Fracture mechanisms of selective laser sintered parts manufactured in build direction

被引:0
作者
Cronau, J. [1 ]
Kroenert, M. [2 ]
Engstler, F. [1 ]
机构
[1] Univ Bundeswehr HAW, Werner Heisenberg Weg 39, D-85577 Munich, Germany
[2] Wehrwissensch Inst Werk & Betriebsstoffe WIWeB, Inst Weg 1, D-85435 Erding, Germany
关键词
Selective laser sintering (SLS); Surface roughness; Build direction; Fracture; MULTI JET FUSION; PERFORMANCE; PARAMETERS; BEHAVIOR;
D O I
10.1007/s40964-024-00677-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Selective laser sintering (SLS) is an additive manufacturing process that, in addition to rapid prototyping, is becoming increasingly popular to produce end-use parts. Predictable mechanical properties of the produced parts through this process is a desired primary goal. It has long been known that the mechanical properties especially the elongation at break of SLS components decrease in the build direction. In various test series with tensile specimen fabricated in build direction by SLS, it was found that, on the one hand, these have a very large scatter of the elongation at break, and, on the other hand, it was noticed that these frequently break outside the test range in the upskin radius. The upskin area describes regions that point in a positive build direction relative to the building plate. The fracture occurs at a point where, due to the specimen cross-section, a lower fracture stress occurs than in the test area of the specimen. This fracture leads to a much lower elongation at break than in the case of specimens that fracture in the test area. This study investigates which mechanism triggers this behavior. It turns out that different roughnesses can be determined in the upskin and downskin radius and different defects can be seen in the fracture surfaces, especially in the edge areas. It cannot be predicted based on surface roughness measurements or surface profiling exactly where, or in which layer the fracture occurs. However, the defects lead to a local stress spike, at which the failure of the specimen begins.
引用
收藏
页码:1407 / 1413
页数:7
相关论文
共 26 条
[1]   Anisotropic material properties of fused deposition modeling ABS [J].
Ahn, SH ;
Montero, M ;
Odell, D ;
Roundy, S ;
Wright, PK .
RAPID PROTOTYPING JOURNAL, 2002, 8 (04) :248-257
[2]  
[Anonymous], 1996, 4288199804 DIN EN IS
[3]  
[Anonymous], 2019, PlasticsDetermination of Tensile PropertiesPart 1: General Principles
[4]  
[Anonymous], 2012, DIN EN ISO 527-2:2012-06
[5]  
Berretta S, 2014, HIGH VALUE MANUFACTURING: ADVANCED RESEARCH IN VIRTUAL AND RAPID PROTOTYPING, P49
[6]   Effect of the build orientation on the mechanical performance of polymeric parts produced by multi jet fusion and selective laser sintering [J].
Calignano, Flaviana ;
Giuffrida, Federico ;
Galati, Manuela .
JOURNAL OF MANUFACTURING PROCESSES, 2021, 65 :271-282
[7]   Dependence of mechanical properties of polyamide components on build parameters in the SLS process [J].
Caulfield, B. ;
McHugh, P. E. ;
Lohfeld, S. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 182 (1-3) :477-488
[8]   Effect of PA12 powder reuse on coalescence behaviour and microstructure of SLS parts [J].
Dadbakhsh, Sasan ;
Verbelen, Leander ;
Verkinderen, Olivier ;
Strobbe, Dieter ;
Van Puyvelde, Peter ;
Kruth, Jean-Pierre .
EUROPEAN POLYMER JOURNAL, 2017, 92 :250-262
[9]   O Mechanical characterization of 3D-printed polymers [J].
Dizon, John Ryan C. ;
Espera, Alejandro H., Jr. ;
Chen, Qiyi ;
Advincula, Rigoberto C. .
ADDITIVE MANUFACTURING, 2018, 20 :44-67
[10]   Impact of surface porosity and topography on the mechanical behavior of high strength biomedical polymers [J].
Evans, Nathan T. ;
Irvin, Cameron W. ;
Safranski, David L. ;
Gall, Ken .
JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 59 :459-473