The wetting of silicon nitride by chromium-containing alloys

被引:10
作者
Xiao, P
Derby, B
机构
[1] Department of Materials, University of Oxford, Oxford, OX1 3PH, Parks Road
关键词
D O I
10.1007/BF01151505
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The wetting of ceramic materials by metallic melts is the most important characteristic of brazing alloys. The effect of chromium additions to copper-base alloys on the wetting of silicon nitride was investigated. Wetting experiments were carried out on Si3N4 using liquid Cu-Cr, Cu-Ni-Cr, Cu-Si-Cr and Cu-Ni-Si-Cr alloys. The addition of chromium to liquid copper up to its solubility limit promoted wetting on Si3N4. Improved wetting with a higher chromium content was achieved by the addition of nickel to the Cu-Cr alloys. The formation of an interfacial reaction layer, which is detrimental for brazing ceramics, was suppressed by the addition of silicon to the chromium-containing brazing alloys.
引用
收藏
页码:5915 / 5922
页数:8
相关论文
共 15 条
[1]  
Nicholas M.G., Mortimer D.A., Jones L.M., Crispin R.M., J. Mater. Sci., 25, (1990)
[2]  
Kim D.H., Hwang S.H., Chun S.S., Ceramic. Int., 16, (1990)
[3]  
Kristalis P., Courdrier L., Eustathopoulos N., J. Mater. Sci., 26, (1991)
[4]  
Nicholas M.G., Joining of Ceramics, (1990)
[5]  
Naidich, The Wettability of Solids by Liquid Metals, Prog. Surf. Memb. Sci., 14, (1981)
[6]  
Kristalis P., Merlin V., Courdrier L., Eustathopoulos N., Effect of Cr on interfacial interaction and wetting mechanisms in Ni Alloy/Alumina systems, Acta Metallurgica et Materialia, 40, (1992)
[7]  
Chakrabarti D.J., Laughlin D.E., Bull. Alloy Phase Diagr., 5, (1984)
[8]  
Brandes E.A., Brook G.B., Smithells Metals Reference Book, (1992)
[9]  
Austin Chang Y., Fitzner K., Zhang, Prog. Mater. Sci., 32, (1988)
[10]  
Peteves S.D., Moulaert M., Nicholas M.G., Metall. Trans., 23 A, (1992)