Effect of Ladle Washing Operation on Non-metallic Inclusions in Tire Cord Steel: Laboratory Simulation

被引:1
作者
Song, Guodong [1 ,2 ]
Deng, Zhiyin [1 ,2 ]
Zhu, Miaoyong [1 ,2 ]
机构
[1] Northeastern Univ, Key Lab Ecol Met Multimet Mineral, Minist Educ, Shenyang 110819, Peoples R China
[2] Northeastern Univ, Sch Met, Shenyang 110819, Peoples R China
来源
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE | 2024年 / 55卷 / 04期
关键词
CHEMICAL-REACTION; SLAG; GLAZE; AGGLOMERATION; EVOLUTION;
D O I
10.1007/s11663-024-03143-w
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to simulate ladle exchange in secondary steelmaking, MgO refractory rods with different apparent porosities (2.67 pct and 0.70 pct) were glazed by CaO-Al2O3 system slag (R = w(CaO)/w(SiO2) = 5.5, w(Al2O3) = 30 pct) and CaO-SiO2 system slag (R = 1.0, w(Al2O3) = 2 pct), respectively, and the interaction between the glazed rods and tire cord steel grade LX72A was investigated at 1823 K (1550 degrees C) in laboratory. By using BaO as a tracer of glaze, it was found that ladle glaze is also a source of inclusions in tire cord steel. The direct flush-off of CaO-Al2O3 system glaze and its impact on the rise of the Al content (up to 15 ppm) in liquid steel are not conducive to the plasticity of inclusions. Besides, the structure of the refractory rods influences the effect of glaze evidently. Initial glaze can penetrate into the pores of the refractory, and it can hardly be washed out by the glazes formed in the following heats. Therefore, it is difficult to avoid the negative impact of the penetrated high Al2O3 slag on inclusions. Although dense refractory (apparent porosity 0.70 pct) could restrain slag penetration and weaken the negative effect of high Al2O3 slags, the refractory used in industry is much looser than that in laboratory. In this case, specialized ladles at a suitable age with pure and dense lining are recommended for the refining process of high-end tire cord steel grades.
引用
收藏
页码:2805 / 2816
页数:12
相关论文
共 50 条
[41]   Effect of rare earth lanthanum on non-metallic inclusions in Fe-Mn-C-Al alloy [J].
Zhang, Ze-Zhong ;
Zhuang, Chang-Ling ;
Xiang, Jiang-Hua ;
Hu, Zhong-Jie .
CANADIAN METALLURGICAL QUARTERLY, 2024,
[42]   Metallurgical Model of Diffusible Hydrogen and Non-Metallic Slag Inclusions in Underwater Wet Welding of High-Strength Steel [J].
Parshin, Sergey G. ;
Levchenko, Alexey M. ;
Maystro, Alexey S. .
METALS, 2020, 10 (11) :1-17
[43]   Formation and Evolution of Non-Metallic Inclusions in Calcium Treatment H13 Steel during Electroslag Remelting Process [J].
Wang, Hao ;
Li, Jing ;
Shi, Chengbin ;
Qi, Yongfeng ;
Dai, Yuxiang .
ISIJ INTERNATIONAL, 2019, 59 (05) :828-838
[44]   Effect of Non-metallic Inclusions in Fe-Al-Ti-O-N-S Alloy on Grain Size [J].
Choi, Wonjin ;
Matsuura, Hiroyuki ;
Tsukihashi, Fumitaka .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2016, 47 (03) :1851-1857
[45]   ORIGIN AND EVOLUTION OF NON-METALLIC INCLUSIONS FOR Al-KILLED STEEL DURING EAF-LF-VD-CC PROCESS [J].
Tang Hai-yan ;
Guo Xiao-chen ;
Cheng Peng-fei ;
Liang Yong-cang ;
Li Jing-she ;
Zhao Baojun .
7TH INTERNATIONAL SYMPOSIUM ON HIGH-TEMPERATURE METALLURGICAL PROCESSING, 2016, :271-278
[46]   Role of Synthetic Slag Treatment on the Morphology of Non-Metallic Inclusions and Subsequent Cold Drawability of the High Carbon Wire Rod Steel [J].
Srivastava, Alok ;
Kamaraj, Ashok ;
Mandal, Durbadal ;
Mondal, K. ;
Mandal, Gopi K. .
METALS AND MATERIALS INTERNATIONAL, 2022, 28 (07) :1763-1777
[47]   Comparison of Sub-rapid Solidification and Lower Cooling Rates on Non-metallic Inclusions in Molten Steel and Its Transformation Mechanism [J].
Li, Rensheng ;
Liu, Ligang ;
Zhou, You ;
Lyu, Peisheng ;
Wang, Wanlin ;
Liang, Yutian ;
Xie, Boquan .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2025,
[48]   Effect of Al2O3 on Evolution of Oxide Inclusions in Tire Cord Steel during Hot Rolling [J].
Niu, Kaijun ;
Conejo, Alberto N. .
ISIJ INTERNATIONAL, 2021, 61 (10) :2605-2612
[49]   In Situ Observations of Agglomeration of Non-metallic Inclusions at Steel/Ar and Steel/Slag Interfaces by High-Temperature Confocal Laser Scanning Microscope: A Review [J].
Mu, Wangzhong ;
Dogan, Neslihan ;
Coley, Kenneth S. .
JOM, 2018, 70 (07) :1199-1209
[50]   Effect of continuous casting speed on mold surface flow and the related near-surface distribution of non-metallic inclusions [J].
Fei, Peng ;
Min, Yi ;
Liu, Cheng-jun ;
Jiang, Mao-fa .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2019, 26 (02) :186-193