High-Resolution Ultrasound to Quantify Sub-Surface Wrinkles in a Woven CFRP Laminate

被引:3
作者
Amif, Md Admay [1 ]
Jack, David A. [1 ]
机构
[1] Baylor Univ, Dept Mech Engn, Waco, TX 76706 USA
关键词
woven fiber carbon composite; out-of-plane wrinkle; conventional ultrasound; A-scan; peak tracking; ELASTIC PROPERTIES; COMPOSITE;
D O I
10.3390/ma17092002
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Carbon fiber reinforced polymer (CFRP) composites are popular materials in the aerospace and automotive industries because of their low weight, high strength, and corrosion resistance. However, wrinkles or geometric distortions in the composite layers significantly reduce their mechanical performance and structural integrity. This paper presents a method for non-destructively extracting the three-dimensional geometry, lamina by lamina, of a laminated composite. A method is introduced for fabricating consistent out-of-plane wrinkled CFRP laminate panels, simulating the in-service wrinkle observed in industries that utilize thick structure composites such as the vertical lift or wind power industries. The individual lamina geometries are extracted from the fabricated coupon with an embedded wrinkle from captured ultrasonic waveforms generated from single-element conventional ultrasonic (UT) scan data. From the extracted waveforms, a method is presented to characterize the wrinkle features within each individual lamina, specifically the spatially varying wrinkle height and intensity for the wrinkle. Parts were fabricated with visibly undetectable wrinkles using a wet layup process and a hot press for curing. Scans were performed in a conventional immersion tank scanning system, and the scan data were analyzed for wrinkle detection and characterization. Extraction of the layers was performed based on tracking the voltage peaks from A-scans in the time domain. Spatial Gaussian averaging was performed to smooth the A-scans, from which the surfaces were extracted for each individual lamina. The extracted winkle surface aligned with the anticipated wrinkle geometry, and a single parameter for quantification of the wrinkle intensity for each lamina is presented.
引用
收藏
页数:11
相关论文
共 27 条
  • [11] Wrinkle Detection in Carbon Fiber-Reinforced Polymers Using Linear Phase FIR-Filtered Ultrasonic Array Data
    Ma, Tengfei
    Li, Yang
    Zhou, Zhenggan
    Meng, Jia
    [J]. AEROSPACE, 2023, 10 (02)
  • [12] Minnie W.H., 2021, Masters Thesis
  • [13] Nargis R.A., Automated Detection of Foreign Object Debris in Woven Carbon Fiber Laminate at Different Environmental Conditions
  • [14] Fibre direction and stacking sequence measurement in carbon fibre composites using Radon transforms of ultrasonic data
    Nelson, L. J.
    Smith, R. A.
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2019, 118 : 1 - 8
  • [15] Ozkan D., 2020, Engineering Design Applications III: Structures, Materials and Processes, P235
  • [16] Detection of Fibre Waviness Using Ultrasonic Array Scattering Data
    Pain, Damien
    Drinkwater, Bruce W.
    [J]. JOURNAL OF NONDESTRUCTIVE EVALUATION, 2013, 32 (03) : 215 - 227
  • [17] The Use of CFRP for Structural Reinforcement-Literature Review
    Pawlak, Aleksandra M.
    Gorny, Tomasz
    Dopierala, Lukasz
    Paczos, Piotr
    [J]. METALS, 2022, 12 (09)
  • [18] A statistical approach for failure analysis involving uncertainty in determining ply orientation
    Rahul, Kirtunia
    Jack, David A.
    Smith, Douglas E.
    [J]. POLYMER COMPOSITES, 2024, 45 (06) : 5192 - 5206
  • [19] Sandhu A., 2016, P 17 EUR C COMP MAT, P9
  • [20] Schmerr LW., 1998, Fundamentals of ultrasonic nondestructive evaluation-a modeling approach