The precipitation evolution and mechanical properties of an Al-Cu-Li-Mg alloy during natural aging

被引:17
作者
Deng, San -Xi [1 ]
Liu, Zhen-zhen [1 ]
Zeng, Guang-jun [1 ]
Xiang, Hui [1 ]
Ma, Peng-cheng [2 ]
Yin, Jia-ming [2 ]
Kang, Li [2 ]
Wen, Si-han [2 ]
Li, Jin-feng [1 ]
Liu, Dan -Yang [1 ]
机构
[1] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Peoples R China
[2] Aerosp Res Inst Mat & Proc Technol, Beijing 100076, Peoples R China
来源
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY | 2024年 / 192卷
关键词
Al-Cu-Li-Mg alloy; Precipitation evolution; Mechanical properties; Natrual aging; HAADF-STEM; MINOR SOLUTE ADDITIONS; STRENGTHENING MECHANISMS; ALUMINUM; KINETICS; AG; MICROSTRUCTURE; PHASE; QUANTIFICATION; DISLOCATIONS; PROPAGATION;
D O I
10.1016/j.jmst.2023.12.050
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The precipitation evolution and mechanical properties of a commercial Al -Cu -Li -Mg alloy in natural aging (NA) tempers (T3 and T4) were investigated in detail. It was demonstrated that GPI zones were the predominant precipitate throughout the NA process. In the T3 -aged sample, the precipitation sequence was determined: supersaturated solid solution (SSSS) -> atom clusters -> GPI zones, whereas in the T4 -aged sample, it was SSSS -> atom clusters -> GPI zones -> GPI zones + 8 ' /GPI zones/ 8 ' . For samples without NA, the strength of the T3 sample was 76.0 MPa higher than that in the T4 sample, which was attributed to the pre -deformation -introduced dislocations. During the early stage of NA, GPI zone nucleation was substantially restricted in the T3 sample, resulting in a much lower number density of GPI zones. It retarded the aging response and strength improvement, consequently narrowing the strength difference between T3 and T4 samples. As the NA process progressed, the average diameter of GPI zones in the T4 sample increased to approximately 4.5 nm, accompanied by the formation of 8 ' /GPI zones/ 8 ' composite precipitate. However, GPI zone growth and 8 ' /GPI zones/ 8 ' composite precipitate formation were significantly inhibited in the T3 sample, as evidenced by its much smaller average diameter of approximately 2.1 nm and the absence of composite precipitates. It inhibited the strength improvement of the T3 sample. Therefore, after a long period (5 months) of NA, the strength of the T4 sample was about 13.0 MPa higher than that of the T3 samples, instead. (c) 2024 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:42 / 53
页数:12
相关论文
共 62 条
[1]   Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: A review [J].
Abd El-Aty, Ali ;
Xu, Yong ;
Guo, Xunzhong ;
Zhang, Shi-Hong ;
Ma, Yan ;
Chen, Dayong .
JOURNAL OF ADVANCED RESEARCH, 2018, 10 :49-67
[2]   Coupled precipitation and yield strength modelling for non-isothermal treatments of a 6061 aluminium alloy [J].
Bardel, D. ;
Perez, M. ;
Nelias, D. ;
Deschamps, A. ;
Hutchinson, C. R. ;
Maisonnette, D. ;
Chaise, T. ;
Gamier, J. ;
Bourlier, F. .
ACTA MATERIALIA, 2014, 62 :129-140
[3]   Yield strength modeling of an Al-Cu-Li alloy through circle rolling and flow stress superposition approach [J].
Bharti, Purnima ;
Singh, Ripudaman ;
Sahoo, Jyoti Ranjan ;
Tripathi, Aparna ;
Mishra, Sumeet .
JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 964
[4]   Pre-straining to improve the bake hardening response of a twin-roll cast Al-Mg-Si alloy [J].
Birol, Y .
SCRIPTA MATERIALIA, 2005, 52 (03) :169-173
[5]   Transforming solid-state precipitates via excess vacancies [J].
Bourgeois, Laure ;
Zhang, Yong ;
Zhang, Zezhong ;
Chen, Yiqiang ;
Medhekar, Nikhil, V .
NATURE COMMUNICATIONS, 2020, 11 (01)
[6]   Structure and energetics of the coherent interface between the θ′ precipitate phase and aluminium in Al-Cu [J].
Bourgeois, Laure ;
Dwyer, Christian ;
Weyland, Matthew ;
Nie, Jian-Feng ;
Muddle, Barrington C. .
ACTA MATERIALIA, 2011, 59 (18) :7043-7050
[7]   Portevin-Le Chatelier effect in Al-Zn-Mg-Cu-Zr aluminum alloy [J].
Chen Jun-zhou ;
Zhen Liang ;
Fan Li-wei ;
Yang Shou-jie ;
Dai Sheng-long ;
Shao Wen-zhu .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2009, 19 (05) :1071-1075
[8]   Microstructure evolution and shearing behaviour of δ′/θ′/δ′ precipitates in an aged Al-Cu-Li-Mg aluminium alloy [J].
Chung, Tsai-Fu ;
Lin, Shan-Qiao ;
Li, Hongxing ;
Hsiao, Chien-Nan ;
Yang, Jer-Ren ;
Tsao, Cheng-Si ;
Ohmura, Takahito .
JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 953
[9]   Precipitation behavior of an Al-Cu-Li-X alloy and competing relationships among precipitates at different aging temperatures [J].
Cui, Shuai ;
Zhang, Cunsheng ;
Liu, Mingfu ;
Chen, Liang ;
Zhao, Guoqun .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 814 (814)
[10]   The influence of Cu/Li ratio on precipitation in Al-Cu-Li-x alloys [J].
Decreus, B. ;
Deschamps, A. ;
De Geuser, F. ;
Donnadieu, P. ;
Sigli, C. ;
Weyland, M. .
ACTA MATERIALIA, 2013, 61 (06) :2207-2218