In situ study on the tensile deformation in high-density polyethylene/ hexagonal boron nitride composite

被引:2
作者
Liu, Yi [1 ]
Feng, Yao [1 ]
Li, Zichao [1 ]
Lu, Ying [2 ]
Su, Fengmei [1 ]
机构
[1] Zhengzhou Univ, Coll Mat Sci & Engn, Natl Engn Res Ctr Adv Polymer Proc Technol, Key Lab Mat Proc & Mold,Minist Educ, Zhengzhou 450002, Peoples R China
[2] Chinese Acad Sci, Changchun Inst Appl Chem, State Key Lab Polymer Phys & Chem, Changchun 130022, Peoples R China
基金
中国国家自然科学基金;
关键词
High density polyethylene; Hexagonal boron nitride; Tensile deformation; In-situ WAXD and SAXS measurement; HOT-STRETCHING PROCESS; SHISH-KEBAB; NEUTRON-SCATTERING; CRYSTAL SLIP; DRAWN FIBERS; ETHYLENE COPOLYMERS; PLASTIC-DEFORMATION; FIBRILLAR CRYSTALS; TEMPERATURE; RELAXATION;
D O I
10.1016/j.polymer.2024.126865
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Tensile deformation in the post processing of polymer plays a critical role in determining its mechanical properties. In this work, we investigated the structure evolution of high-density polyethylene/hexagonal boron nitride (HDPE/h-BN) composite during stretching in a wide temperature range from 25 degrees C to 100 degrees C in order to reveal the suitable post processing temperature of HDPE/h-BN composites fiber. The structure transition of HDPE crystal and the distribution of h-BN were investigated by in-situ small-angle X-ray scattering (SASX), in-situ wideangle X-ray diffraction (WAXD) measurements, and scanning electron microscopy (SEM). The result shows that the parent HDPE crystal would be broken and recrystallize into highly oriented daughter crystal along the tensile direction when the tensile temperature (Tten) is in the range from 70 degrees C to 100 degrees C, though the recrystallization rate is low at high Tten. When Tten is low (25 degrees C), the crystallinity decreases continuously as no recrystallization takes place. In addition, the h-BN migrates accompany with the HDPE matrix and becomes oriented during the tensile direction. Combining the result of WAXD, SAXS, and the SEM measurement, it is concluded that the temperature of 70 degrees C is suitable for post processing of the HDPE/h-BN composite fiber.
引用
收藏
页数:8
相关论文
共 70 条
[41]   FOLDED CHAIN MODEL OF HIGHLY DRAWN POLYETHYLENE [J].
PETERLIN, A .
POLYMER ENGINEERING AND SCIENCE, 1969, 9 (03) :172-&
[42]   FOLDED CHAIN CONCEPT OF FIBER STRUCTURE [J].
PETERLIN, A .
KOLLOID-ZEITSCHRIFT AND ZEITSCHRIFT FUR POLYMERE, 1967, 216 (MAR) :129-&
[44]   STRUCTURE OF DRAWN FIBERS .3. NEUTRON-SCATTERING STUDIES OF POLYETHYLENE FIBERS DRAWN BEYOND THE NECK [J].
SADLER, DM ;
BARHAM, PJ .
POLYMER, 1990, 31 (01) :46-50
[45]   STRUCTURE OF DRAWN FIBERS .2. NEUTRON-SCATTERING AND NECKING IN SINGLE-CRYSTAL MATS OF POLYETHYLENE [J].
SADLER, DM ;
BARHAM, PJ .
POLYMER, 1990, 31 (01) :43-45
[46]   STRUCTURE OF DRAWN FIBERS .1. NEUTRON-SCATTERING STUDIES OF NECKING IN MELT-CRYSTALLIZED POLYETHYLENE [J].
SADLER, DM ;
BARHAM, PJ .
POLYMER, 1990, 31 (01) :36-42
[47]   Plastic deformation of polyethylene and ethylene copolymers - Part I homogeneous crystal slip and molecular mobility [J].
Seguela, R ;
Gaucher-Miri, V ;
Elkoun, S .
JOURNAL OF MATERIALS SCIENCE, 1998, 33 (05) :1273-1279
[48]   Plastic deformation of polyethylene and ethylene copolymers - Part II Heterogeneous crystal slip and strain-induced phase change [J].
Seguela, R ;
Elkoun, S ;
Gaucher-Miri, V .
JOURNAL OF MATERIALS SCIENCE, 1998, 33 (07) :1801-1807
[49]   On the natural draw ratio of semi-crystalline polymers:: Review of the mechanical, physical and molecular aspects [J].
Seguela, Roland .
MACROMOLECULAR MATERIALS AND ENGINEERING, 2007, 292 (03) :235-244
[50]  
Seguela R, 2007, E-POLYMERS