Effect of Aging on Tensile and Chemical Properties of Polylactic Acid and Polylactic Acid-Like Polymer Materials for Additive Manufacturing

被引:3
作者
Golubovic, Zorana [1 ]
Bojovic, Bozica [1 ]
Kirin, Snezana [2 ]
Milovanovic, Aleksa [2 ]
Petrov, Ljubisa [2 ]
Andelkovic, Boban [3 ]
Sofrenic, Ivana [3 ]
机构
[1] Univ Belgrade, Fac Mech Engn, Belgrade 11120, Serbia
[2] Innovat Ctr Fac Mech Engn, Belgrade 11120, Serbia
[3] Univ Belgrade, Fac Chem, Belgrade 11158, Serbia
关键词
additive manufacturing; 3D printing; PLA; PLA-like resin; fused deposition modeling (FDM); digital light processing (DLP); tensile testing; Fourier transform infrared spectrometry (FTIR); 3D scanning; statistical analysis; MECHANICAL-PROPERTIES; POLY(LACTIC ACID); LACTIC-ACID; PLA; DEGRADATION; BEHAVIOR; PARAMETERS; IMPACT;
D O I
10.3390/polym16081035
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Additive manufacturing, with its fast development and application of polymeric materials, led to the wide utilization of polylactic acid (PLA) materials. As a biodegradable and biocompatible aliphatic polyester, produced from renewable sources, PLA is widely used in different sectors, from industry to medicine and science. The aim of this research is to determine the differences between two forms of the PLA material, i.e., fused deposition modeling (FDM) printed filament and digital light processing (DLP) printed resin, followed by aging due to environmental and hygiene maintenance conditions for a period of two months. Specimens underwent 3D scanning, tensile testing, and Fourier transform infrared (FTIR) spectrometry to obtain insights into the material changes that occurred. Two-way Analysis of Variance (ANOVA) statistical analysis was subsequently carried out to determine the statistical significance of the determined changes. Significant impairment can be observed in the dimensional accuracies between both materials, whether they are non-aged or aged. The mechanical properties fluctuated for aged FDM specimens: 15% for ultimate tensile stress, 15% for elongation at yield, and 12% for elastic modulus. Regarding the DLP aged specimens, the UTS decreased by 61%, elongation at yield by around 61%, and elastic modulus by 62%. According to the FTIR spectral analysis, the PLA materials degraded, especially in the case of resin specimens. Aging also showed a significant influence on the elastic modulus, ultimate tensile stress, elongation at yield, elongation at break, and toughness of both materials, which was statistically shown by means of a two-way ANOVA test. The data collected in this research give a better understanding of the underlying aging mechanism of PLA materials.
引用
收藏
页数:14
相关论文
共 63 条
  • [1] In Vitro Comparison of the Cytotoxicity and Water Sorption of Two Different Denture Base Systems
    Akin, Hakan
    Tugut, Faik
    Polat, Zubeyde Akin
    [J]. JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2015, 24 (02): : 152 - 155
  • [2] Aging of 3D Printed Polymers under Sterilizing UV-C Radiation
    Amza, Catalin Gheorghe
    Zapciu, Aurelian
    Baciu, Florin
    Vasile, Mihai Ion
    Popescu, Diana
    [J]. POLYMERS, 2021, 13 (24)
  • [3] Accelerated Aging Effect on Mechanical Properties of Common 3D-Printing Polymers
    Amza, Catalin Gheorghe
    Zapciu, Aurelian
    Baciu, Florin
    Vasile, Mihai Ion
    Nicoara, Adrian Ionut
    [J]. POLYMERS, 2021, 13 (23)
  • [4] One Year Evaluation of Material Properties Changes of Polylactide Parts in Various Hydrolytic Degradation Conditions
    Andrzejewska, Angela
    [J]. POLYMERS, 2019, 11 (09)
  • [5] [Anonymous], 2012, PlasticsDetermination of Tensile PropertiesPart 2: Test Conditions for Moulding and Extrusion Plastics
  • [6] A review on PLA with different fillers used as a filament in 3D printing
    Arockiam, A. Joseph
    Subramanian, Karthikeyan
    Padmanabhan, R. G.
    Selvaraj, Rajeshkumar
    Bagal, Dilip Kumar
    Rajesh, S.
    [J]. MATERIALS TODAY-PROCEEDINGS, 2022, 50 : 2057 - 2064
  • [7] Tribological behavior of natural fiber reinforced PLA composites
    Bajpai, Pramendra Kumar
    Singh, Inderdeep
    Madaan, Jitendra
    [J]. WEAR, 2013, 297 (1-2) : 829 - 840
  • [8] Recent update on potential cytotoxicity, biocompatibility and preventive measures of biomaterials used in dentistry
    Bapat, Ranjeet Ajit
    Parolia, Abhishek
    Chaubal, Tanay
    Dharamadhikari, Suyog
    Abdulla, Anshad Mohamed
    Sakkir, Nasil
    Arora, Suraj
    Bapat, Prachi
    Sindi, Amal M.
    Kesharwani, Prashant
    [J]. BIOMATERIALS SCIENCE, 2021, 9 (09) : 3244 - 3283
  • [9] Effect of Thermal and Hydrothermal Accelerated Aging on 3D Printed Polylactic Acid
    Bergaliyeva, Saltanat
    Sales, David L. L.
    Delgado, Francisco J. J.
    Bolegenova, Saltanat
    Molina, Sergio I. I.
    [J]. POLYMERS, 2022, 14 (23)
  • [10] Bigg DM, 1996, SOC PLAST E, V42, P2028