu, Yang [1 ,2 ]
Liu, Xiaofeng [1 ,2 ]
Wen, Bo [3 ]
Liu, Peihan [3 ]
机构
[1] Shenyang Univ Chem Technol, Dept Polymer Sci & Engn, Shenyang 110142, Peoples R China
[2] Liaoning Polymer Mat Engn & Technol Res Ctr, Shenyang 110142, Peoples R China
[3] Liaoning Dongsheng Plast Ind Co Ltd, Yingkou 115003, Peoples R China
关键词
melt polycondensation; diphenylsilanediol; thermal stability; mechanical properties; DEGRADATION; POLYESTERS; FILMS; PBAT;
D O I
10.3390/polym16081122
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The copolyester poly(butylene glycol adipate-co-terephthalate/diphenylsilanediol adipate-co-terephthalate) (PBDAT) was synthesized by the melt polycondensation method using terephthalic acid, adipic acid, 1,4-butanediol, and diphenylsilylene glycol as the raw materials. The molecular chain structure, thermal properties, thermal stability, mechanical properties, and degradation behaviors of the copolyesters were investigated. The results showed that the prepared PBDAT copolyesters exhibited good thermal stability and mechanical properties. With the increase in diphenylsilanediol (DPSD) content, the thermal stability of PBDAT and the melting temperature both increased. The tensile strength and elastic modulus of PBDAT also exhibited an increasing tend. When the DPSD content was 12.5% (PBDAT-12.5), the tensile strength, the elastic modulus, and elongation at break were 30.56 MPa, 238 MPa, and 219%, respectively. With the increase in diphenylsilanediol content, the hydrophilicity of PBDAT decreased, but PBDAT still shows good degradability and the thermal degradation T5% temperature was 355 degrees C. The thermal degradation of PBDAT was also improved.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Nonisothermal Crystallization Kinetics of Poly(butylene adipate-co-terephthalate) Copolyester
    Wang Xiaohui
    Shi Jun
    Chen Ying
    Fu Zhifeng
    Shi Yan
    CHINA PETROLEUM PROCESSING & PETROCHEMICAL TECHNOLOGY, 2012, 14 (01) : 74 - 79
  • [2] Nonisothermal Crystallization Kinetics of Poly(butylene adipate-co-terephthalate) Copolyester
    Wang Xiaohui1
    Shi Jun2
    Chen Ying2
    Fu Zhifeng1
    Shi Yan1(1.State Key Laboratory of Chemical Resource Engineering
    2.Research Institute of PetroChina Liaoyang Petrochemical Company
    ChinaPetroleumProcessing&PetrochemicalTechnology, 2012, 14 (01) : 74 - 79
  • [3] Biodegradable poly(butylene adipate-co-terephthalate) (PBAT)
    Burford, Ty
    Rieg, William
    Madbouly, Samy
    PHYSICAL SCIENCES REVIEWS, 2021, : 1127 - 1156
  • [4] Thermo stabilisation of poly (butylene adipate-co-terephthalate)
    Chaves, Rodrigo Paulino
    Macedo Fechine, Guilhermino Jose
    POLIMEROS-CIENCIA E TECNOLOGIA, 2016, 26 (02): : 102 - 105
  • [5] Characterization and degradation behavior of poly(butylene adipate-co-terephthalate)s
    Herrera, R
    Franco, L
    Rodríguez-Galán, A
    Puiggalí, J
    JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 2002, 40 (23) : 4141 - 4157
  • [6] Synthesis of Bio-Nanomagnetite Using Poly(butylene adipate) and Poly(butylene adipate-co-terephthalate)
    F. Hosseini
    Z. Es’haghi
    Journal of Inorganic and Organometallic Polymers and Materials, 2020, 30 : 4361 - 4371
  • [7] Synthesis of Bio-Nanomagnetite Using Poly(butylene adipate) and Poly(butylene adipate-co-terephthalate)
    Hosseini, F.
    Es'haghi, Z.
    JOURNAL OF INORGANIC AND ORGANOMETALLIC POLYMERS AND MATERIALS, 2020, 30 (11) : 4361 - 4371
  • [8] Characterization of Nanocomposites of Poly(butylene adipate-co-terephthalate) blending with Organoclay
    Chen, Jung-Hung
    Chen, Chin-Chi
    Yang, Ming-Chien
    JOURNAL OF POLYMER RESEARCH, 2011, 18 (06) : 2151 - 2159
  • [9] Characterization of a mesophilic actinobacteria that degrades poly(butylene adipate-co-terephthalate)
    Soulenthone, Phouvilay
    Tachibana, Yuya
    Muroi, Fumihiro
    Suzuki, Miwa
    Ishii, Nariaki
    Ohta, Yukari
    Kasuya, Ken-ichi
    POLYMER DEGRADATION AND STABILITY, 2020, 181
  • [10] Characterization of Nanocomposites of Poly(butylene adipate-co-terephthalate) blending with Organoclay
    Jung-Hung Chen
    Chin-Chi Chen
    Ming-Chien Yang
    Journal of Polymer Research, 2011, 18 : 2151 - 2159