Effect of Welding Thermal Cycling on Microstructures and Cryogenic Impact Toughness of Medium-Mn Low-Temperature Steel

被引:0
作者
Sun, Qing [1 ]
Du, Yu [2 ]
Wang, Xiaonan [2 ]
Liu, Tao [1 ]
Tao, Zhen [1 ]
Li, Lei [1 ]
Liao, Zhihui [1 ]
Du, Linxiu [1 ]
机构
[1] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
[2] Soochow Univ, Sch Iron & Steel, Suzhou 215021, Peoples R China
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2024年 / 55卷 / 10期
关键词
MEDIUM-MANGANESE STEEL; HEAT-AFFECTED ZONE; MECHANICAL-PROPERTIES; REVERSED AUSTENITE; RETAINED AUSTENITE; GRAIN-SIZE; STABILITY; STRENGTH; COMBINATION; DUCTILITY;
D O I
10.1007/s11661-024-07521-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work studied the effect of welding thermal cycling on the microstructures and cryogenic impact toughness of medium-Mn low-temperature steel by single-pass welding thermal simulation test. The microstructures of the heat-affected zone (HAZ) were characterized by optical microscopy, electron backscatter diffraction, X-ray diffraction, and transmission electron microscopy. The results indicated that the microstructures of fine-grain HAZ are fine-lath martensite with film-like retained austenite in the heat input range of 10 similar to 30 kJ/cm. Meanwhile, fine-grain HAZ has excellent low-temperature impact toughness, and the impact energy tested at - 40 degrees C can reach about 245 J. The coarse martensitic packet and block in the coarse grain HAZ seriously deteriorated the cryogenic impact toughness, and the greater the heat input, the worse the cryogenic impact toughness. The impact energy tested at - 40 degrees C was 71 J when the heat input was 10 kJ/cm. The cryogenic impact toughness of HAZ gradually deteriorated with the peak temperature increase because of the decrease of retained austenite content and the increase of martensitic lath width.
引用
收藏
页码:3869 / 3882
页数:14
相关论文
共 30 条
[21]   Stabilization mechanisms of retained austenite in transformation-induced plasticity steel [J].
Wang, JJ ;
van der Zwaag, S .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2001, 32 (06) :1527-1539
[22]   Improvement in toughness and ductility of friction stir welded medium-Mn steel joint via post-welding annealing [J].
Wang, Y. Q. ;
Duan, R. H. ;
Hu, J. ;
Luo, Z. A. ;
Ma, Z. Y. ;
Xie, G. M. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2022, 306
[23]  
Wu DY., 2015, METALL MATER TRANS A, V46A, P8842
[24]   Correlation between deformation behavior and austenite characteristics in a Mn-Al type TRIP steel [J].
Xu, Y. B. ;
Zou, Y. ;
Hu, Z. P. ;
Han, D. T. ;
Chen, S. Q. ;
Misra, R. D. K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 698 :126-135
[25]  
Xuming Wang, 2021, International Journal of Microstructure and Materials Properties, P356, DOI [10.1504/ijmmp.2021.121637, 10.1504/IJMMP.2021.121637]
[26]   Austenite grain size and the martensite-start temperature [J].
Yang, Hong-Seok ;
Bhadeshia, H. K. D. H. .
SCRIPTA MATERIALIA, 2009, 60 (07) :493-495
[27]  
Yi HJ., 2022, WELD TECHNIQUE, V51, P57
[28]   Correlation between microstructure and mechanical properties of heat affected zones in Fe-8Mn-0.06C steel welds [J].
Yoo, Jaehong ;
Han, Kyutae ;
Park, Younghwan ;
Lee, Changhee .
MATERIALS CHEMISTRY AND PHYSICS, 2014, 146 (1-2) :175-182
[29]   Microstructure and toughness of the CGHAZ of an offshore platform steel [J].
Zhou, Yanlei ;
Jia, Tao ;
Zhang, Xiangjun ;
Liu, Zhenyu ;
Misra, R. D. K. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2015, 219 :314-320
[30]   Austenite stability and its effect on the toughness of a high strength ultra-low carbon medium manganese steel plate [J].
Zou, Y. ;
Xu, Y. B. ;
Hu, Z. P. ;
Gu, X. L. ;
Peng, F. ;
Tan, X. D. ;
Chen, S. Q. ;
Han, D. T. ;
Misra, R. D. K. ;
Wang, G. D. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 675 :153-163