MICROSTRUCTURAL COARSENING AT HIGH-TEMPERATURES IN RAPIDLY SOLIDIFIED TI-5WT-PERCENT-AL-2.9WT-PERCENT-Y AND TI-5WT-PERCENT-AL-7.5WT-PERCENT-TH

被引:1
|
作者
WHANG, SH [1 ]
PARK, WW [1 ]
KIM, PK [1 ]
KIM, DH [1 ]
机构
[1] SEOUL NATL UNIV,DEPT MET ENGN,SEOUL 151,SOUTH KOREA
来源
关键词
D O I
10.1016/0025-5416(88)90150-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:173 / 177
页数:5
相关论文
共 50 条
  • [1] A STUDY OF PRECIPITATION IN TI-3WT-PERCENT-CU AND TI-3WT-PERCENT-CU-5WT-PERCENT-AL ALLOYS BY TEM AND ATOM PROBE
    MENAND, A
    HADJADJ, L
    VASSEL, A
    SCRIPTA METALLURGICA, 1987, 21 (10): : 1295 - 1300
  • [2] MICROSTRUCTURAL TRANSITIONS IN RAPIDLY SOLIDIFIED AL-7.5WT-PERCENT FE ALLOYS
    DESANCTIS, M
    WOODFIELD, AP
    LORETTO, MH
    INTERNATIONAL JOURNAL OF RAPID SOLIDIFICATION, 1988, 4 (1-2): : 53 - 74
  • [3] SUPERPLASTIC FORMING AND THE RESULTING MECHANICAL-PROPERTIES OF TI-14WT-PERCENT-AL-20WT-PERCENT-NB-3.2WT-PERCENT-V-2WT-PERCENT-MO
    LEDERICH, RJ
    MCAFEE, JL
    SCHWARTZ, DS
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1994, 189 (1-2): : 29 - 33
  • [4] SUPERPLASTIC BEHAVIOR OF AL-5WT-PERCENT-CA-5WT-PERCENT-ZN ALLOY
    RAMIREZ, P
    ALDAY, FG
    ADABBO, HE
    RUANO, OA
    MATERIALS SCIENCE AND ENGINEERING, 1987, 93 : L11 - L15
  • [5] THE CONSOLIDATION OF RAPIDLY SOLIDIFIED AL-5WT PERCENT-CR-2WT PERCENT-ZR(-1 WT PERCENT-MN) ALLOY PARTICULATE BY HOT-ROLLING
    SILVA, MP
    JONES, H
    SELLARS, CM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1991, 134 : 1107 - 1110
  • [6] DOUBLE MECHANICAL ALLOYING OF AL-5WT-PERCENT-FE-4WT-PERCENT-MN
    LEBRUN, P
    FROYEN, L
    DELAEY, L
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 157 (01): : 79 - 88
  • [7] THE MICROSTRUCTURE OF RAPIDLY SOLIDIFIED AL-3.7 WT-PERCENT NI-1.5 WT-PERCENT FE
    BENDERSKY, LA
    BOETTINGER, WJ
    SCHAEFER, RJ
    BIANCANIELLO, FS
    JOURNAL OF METALS, 1985, 37 (08): : A66 - A66
  • [8] THE EFFECT OF A MAGNESIUM ADDITION ON THE MICROSTRUCTURE OF RAPIDLY SOLIDIFIED AL-8WT-PERCENT-FE-3WT-PERCENT-MM
    PARADKAR, AG
    RAO, KN
    RAO, PV
    MISHRA, RS
    INTERNATIONAL JOURNAL OF RAPID SOLIDIFICATION, 1992, 7 (03): : 167 - 175
  • [9] MICROSTRUCTURAL CHARACTERIZATION OF AL98.5WT-PERCENT-SI1.0WT-PERCENT-CU0.5WT-PERCENT ON CHEMICAL-VAPOR-DEPOSITED-W
    PICO, CA
    BONIFIELD, TD
    JOURNAL OF MATERIALS RESEARCH, 1993, 8 (05) : 1001 - 1009
  • [10] SPINODAL DECOMPOSITION IN CO-3WT-PERCENT TI-1WT-PERCENT FE AND CO-3 WT-PERCENT TI-2 WT-PERCENT FE ALLOYS
    SINGH, J
    LELE, S
    RANGANATHAN, S
    JOURNAL OF MATERIALS SCIENCE, 1980, 15 (08) : 2010 - 2016