摘要
In an effort to understand the various phenomena which occur during aging of silica gels at different pH, silica particles prepared by three routes distinguished principally by their silicon coordination (Q(n) distributions) (Stober silica spheres, Ludox and Cab-O-Sil) were employed. In situ techniques were used including proton spin-lattice relaxation, SAXS and zeta potential for the wet state and Si-29 MAS-NMR, SEM, TEM and N-2 sorption for dry samples. In solution, the surface area increased in the following order after aging at pH 10 as compared with that at pH 7 and the initial dry surface area: Cab-O-Sil < Ludox << Stober which is inversely proportional to the degree of silicon coordination. This same trend was observed for the surface charge measurements. Surface areas calculated from Si-29 MAS-NMR for four different Stober sphere sizes were of order 1000 m(2)/g as compared with nitrogen/BET surface areas which varied from 9 to 370 m(2)/g, indicating significant internal surface which is inaccessible to nitrogen. The Si-29 NMR results for the Stober spheres were consistent with a close packed aggregate of similar to 3 nm primary particles. In addition to particulate silica, aging at varying pH of a two-step acid/base-catalyzed silica gel was studied. At all pH values, the surface area was higher in the wet gel as compared with the xerogel. Aging at higher pH was found to yield lower surface area, larger pore volume and a narrower pore size distribution depending upon the pH, aging time and surface tension of the final pore fluid.
引用
收藏
页码:295 / 306
页数:12
相关论文
共 37 条
  • [1] PORE STRUCTURE EVOLUTION IN SILICA-GEL DURING AGING DRYING .2. EFFECT OF PORE FLUIDS
    DAVIS, PJ
    BRINKER, CJ
    SMITH, DM
    ASSINK, RA
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1992, 142 (03) : 197 - 207
  • [2] THE ROLE OF PORE FLUID IN AGING ON SILICA-GEL PORE STRUCTURE
    SMITH, DM
    DAVIS, PJ
    BRINKER, CJ
    ASSINK, R
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1990, 200 : 243 - COLL
  • [3] PORE STRUCTURE EVOLUTION IN SILICA-GEL DURING AGING DRYING .1. TEMPORAL AND THERMAL AGING
    DAVIS, PJ
    BRINKER, CJ
    SMITH, DM
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1992, 142 (03) : 189 - 196
  • [4] PORE STRUCTURE EVOLUTION IN SILICA-GEL DURING AGING DRYING .3. EFFECTS OF SURFACE-TENSION
    DESHPANDE, R
    HUA, DW
    SMITH, DM
    BRINKER, CJ
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1992, 144 (01) : 32 - 44
  • [5] PORE STRUCTURE OF SILICA-GEL
    SARAN, T
    PAUL, IB
    CHATTERJEE, DS
    JOURNAL OF APPLIED CHEMISTRY AND BIOTECHNOLOGY, 1978, 28 (09): : 633 - 637
  • [6] FORMATION OF THE PORE STRUCTURE OF SILICA-GEL
    PENKOV, NV
    SHAMRIKOV, VM
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 1994, 67 (04) : 585 - 587
  • [7] EFFECTS OF CALCINATION ON PORE STRUCTURE OF SILICA-GEL
    KATSUZAWA, H
    KATOH, T
    KOBAYASHI, J
    NIPPON KAGAKU KAISHI, 1975, (08) : 1280 - 1285
  • [8] THEORY OF THE FORMATION OF THE PORE STRUCTURE OF SILICA-GEL
    SHAMRIKOV, VM
    PENKOV, NV
    MALKIMAN, VI
    KESAREVA, GM
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 1993, 66 (12) : 2114 - 2115
  • [9] FORMATION OF STRUCTURE OF SILICA-GEL DURING DRYING
    FENELONOV, VB
    TARASOVA, DV
    GAVRILOV, VY
    KINETICS AND CATALYSIS, 1977, 18 (02) : 402 - 408
  • [10] CHEMISORPTION OF DIBORANE ON SILICA-GEL - A STUDY OF THE CHANGES IN PORE STRUCTURE
    GILLISDHAMERS, I
    VRANCKEN, KC
    VANDERVOORT, P
    VANSANT, EF
    DEROY, G
    JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS, 1992, 88 (10): : 1459 - 1462