Theoretical and experimental study on mixed-mode I plus II fracture characteristics of thermally treated granite under liquid nitrogen cooling

被引:2
|
作者
Yuan, Yilei [1 ]
Wang, Chaolin [1 ]
Zhao, Yu [1 ]
Zheng, Kun [1 ]
Bi, Jing [1 ]
机构
[1] Guizhou Univ, Coll Civil Engn, Guiyang 550025, Peoples R China
基金
中国国家自然科学基金;
关键词
HDR; Granite; Liquid nitrogen cooling; Fracture toughness; GMTS; TOUGHNESS; BRITTLE; DIMENSION; STRESS; CRITERION; GEOMETRY;
D O I
10.1016/j.tafmec.2024.104426
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Liquid nitrogen fracturing technology is widely used in the exploitation of hot dry rock (HDR) geothermal resources. It is necessary to understand the fracture characteristics of hot dry rocks under liquid nitrogen cooling. In this study, the mixed-mode I + II fracture characteristics of the thermally treated granite under liquid nitrogen cooling were investigated. The results indicate that as the exposed temperature increases, the number of internal microcracks increases, while the fracture energy and fracture toughness of the granites decrease. From 25 degrees C to 600 degrees C, mode I fracture toughness decreases from 1.286MP & sdot;m1/2 to 0.612MP & sdot;m1/2; mode II fracture toughness decreases from 0.830MP & sdot;m1/2 to 0.413MP & sdot;m1/2; mixed-mode I+II fracture toughness decreases from 1.082 MP & sdot;m1/2 to 0.530MP & sdot;m1/2 at Me = 0.705 and from 0.914 MP & sdot;m1/2 to 0.445 MP & sdot;m1/2 at Me = 0.427, respectively. Additionally, the intergranular fracture behavior increases as temperature increases, resulting in an increase in irregularity of fracture surfaces. The generalized maximum tangential stress (GMTS) criterion is used for predicting the fracture characteristics (fracture initiation angle and fracture toughness) of thermal damaged granites. The accuracy of the GMTS criterion in predicting crack resistance when mode II loading dominates has been improved by considering the variation of critical damage radius.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Experimental and numerical mixed-mode I plus II fracture characterization of carbon fi bre reinforced polymer laminates using a novel strategy
    Ramirez, Francis M. G.
    de Moura, Marcelo F. S. F.
    Moreira, Raul D. F.
    Silva, Filipe G. A.
    COMPOSITE STRUCTURES, 2021, 263
  • [42] Mixed-mode I plus II fracture characterization of human cortical bone using the Single Leg Bending test
    Silva, F. G. A.
    de Moura, M. F. S. F.
    Dourado, N.
    Xavier, J.
    Pereira, F. A. M.
    Morais, J. J. L.
    Dias, M. I. R.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 54 : 72 - 81
  • [43] Mixed-mode I plus II fatigue/fracture characterisation of bi-material Aluminium/CFRP bonded joints
    Moreira, R. D. F.
    de Moura, M. F. S. F.
    Silva, F. G. A.
    Reina, J. P. A.
    COMPOSITES PART B-ENGINEERING, 2022, 246
  • [44] Characteristics of mixed-mode I-II fracture of bedding mud shale based on discrete element method
    Suo, Yu
    Dong, Muyu
    Wang, Zijian
    Gao, Jiahao
    Fu, Xiaofei
    Pan, Zhejun
    Xie, Kun
    Qi, Tiantian
    Wang, Guanzhong
    JOURNAL OF PETROLEUM SCIENCE AND ENGINEERING, 2022, 219
  • [45] Pure (I and II) and mixed-mode (I plus II) fracture characterisation of unidirectional AS4/Low-melt-Polyaryletherketone™ polymer composites
    Pereira, Ruben
    de Moura, Marcelo
    Moreira, Raul
    Correia, Nuno
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2024, 43 (23-24) : 1393 - 1404
  • [46] Local Strain Energy Density Applied to Bainitic Functionally Graded Steels Plates Under Mixed-Mode (I plus II) Loading
    Salavati, H.
    Alizadeh, Y.
    Berto, F.
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2015, 28 (02) : 164 - 172
  • [47] Loading rate effect on mixed-mode I plus II fracture of V-notched Brazilian disc rock specimen under impact loads
    Liu, Wei
    Li, Yulong
    Zhang, Zhiqian
    Yang, Liyun
    Luo, Yi
    Yue, Zhongwen
    ENGINEERING FRACTURE MECHANICS, 2023, 291
  • [48] Study of the fracture behavior of mode I and mixed mode I/II cracks in tunnel under impact loads
    Zhou, Lei
    Zhu, Zheming
    Dong, Yuqing
    Ying, Peng
    Wang, Meng
    TUNNELLING AND UNDERGROUND SPACE TECHNOLOGY, 2019, 84 : 11 - 21
  • [49] Mixed-mode I/II fracture behavior for adhesively-bonded pultruded GFRP joint under four-point bending
    Jiang, Zhengwen
    Fang, Zhi
    Wan, Shui
    COMPOSITE STRUCTURES, 2020, 252
  • [50] Mixed mode I/II and I/III fracture toughness investigation for preplaced aggregate concrete mixtures: Experimental study and theoretical prediction
    Raeisi, Roya
    Rezaie, Freydoon
    Aliha, M. R. M.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2024, 47 (08) : 2873 - 2887