THE FRACTURE-RESISTANCE OF METAL-CERAMIC INTERFACES

被引:45
作者
EVANS, AG
DALGLEISH, BJ
机构
[1] Materials Department, College of Engineering, University of California, Santa Barbara
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 1993年 / 162卷 / 1-2期
关键词
D O I
10.1016/0921-5093(90)90025-X
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effects of interface structure and microstructure on the fracture energy GAMMA(i) of metal-ceramic interfaces are reviewed. Some systems exhibit a ductile fracture mechanism and others fail by brittle mechanisms. In the absence of either interphases phases or reaction products, GAMMA(i) is dominated by plastic dissipation (for both fracture mechanisms), leading to important effects of metal thickness h, and yield strength sigma0,. Additionally, GAMMA(i) is larger when fracture occurs by ductile void growth (for the same h and sigma0). A fundamental understanding now exists for the ductile fracture mechanism. However, some basic issues remain to be understood when fracture occurs by brittle bond rupture, particularly with regard to the role of the work of adhesion W(ad). Interphases and reaction products have been shown to have an important effect on GAMMA(i). A general trend found by experiments is that GAMMA(i) scales with the fracture energy of the interphase itself, wherein GAMMA(i) tends to increase for the interphase sequence amorphous oxides > crystalline oxides > intermetallics. However, there also appear to be important effects of the residual stresses in the interface (which influence the fracture mechanism) and the layer thickness.
引用
收藏
页码:1 / 13
页数:13
相关论文
共 50 条
[11]   Constrained cavitation and fast fracture at metal-ceramic interfaces at elevated temperatures [J].
Kennefick, CM .
JOURNAL OF MATERIALS RESEARCH, 1999, 14 (04) :1306-1315
[12]   Metal-ceramic and ceramic-ceramic interfaces and their applications [J].
Feuersanger, AE .
HIGH TEMPERATURE MATERIALS CHEMISTRY, PTS I AND II, PROCEEDINGS, 2000, 15 :293-296
[13]   Fracture in metal-ceramic composites [J].
Agrawal, P ;
Sun, CT .
COMPOSITES SCIENCE AND TECHNOLOGY, 2004, 64 (09) :1167-1178
[14]   METAL CERAMIC INTERFACIAL FRACTURE-RESISTANCE USING THE CONTINUOUS MICROSCRATCH TECHNIQUE [J].
VENKATARAMAN, SK ;
KOHLSTEDT, DL ;
GERBERICH, WW .
THIN SOLID FILMS, 1993, 223 (02) :269-275
[15]   THE EFFECT OF REACTION-PRODUCTS ON THE FRACTURE-RESISTANCE OF A METAL CERAMIC INTERFACE [J].
BARTLETT, A ;
EVANS, AG .
ACTA METALLURGICA ET MATERIALIA, 1993, 41 (02) :497-504
[16]   Phase formation at metal-ceramic interfaces [J].
Schuster, JC .
INTERFACIAL SCIENCE IN CERAMIC JOINING, 1998, 58 :183-194
[17]   Misfit dislocations at metal-ceramic interfaces [J].
Vellinga, W.P. ;
De Hosson, J.Th.M. .
Physica Status Solidi (A) Applied Research, 1995, 149 (01) :95-103
[18]   MISFIT DISLOCATIONS AT METAL-CERAMIC INTERFACES [J].
VELLINGA, WP ;
DEHOSSON, JTM .
PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1995, 149 (01) :95-103
[19]   Special issue on metal-ceramic interfaces [J].
Kaplan, WD ;
Finnis, MW .
INTERFACE SCIENCE, 2004, 12 (01) :5-5
[20]   Fracture resistance of five different metal framework designs for metal-ceramic restorations [J].
Ulusoy, M ;
Toksavul, S .
INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2002, 15 (06) :571-574