Face bonding strength of cross laminated northern hardwoods and softwoods lumber

被引:4
|
作者
Musah, Munkaila [1 ,2 ]
Ma, Yunxiang [1 ]
Wang, Xiping [1 ,3 ]
Ross, Robert [1 ,3 ]
Hosseinpourpia, Reza [1 ,4 ]
Jiang, Xiaolei [1 ,5 ]
Xie, Xinfeng [1 ]
机构
[1] Michigan Technol Univ, Coll Forest Resources & Environm Sci, Houghton, MI 49931 USA
[2] Univ Massachusetts Amherst, Dept Environm Conservat, Amherst, MA 01003 USA
[3] USDA, Forest Prod Lab, Madison, WI 53726 USA
[4] Linneaus Univ, Dept Forestry & Wood Technol, Vaxjo, Sweden
[5] Henan Agr Univ, Coll Forestry, Zhengzhou 450002, Henan, Peoples R China
关键词
Hardwood; Cross-laminated timber (CLT); Specific gravity; Pore distribution; Bond properties; Bond strength; Percentage of wood failure;
D O I
10.1016/j.conbuildmat.2024.135405
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Producing cross-laminated timber (CLT) has opened a new market for the lumber industry in North America, while few hardwood species have been studied in the U.S. for CLT production. Combining hardwood species in mixed hardwood CLT or in hybrid CLT can be a solution to boost the market of the undervalued hardwoods. However, the knowledge gap on bonding hardwoods needs to be filled to provide evidence of feasibility. This study focused on the face bonding properties of the cross laminations made of seven hardwood species and two softwood species from the Great Lakes region using two commercial structural adhesives, the phenol resorcinol adhesive (the Resorcinol) and the melamine urea formaldehyde adhesive (the Melamine). A total of 45 combinations of the selected species were studied for the bonding strength (shear under compression) and the percentage of wood failure. For single species samples, the bond strength was positively related to the specific gravity of wood and the bond strength of hardwoods was 33% and 82% stronger than that of softwoods bonded with the Resorcinol and the Melamine respectively. The mixed hardwoods showed higher bonding strength (the Melamine: 5.45 MPa, the Resorcinol: 5.28 MPa) than mixed softwoods (the Melamine: 2.8 MPa and the Resorcinol: 2.7 MPa). Among the Resorcinol bonded mixed combinations, 54% had a percentage of wood failure less than 80%, while the Melamine bonded had only 4 out of 22 which had a percentage of wood failure less than 80%. The overall bonding strength of the hybrid combinations was 5% weaker than that of the mixed hardwoods. All hybrid combinations bonded with the Melamine met the 80% wood failure criterium, but some bonded with the Resorcinol had a percentage of wood failure less than 80%. Anatomical features, especially pore distribution, played a key role in the bonding performance. However, the Melamine adhesive consistently achieved over 80% wood failure across all pore distribution types.
引用
收藏
页数:10
相关论文
共 6 条
  • [1] Durability of the adhesive bond in cross-laminated northern hardwoods and softwoods
    Musah, Munkaila
    Wang, Xiping
    Dickinson, Yvette
    Ross, Robert J.
    Rudnicki, Mark
    Xie, Xinfeng
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 307
  • [2] Cross-Laminated Timber in the USA: Opportunity for Hardwoods?
    Omar Espinoza
    Urs Buehlmann
    Current Forestry Reports, 2018, 4 : 1 - 12
  • [3] Cross-Laminated Timber in the USA: Opportunity for Hardwoods?
    Espinoza, Omar
    Buehlmann, Urs
    CURRENT FORESTRY REPORTS, 2018, 4 (01): : 1 - 12
  • [4] Screw Withdrawal Strength of Heat-Treated and Laminated Veneer Lumber Reinforced with Carbon and Glass Fibers
    Percin, Osman
    Uzun, Oguzhan
    BIORESOURCES, 2022, 17 (02) : 2486 - 2500
  • [5] Evaluation of bond strength of cross-laminated LSL specimens under short-span bending
    Gong, Meng
    Li, Ling
    Chui, Ying-Hei
    HOLZFORSCHUNG, 2019, 73 (08) : 789 - 795
  • [6] The effects of ply organization and loading direction on bending strength and modulus of elasticity in laminated veneer lumber (LVL) obtained from beech (Fagus orientalis L.) and lombardy poplar (Populus nigra L.)
    Burdurlu, Erol
    Kilic, Murat
    Ilce, Abdullah Cemil
    Uzunkavak, Ozan
    CONSTRUCTION AND BUILDING MATERIALS, 2007, 21 (08) : 1720 - 1725