SOLID-STATE WELDING OF A 027 CARBON, CHROMIUM MOLYBDENUM STEEL

被引:0
|
作者
LEFRANCOIS, P [1 ]
CRIQUI, B [1 ]
HOURCADE, M [1 ]
机构
[1] RENAULT AUTOMOBILES,RUEIL MALMAISON,FRANCE
关键词
SOLID-STATE WELDING; DYNAMIC DIFF WELDING; STEEL DIFFUSION WELDING VS FRICTION WELDING; 27CD4; STEEL; RAPID WELDING TIME; MECHANICAL TESTING; METALLOGRAPHIC ANALYSIS; FRACTOGRAPHIC ANALYSIS; INDUSTRIAL PRODUCTION;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Solid state welding is often carried out in a vacuum chamber under rather low pressure (2 to 50 MPa) and temperatures. It offers considerable advantages, especially metallurgical ones. Indeed, with good process conditions, it generates no important microstructural degradation such as those occurring with classical techniques of fusion or friction welding. It is a soft joining process that generates only a small deformation of the samples. However, classical diffusion welding requires welding durations ranging from some dozens of minutes to several hours. Because of the cost incurred, the process can be employed only in industries such as the electronic, nuclear, aerospace and military industries. A new process, dynamic diffusion welding (DDW), was improved in our laboratory (Ref. 4). It offers the advantages of both classical diffusion welding and rapidity. With DDW, new perspectives are opened for using this welding process in mass production, since it is consistent with the constraints of productivity. For this reason, dynamic diffusion welding of 27CD4 steel has been studied. The application targeted has been the welding of transmission shafts, which are presently made by friction welding. It was proven possible to carry out high-strength joints in a very short time: 30 s for heating to the welding temperature and a few seconds at the isothermal anneal. With the optimal conditions defined in this study, namely a welding time of several seconds, in a nitrogen with 5% hydrogen gas, with a proper surface preparation (Rmax = 0.4 mum) and under a modulated pressure during the whole welding process: 1) The tensile behavior of the joints is reproducible. 2) Failure occurs out of the interface with a tensile strength of 950 MPa and with an elongation of 22% (bainitic and martensitic structure). 3) Deformation of the welded specimens is limited to about 2% of the heated length. 4) The failure energy of joints measured with impact tests is lower than that of the base metal. This process is also efficient for making other ferrous alloy welds. An additional mechanical characterization is now going on in our laboratory, our purpose being, among others, to assess the fatigue endurance.
引用
收藏
页码:S313 / S320
页数:8
相关论文
共 50 条
  • [21] Solid state welding of steel and magnesium alloy using a rotating pin - Solid state welding of dissimilar metals using a rotating pin (report 3)
    Watanabe, Takehiko
    Kagiya, Kazuhiko
    Yanagisawa, Atsushi
    Tanabe, Hiroshi
    Yosetsu Gakkai Ronbunshu/Quarterly Journal of the Japan Welding Society, 2006, 24 (01): : 108 - 115
  • [22] A SOLID-STATE POTENTIOMETRIC SENSOR FOR MONITORING HYDROGEN IN COMMERCIAL PIPELINE STEEL
    MORRIS, DR
    WAN, L
    CORROSION, 1995, 51 (04) : 301 - 311
  • [23] Finite Element Simulative Analysis on the Influence of Solid-state Transformation on Welding Residual Stress
    Li, Chunrun
    Zhang, Zhipeng
    Zhang, Yiming
    Fang, Zongtao
    CURRENT TRENDS IN THE DEVELOPMENT OF INDUSTRY, PTS 1 AND 2, 2013, 785-786 : 1229 - +
  • [24] Effect of cooling media on residual stresses induced by a solid-state welding: underwater FSW
    Papahn, Hossein
    Bahemmat, Pouya
    Haghpanahi, Mohammad
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2016, 83 (5-8) : 1003 - 1012
  • [25] Advanced solid-state welding based on computational manufacturing using the additive manufacturing process
    Shah, Preet Ashok
    Srinath, M. K.
    Gayathri, R.
    Puvandran, P.
    Selvaraj, Senthil Kumaran
    INTERNATIONAL JOURNAL OF INTERACTIVE DESIGN AND MANUFACTURING - IJIDEM, 2023,
  • [26] Effect of cooling media on residual stresses induced by a solid-state welding: underwater FSW
    Hossein Papahn
    Pouya Bahemmat
    Mohammad Haghpanahi
    The International Journal of Advanced Manufacturing Technology, 2016, 83 : 1003 - 1012
  • [27] High-throughput micromachining of steel and ceramics with solid-state UV laser
    Govorkov, SV
    Slobodchikov, EV
    Wiessner, AO
    Basting, D
    HIGH-POWER LASER ABLATION III, 2000, 4065 : 790 - 800
  • [28] Effect of tempering on the chemical and phase composition of MxCy precipitates in low carbon chromium-molybdenum-vanadium steel
    Skobir, DA
    Vodopivec, F
    Spaic, S
    Markoli, B
    ZEITSCHRIFT FUR METALLKUNDE, 2004, 95 (11): : 1020 - 1024
  • [29] Interfacial corrosion behavior of aluminum/steel joints prepared by solid-state additive manufacturing
    Li, Yidi
    Teng, Jianwei
    Wang, Jun
    Wang, Hui
    Liu, Qinglin
    Lai, Ruilin
    Yang, Biaobiao
    Wang, Zhongchang
    Li, Yunping
    CORROSION SCIENCE, 2025, 244
  • [30] Performance Comparison of Advanced Ceramic Cladding Approaches via Solid-State and Traditional Welding Processes: A Review
    Selvaraj, Senthil Kumaran
    Srinivasan, Kathiravan
    Deshmukh, Jainendra
    Agrawal, Darshit
    Mungilwar, Sailam
    Jagtap, Rucha
    Hu, Yuh-Chung
    MATERIALS, 2020, 13 (24) : 1 - 22