The straining metal electrode technique was applied to the study of stress corrosion cracking (SCC) susceptibility of Type 304 austenitic stainless steel in H//2SO//4 solutions and in H//2SO//4 plus NaCl solutions, at room temperature. A film formation process was detected in the active zone of Type 304 in H//2SO//4 plus NaCl solutions. It is concluded that a film rupture mechanism operates during SCC of this metal in H//2SO//4 plus NaCl solutions.
引用
收藏
页码:60 / 66
页数:7
相关论文
共 18 条
[1]   STRESS-CORROSION CRACKING OF AUSTENITIC STAINLESS-STEEL IN HYDROCHLORIC-ACID MEDIA AT ROOM-TEMPERATURE [J].
BIANCHI, G ;
MAZZA, F ;
TORCHIO, S .
CORROSION SCIENCE, 1973, 13 (03) :165-&
[2]   DEFORMATION OF ANODIC OXIDE FILMS [J].
BUBAR, SF ;
VERMILYEA, DA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1966, 113 (09) :892-+
[3]  
Galvele J. R., 1974, LOCALIZED CORROSION, P580
[4]   FILM RUPTURE MECHANISM FOR STRESS-CORROSION CRACKING OF AISI-304 IN HCL SOLUTIONS [J].
GALVELE, JR ;
DEWEXLER, SB ;
GARDIAZABAL, I .
CORROSION, 1975, 31 (10) :352-357
[5]  
GALVELE JR, 1976, PASSIVITY ITS BREAKD, P178
[6]  
GALVELE JR, 1978, 7TH INT C MET CORR R
[7]   GRAIN-BOUNDARY CORROSION OF AISI TYPE 304L STEEL IN AN H2 SO4-NACL ENVIRONMENT [J].
HAKKARAINEN, TJ ;
HONKASALO, A .
CORROSION, 1976, 32 (07) :271-273
[8]   MECHANISM OF CAUSTIC CRACKING OF CARBON-STEELS .1. INFLUENCE OF ELECTRODE POTENTIAL AND FILM FORMATION [J].
HOAR, TP ;
JONES, RW .
CORROSION SCIENCE, 1973, 13 (10) :725-738
[9]   MECHANOCHEMICAL ANODIC DISSOLUTION OF AUSTENITIC STAINLESS STEEL IN HOT CHLORIDE SOLUTION AT CONTROLLED ELECTRODE POTENTIAL [J].
HOAR, TP ;
SCULLY, JC .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1964, 111 (03) :348-352
[10]   MECHANO-CHEMICAL ANODIC DISSOLUTION [J].
HOAR, TP ;
WEST, JM .
NATURE, 1958, 181 (4612) :835-835