Enhanced rolling contact fatigue property of a rare earth addition bearing steel with a gradient nanostructured surface layer

被引:4
|
作者
Dong, G. S. [1 ,2 ]
Gao, B. [1 ]
Yang, C. Y. [1 ]
Wang, Z. B. [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, 72 Wenhua Rd, Shenyang 110016, Peoples R China
[2] Univ Sci & Technol China, Sch Mat Sci & Engn, 72 Wenhua Rd, Shenyang 110016, Peoples R China
来源
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY | 2025年 / 211卷
关键词
Rare earth addition bearing steel; Surface mechanical rolling treatment; Rolling contact fatigue; Gradient nanostructured; Microcrack; MECHANICAL-PROPERTIES; CRACK INITIATION; STAINLESS-STEEL; BEHAVIOR; MICROSTRUCTURE; PROPAGATION; STRESS; ELEMENTS; IMPACT; LIFE;
D O I
10.1016/j.jmst.2024.06.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Rolling contact fatigue performance is among the most important issues for applications of bearing steels. In this work, a recently developed surface modification technique, surface mechanical rolling treatment, was applied on a rare-earth addition bearing steel. And rolling contact fatigue behavior of treated samples was compared with that of as-received counterparts at different contacting stresses. The results demonstrated that a 700 mu m-thick gradient nanostructured surface layer is produced on samples by surface mechanical rolling treatment. The grain size decreases while the microhardness increases gradually with decreasing depth, reaching -23 nm and -10.2 GPa, respectively, at the top surface. Consequently, the rolling contact fatigue property is significantly enhanced. The characteristic life of treated samples is -3.2 times that of untreated counterparts according to Weibull curves at 5.6 GPa. Analyses of fatigue mechanisms demonstrated that the gradient nanostructured surface layer might not only retard material degradation and microcrack formation, but also prolong the steady-state elastic response stage under rolling contact fatigue. (c) 2024 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:267 / 277
页数:11
相关论文
共 50 条
  • [21] Microstructural evolution and performance change of a carburized nanostructured bainitic bearing steel during rolling contact fatigue process
    Yang, Z. N.
    Ji, Y. L.
    Zhang, F. C.
    Zhang, M.
    Nawaz, B.
    Zheng, C. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 725 : 98 - 107
  • [22] Investigation on rolling contact fatigue of railway wheel steel with surface defect
    Zeng, Dongfang
    Xu, Tian
    Liu, Weidong
    Lu, Liantao
    Zhang, Jiwang
    Gong, Yanhua
    WEAR, 2020, 446 (446-447)
  • [23] Strain-induced formation of a gradient nanostructured surface layer on an ultrahigh strength bearing steel
    K.Zhang
    Z.B.Wang
    JournalofMaterialsScience&Technology, 2018, 34 (09) : 1676 - 1684
  • [24] Strain-induced formation of a gradient nanostructured surface layer on an ultrahigh strength bearing steel
    Zhang, L.
    Wang, Z. B.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 34 (09) : 1676 - 1684
  • [25] Enhanced repeated frictional sliding properties in 304 stainless steel with a gradient nanostructured surface
    Bernoulli, Daniel
    Cao, Shan Cecilia
    Lu, Jian
    Dao, Ming
    SURFACE & COATINGS TECHNOLOGY, 2018, 339 : 14 - 19
  • [26] Rolling contact fatigue property and failure mechanism of carburized 30CrSiMoVM steel at elevated temperature
    Wang, Guanghong
    Qu, Shengguan
    Yin, Lianmin
    Li, Xiaoqiang
    Yue, Wen
    Fu, ZhiQiang
    TRIBOLOGY INTERNATIONAL, 2016, 98 : 144 - 154
  • [27] New microstructure of butterfly white etching area in rolling contact fatigue of bearing steel
    Wang, Yi-Bo
    Li, Shu-Xin
    Lu, Si-Yuan
    Cao, Jun
    TRIBOLOGY INTERNATIONAL, 2023, 188
  • [28] Influence of Cu nanofluids on the rolling contact fatigue life of bearing steel
    Thapliyal, Prashant
    Thakre, Gananath D.
    ENGINEERING FAILURE ANALYSIS, 2017, 78 : 110 - 121
  • [29] Evaluation of the influencing factors of combined surface modification on the rolling contact fatigue performance and crack growth of AISI 52100 steel
    Duan, Chenfeng
    Qu, Shengguan
    Hu, Xiongfeng
    Jia, Siyu
    Li, Xiaoqiang
    WEAR, 2022, 494-495
  • [30] Enhanced Impact Toughness of Previously Cold Rolled High-Carbon Chromium Bearing Steel with Rare Earth Addition
    Dong, Zhaohua
    Qian, Dongsheng
    Yin, Fei
    Wang, Feng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (11) : 8178 - 8187