HIGH-TEMPERATURE OXIDATION OF NI-20CR-CHI-TIO2 ALLOYS

被引:10
|
作者
NAGAI, H [1 ]
OKABAYASHI, M [1 ]
MURAKAMI, T [1 ]
机构
[1] OSAKA UNIV,GRAD SCH,SUITA,OSAKA 565,JAPAN
来源
TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS | 1982年 / 23卷 / 08期
关键词
D O I
10.2320/matertrans1960.23.473
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
引用
收藏
页码:473 / 479
页数:7
相关论文
共 50 条
  • [41] A similarity of the high-temperature oxidation of high-temperature alloys
    Bagerman, AZ
    Guseva, VI
    Zhivushkin, AA
    PROTECTION OF METALS, 1999, 35 (06): : 600 - 601
  • [42] Effect of Al on high-temperature oxidation of Cr-W alloys
    Dogan, O. N.
    OXIDATION OF METALS, 2008, 69 (3-4): : 233 - 247
  • [43] HIGH-TEMPERATURE OXIDATION OF ALUMINIZED FE-17 CR ALLOYS
    ELMAJID, Z
    LAMBERTIN, M
    JOURNAL DE CHIMIE PHYSIQUE ET DE PHYSICO-CHIMIE BIOLOGIQUE, 1985, 82 (01) : 67 - 73
  • [44] High-temperature oxidation of Fe-Cr alloys in wet oxygen
    Shen Jianian
    Zhou Longjiang
    Li Tiefan
    Oxidation of Metals, 1997, 48 : 347 - 356
  • [45] High-temperature oxidation of Fe-Cr alloys in wet oxygen
    Shen, J
    Zhou, LJ
    Li, TF
    OXIDATION OF METALS, 1997, 48 (3-4): : 347 - 356
  • [46] HIGH-TEMPERATURE EMBRITTLEMENT OF NI AND NI-CR ALLOYS BY TRACE-ELEMENTS
    WHITE, CL
    SCHNEIBEL, JH
    PADGETT, RA
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (04): : 595 - 610
  • [47] Thermodynamic assessment of high-temperature oxidation of Fe—Cr alloys in air
    O. Yu. Goncharov
    Inorganic Materials, 2004, 40 : 1295 - 1300
  • [48] Mechanistic insights into the oxidation behavior of Ni alloys in high-temperature CO2
    Oleksak, Richard P.
    Baltrus, John P.
    Nakano, Jinichiro
    Nakano, Anna
    Holcomb, Gordon R.
    Dogan, Omer N.
    CORROSION SCIENCE, 2017, 125 : 77 - 86
  • [49] High-temperature oxidation behavior of low-energy high-flux nitrided Ni and Ni-20% Cr substrates
    Pedraza, F
    Reffass, M
    Balmain, J
    Bonnet, G
    Dinhut, JF
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 357 (1-2): : 355 - 364
  • [50] High temperature oxidation and erosion-oxidation behaviour of HVOF sprayed Ni-20Cr, WC-20Cr-7Ni and Cr3C2-Ni-20Cr coatings
    Kunioshi, CT
    Correa, OV
    Ramanathan, LV
    SURFACE ENGINEERING, 2006, 22 (02) : 121 - 127