Growth behavior and kinetics of interfacial IMC for ZnSnCuNiAl/Cu solder joints subjected to isothermal aging

被引:3
作者
Chen, Wenjing [1 ]
Hu, Xiaowu [2 ]
Tang, Jiancheng [3 ]
机构
[1] Jiangxi Sci & Technol Normal Univ, Sch Mat & Energy, Nanchang 330038, Peoples R China
[2] Nanchang Univ, Sch Adv Mfg, Nanchang 330031, Peoples R China
[3] Nanchang Univ, Int Inst Mat Innovat, Nanchang 330031, Peoples R China
基金
中国国家自然科学基金;
关键词
LEAD-FREE SOLDER; HIGH-TEMPERATURE SOLDERS; PB-FREE SOLDER; INTERMETALLIC COMPOUND; SN-BI; MICROSTRUCTURE EVOLUTION; MECHANICAL-PROPERTIES; THERMAL PARAMETERS; CU; ALLOY;
D O I
10.1007/s10854-024-13436-0
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Zn-30Sn-2Cu-0.5Ni-0.2Al (ZnSnCuNiAl) solder joints were isothermally aged in the temperature range of 100-170 degrees C for up to 360 h, and the growth behavior and kinetics of the intermetallic compound (IMC) formed between the ZnSnCuNiAl solder and Cu substrate during the aging process were investigated. The results showed that the interfacial reaction between the liquid solder and the solid Cu substrate caused the formation of IMC layers, which were composed of a thin irregular scallop-shaped epsilon-CuZn5 layer and a thick gamma-Cu5Zn8 layer. With the increase in aging temperature and time, the serrated epsilon-CuZn5 layer gradually peeled off from the IMC interface and entered the solder due to thermal mismatch induced cracks between epsilon-CuZn5 and gamma-Cu5Zn8. The growth of the IMC layer at the solder joint interface was controlled by the bulk diffusion, and its thickness had a linear relationship with the square root of the aging time. Diffusion coefficients and activation energy for the interfacial Cu5Zn8 IMC layer were plotted as a function of aging temperature, and the values were calculated by the Arrhenius equation. The calculated activation energy of the Cu5Zn8 IMC layer was 77.78 kJ/mol, which was higher than that of the similar IMC layer in other lead-free solder joints, indicating a slower growth rate of the IMC layer between the solder and substrate during aging.
引用
收藏
页数:15
相关论文
共 47 条
[11]   Interfacial evolution and mechanical properties of Au-Sn solder jointed Cu heat sink during high temperature storage test [J].
Ho, Ching-Yuan ;
Lin, Chia-Wei ;
Lee, Yueh-Yang ;
Cheng, Shao-Chien .
MATERIALS LETTERS, 2020, 275
[12]   Intermetallic compound growth behavior and mechanical performance in Sn58Bi/Cu solder joint bearing Mg particles incorporation during thermal aging [J].
Huang, Xi ;
Zhang, Liang ;
Zhang, Jia-Min ;
Chen, Chen ;
Lu, Xiao ;
Sun, Lei .
MATERIALS CHARACTERIZATION, 2024, 208
[13]   Kinetics of intermetallic compound layer growth and interfacial reactions between Sn-8Zn-5In solder and bare copper substrate [J].
Kim, DG ;
Jang, HS ;
Jung, SB .
MATERIALS SCIENCE AND TECHNOLOGY, 2005, 21 (03) :381-385
[14]   Fe addition to Sn-3.5Ag solder for the suppression of Kirkendall void formation [J].
Kim, S. H. ;
Yu, Jin .
SCRIPTA MATERIALIA, 2013, 69 (03) :254-257
[15]   Prediction of interface reaction products between Cu and various solder alloys by thermodynamic calculation [J].
Lee, BJ ;
Hwang, NM ;
Lee, HM .
ACTA MATERIALIA, 1997, 45 (05) :1867-1874
[16]   Thermodynamic prediction of interface phases at Cu/solder joints [J].
Lee, HM ;
Yoon, SW ;
Lee, BJ .
JOURNAL OF ELECTRONIC MATERIALS, 1998, 27 (11) :1161-1166
[17]   Interfacial properties of Zn-Sn alloys as high temperature lead-free solder on Cu substrate [J].
Lee, JE ;
Kim, KS ;
Suganuma, K ;
Takenaka, J ;
Hagio, K .
MATERIALS TRANSACTIONS, 2005, 46 (11) :2413-2418
[18]   Effects of Cu on the interfacial reactions between Sn-8Zn-3Bi-xCu solders and Cu substrate [J].
Liu, Lijuan ;
Wu, Ping ;
Zhou, Wei .
MICROELECTRONICS RELIABILITY, 2014, 54 (01) :259-264
[19]   Joining of sintered NdFeB permanent magnet to steel using novel Zn-Sn-Bi-Nd alloy: Microstructure and soldering mechanism [J].
Luo, Cui ;
Qiu, Xiaoming ;
Su, Jinlong ;
Xu, Yuxin ;
Zhao, Xiaohui ;
Xing, Fei .
JOURNAL OF MANUFACTURING PROCESSES, 2021, 67 :487-495
[20]   Effect of Bi addition on the activation energy for the growth of Cu5Zn8 intermetallic in the Sn-Zn lead-free solder [J].
Mayappan, Ramani ;
Ahmad, Zainal Arifin .
INTERMETALLICS, 2010, 18 (04) :730-735