Room temperature tensile creep behavior of Mg-6Zn-0.4Mn-0.3Al-0.2Ca (wt%) alloy containing icosahedral quasicrystals

被引:1
作者
Ying, Yu-Lei [1 ,2 ]
Guan, Zhi-Ping [1 ,2 ]
Wang, Xuan [1 ,2 ]
Wang, Gang [3 ]
Yan, Wei [4 ]
机构
[1] Jilin Univ, Key Lab Automobile Mat, Minist Educ, Nanling Campus,5988 Renmin St, Changchun 130025, Peoples R China
[2] Jilin Univ, Sch Mat Sci & Engn, Nanling Campus,5988 Renmin St, Changchun 130025, Peoples R China
[3] FAW Tooling Die Mfg Co Ltd, Res & Dev Dept, Changchun 130000, Jilin, Peoples R China
[4] FAW Tooling Die Mfg Co Ltd, Prod Dev Dept, Changchun 130000, Jilin, Peoples R China
来源
MATERIALS TODAY COMMUNICATIONS | 2024年 / 39卷
基金
中国国家自然科学基金;
关键词
Magnesium alloy; Creep mechanism; Dislocation; Quasicrystal; Room temperature; ZN-Y ALLOYS; DEFORMATION-BEHAVIOR; THRESHOLD STRESSES; NONBASAL SLIP; IN-SITU; MAGNESIUM; CA; TEXTURE; MICROSTRUCTURE; PRECIPITATION;
D O I
10.1016/j.mtcomm.2024.108602
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The poor creep resistance at room temperature is the critical issue limiting magnesium (Mg) alloys to be structural components in engineering fields. In this study, we designed a novel Mg-6Zn-0.4Mn-0.3Al-0.2Ca (ZMAX6000) alloy, which had superior creep properties at room temperature, and the steady creep rate of ZMAX6000 (2.52x10(-9) s(-1)) alloy was one order of magnitude lower than that of pure Mg (5.0x10(-8) s(-1)) and AZ31 alloy (1.5x10(-8) s(-1)), when the creep stress is equivalent to the 0.8 yield stress (YS). The ZMAX6000 alloy featured icosahedral quasicrystal phases (I-phases) distributed at almost all triangular grain boundaries. The room temperature creep threshold stress (sigma(0)) and stress exponent (n) for the I-phase enhanced ZMAX6000 alloy were sigma(0) = 209 MPa and n = 4.9, respectively. I-phases can act as barriers to grain boundary sliding, and the high-density nanoscale second phases inside the grains can impede the dislocation slip. Consequently, the ZMAX6000 alloy exhibits excellent creep properties at room temperature. The cross-slip consisting of basal < a > dislocation and prismatic < a > dislocation, as well as the pyramidal <c + a> slip are the main creep mechanisms of the ZMAX6000 alloy at room temperature.
引用
收藏
页数:8
相关论文
共 34 条
  • [21] Role of extrusion rate on the microstructure and tensile properties evolution of ultrahigh-strength low-alloy Mg-1.0Al-1.0Ca-0.4Mn (wt.%) alloy
    Liu, X. Q.
    Qiao, X. G.
    Pei, R. S.
    Chi, Y. Q.
    Yuan, L.
    Zheng, M. Y.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2023, 11 (02) : 553 - 561
  • [22] Influence of loading path and precipitates on indentation creep behavior of wrought Mg-6 wt% Al-1 wt% Zn magnesium alloy
    Nautiyal, Pranjal
    Jain, Jayant
    Agarwal, Arvind
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 650 : 183 - 189
  • [23] Deteriorated tensile creep resistance of a high-pressure die-cast Mg-4Al-4RE-0.3Mn alloy induced by substituting part RE with Ca
    Yang, Qiang
    Qiu, Xin
    Lv, Shuhui
    Meng, Fanzhi
    Guan, Kai
    Li, Baishun
    Zhang, Deping
    Zhang, Yaqin
    Liu, Xiaojuan
    Meng, Jian
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 716 : 120 - 128
  • [24] Room-temperature stretch formability, tensile properties, and microstructures of precipitation hardenable Mg-6Zn-0.2Ca (mass%) alloy sheets micro-alloyed with Ce or Y
    Nakata, T.
    Li, Z. H.
    Sasaki, T. T.
    Hono, K.
    Kamado, S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 804
  • [25] High-Temperature Mechanical Behavior of an As-Extruded Al-5Zn-2Mg-0.3Cu (in wt.%) Alloy
    Lu, Cuilan
    Xu, Daokui
    Zhang, Lan
    Wang, Shuo
    Xu, Xiangbo
    Wang, Dongliang
    COATINGS, 2023, 13 (10)
  • [26] Development of extruded Mg-6Er-3Y-1.5Zn-0.4Mn (wt.%) alloy with high strength at elevated temperature
    Zhang, Mingquan
    Feng, Yan
    Zhang, Jinghuai
    Liu, Shujuan
    Yang, Qiang
    Liu, Zhuang
    Li, Rongguang
    Meng, Jian
    Wu, Ruizhi
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 35 (10) : 2365 - 2374
  • [27] Large hardening response mediated by room-temperature dynamic solute clustering behavior in a dilute Mg-Zn-Ca-Sn-Mn alloy
    Hua, Zhen-Ming
    Wang, Cheng
    Wang, Tian-Shuai
    Du, Chunfeng
    Jin, Shen-Bao
    Sha, Gang
    Gao, Yipeng
    Jia, Hai -Long
    Zha, Min
    Wang, Hui -Yuan
    ACTA MATERIALIA, 2022, 240
  • [28] Effects of ultrasonic treatment on the tensile properties and microstructure of twin roll casting Mg-3%Al-1%Zn-0.8%Ce-0.3%Mn (wt%) alloy strips
    Zhao, Jun
    Yu, Kun
    Xue, Xinying
    Mao, Daheng
    Li, Jianping
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (34) : 8607 - 8613
  • [29] Effect of minor Sc addition on high temperature tensile behavior of Al-7Zn-2Mg-2Cu-0.2Zr alloy
    Lang, Mo
    Zhao, Ning
    Wang, Yingcai
    He, Min
    Zhu, Jing
    Qiao, Jun
    MATERIALS CHEMISTRY AND PHYSICS, 2022, 288
  • [30] Influence of Sn Addition on the Ignition Resistance and Microstructural Evolution of Non-Flammable Mg-9Al-0.8Zn-0.1Mn-0.3Ca-0.2Y Alloy
    Go, Yohan
    Kim, Young Min
    METALS AND MATERIALS INTERNATIONAL, 2024, : 1708 - 1719