Effect of wheel speed on the microstructure and magnetic properties of Fe-3.0 wt %Si non-oriented silicon steel ultra-thin ribbons prepared by planar flow casting

被引:4
|
作者
Cheng, Yuanyao [1 ]
Bao, Siqian [1 ,2 ]
Liu, Chen [1 ]
Hu, Jiarui [1 ]
Xu, Deming [1 ,2 ]
Chang, Jiaqi [1 ]
Guo, Rui [1 ]
Fan, Xi 'an [1 ,2 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Peoples R China
[2] Wuhan Univ Sci & Technol, Minist Educ, Key Lab Ferrous Met & Resources Utilizat, Wuhan 430081, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 30卷
关键词
Planar flow casting; Fe-3.0 wt %Si; Ultra-thin ribbons; Microstructure; Magnetic properties;
D O I
10.1016/j.jmrt.2024.03.220
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Using the planar flow casting method to prepare ultra-thin silicon steel ribbons is an eco-friendly and efficient production method. However, the poor wettability between silicon steel and copper result in difficulties in formability by planar flow casting, which limits its application in production of silicon steel ultra-thin ribbons. The process parameters of planar flow casting are the key factors affecting the formability and magnetic properties of non-oriented silicon steel ribbons, in which the wheel speed determines the solidification rate of the silicon steel melt, which has an important influence on the surface quality and magnetic properties of silicon steel ultra-thin ribbons. Therefore, in this paper, the effect of wheel speed on microstructures and magnetic properties of Fe-3.0 wt %Si alloy are systematically investigated. The results indicate that as the wheel speed increases, the grain size and thickness gradually decrease. When the wheel speed is between 10 and 15 m/s, the surface of the ribbons is relatively flat. As the wheel speed increases, the surface quality of ribbons gradually deteriorates. The ribbons were in fragment with the wheel speed of 35 m/s. Compared with the ribbons before annealing, the magnetic induction B50 increased significantly and the iron losses P1.0/400 decreased sharply at 400 Hz after annealing. The magnetic induction of the ribbons after annealing with the wheel speed of 10 m/s reaches to 1.628 T as the wheel speed is 10 m/s with the corresponding iron loss is 16.171 W/kg. The lower lamination factor and micropores of the ribbons may cause the poorer magnetic properties.
引用
收藏
页码:2140 / 2146
页数:7
相关论文
共 32 条
  • [1] Effect of phosphorus content on microstructure and magnetic/mechanical properties of ultra-thin non-oriented Fe-3%Si ribbons prepared with planar flow casting
    Liu, Zhixiang
    Xu, Deming
    Bao, Siqian
    Yang, Gengwei
    Chang, Qingming
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 35 : 5362 - 5376
  • [2] Effect of Normalizing Treatment on Microstructure and Mechanical Properties of Non-oriented Fe-3.0% Si Steel
    Xu, Cheng
    Xu, Haijie
    Shu, Xuedao
    Lu, Xubeng
    Jiang, Lulan
    Li, Zixuan
    Zhang, Yuanxiang
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [3] Analysis of the microstructure, texture and magnetic properties of strip casting 4.5 wt.% Si non-oriented electrical steel
    Zu, Guoqing
    Zhang, Xiaoming
    Zhao, Jingwei
    Cui, Yi
    Wang, Yuqian
    Jiang, Zhengyi
    MATERIALS & DESIGN, 2015, 85 : 455 - 460
  • [4] Microstructure and texture evolution of strip casting 3 wt% Si non-oriented silicon steel with columnar structure
    Liu, Haitao
    Liu, Zhenyu
    Cao, Guangming
    Li, Chenggang
    Wang, Guodong
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2011, 323 (21) : 2648 - 2651
  • [5] Effect of rolling process on magnetic properties of Fe-3.3 wt% Si non-oriented electrical steel
    Du, Yizhou
    O'Malley, Ronald J.
    Buchely, M. F.
    Kelly, Paul
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2022, 128 (09):
  • [6] Effect of Cooling Rate on Magnetic Properties of Fe-3.3 wt% Si Non-oriented Electrical Steel
    Du, Yizhou
    O'Malley, Ronald J.
    Buchely, M. F.
    METALS AND MATERIALS INTERNATIONAL, 2022, 28 (12) : 3160 - 3171
  • [7] Effect of Cooling Rate on Magnetic Properties of Fe-3.3 wt% Si Non-oriented Electrical Steel
    Yizhou Du
    Ronald J. O’Malley
    M. F. Buchely
    Metals and Materials International, 2022, 28 : 3160 - 3171
  • [8] Effects of rolling temperature on microstructure, texture, formability and magnetic properties in strip casting Fe-6.5 wt% Si non-oriented electrical steel
    Liu, Hai-Tao
    Li, Hao-Ze
    Li, Hua-Long
    Gao, Fei
    Liu, Guo-Huai
    Luo, Zhong-Han
    Zhang, Feng-Quan
    Chen, Sheng-Lin
    Cao, Guang-Ming
    Liu, Zhen-Yu
    Wang, Guo-Dong
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2015, 391 : 65 - 74
  • [9] Effect of Normalizing Temperature on Microstructure, Texture and Magnetic Properties of Non-Oriented Silicon Steel
    Zhou, Changcheng
    Luan, Shenteng
    Qiao, Jialong
    Wang, Haijun
    METALS, 2025, 15 (02)
  • [10] Effect of rolling reduction on microstructure, texture and magnetic properties of twin-roll casting non-oriented 6.5 wt% Si electrical steel
    Li, Haoze
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2022, 546