Fracture resistance of endodontically treated teeth restored with direct resin restoration reinforced with fibre post and polyethylene fibre - an in vitro study

被引:0
作者
Srinivasan, Archana [1 ]
Nadig, Roopa [1 ]
Gananeela, Usha [1 ]
Boregowda, Vedavathi [1 ]
Venataramanaswamy, Swapna Devarasanahaali [1 ]
Jagdeesh, Karthik [1 ]
机构
[1] Dayananda Sagar Coll Dent Sci, Dept Conservat Dent & Endodont, Bangalore, Karnataka, India
来源
ENDO-ENDODONTIC PRACTICE TODAY | 2013年 / 7卷 / 04期
关键词
fibre post; fracture resistance; polyethylene fibre;
D O I
暂无
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Aims and objective: To evaluate the effect of various reinforcement techniques with polyethylene fibre and fibre post on the fracture resistance of endodontically treated teeth. Materials and methods: Forty intact maxillary premolars receiving endodontic treatment and MOD cavity preparation were divided into four groups: Group I - restored with resin composite; Group II - fibre post inserted into the palatal canal followed by resin composite restoration; Group III - polyethylene fibre inserted in the occlusal third of the MOD cavity followed by resin composite restoration; and Group IV - fibre post transfixed horizontally in a buccolingual direction within the MOD cavity, followed by resin composite restoration. Fracture resistance was evaluated using the Universal testing machine. Results: ANOVA statistical analysis showed no significant difference in the fracture resistance between Group 1 and Group 2, whereas, a significant difference was seen between Group 1 and Group 3 and also Group 1 and Group 4. The difference in mean fracture resistance was found to be statistically significant between Group 2 and Group 3 as well as between Group 2 and Group 4. No statistically significant difference was observed between Group 3 and Group 4 with respect to the mean fracture resistance (P > 0.05). Conclusion: Horizontally transfixed fibre post and polythelene fibre placed within the resin composite restoration showed improved fracture resistance.
引用
收藏
页码:305 / 310
页数:6
相关论文
共 20 条
  • [1] Ausiello P, 1997, AM J DENT, V10, P237
  • [2] BARKMEIER WW, 1992, OPER DENT, P50
  • [3] Reinforcement effect of polyethylene fibre in root-filled teeth: comparison of two restoration techniques
    Belli, S
    Erdemir, A
    Yildirim, C
    [J]. INTERNATIONAL ENDODONTIC JOURNAL, 2006, 39 (02) : 136 - 142
  • [4] Ex vivo fracture resistance of direct resin composite complete crowns with and without posts on maxillary premolars
    Fokkinga, WA
    Le Bell, AM
    Kreulen, CM
    Lassila, LVJ
    Vallittu, PK
    Creugers, NHJ
    [J]. INTERNATIONAL ENDODONTIC JOURNAL, 2005, 38 (04) : 230 - 237
  • [5] Beltrao MCG, 2009, AM J DENT, V22, P9
  • [6] The effect of fiber reinforcement on the fracture toughness and flexural strength of provisional restorative resins
    Hamza, TA
    Rosenstiel, SF
    Elhosary, MM
    Ibraheem, RM
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 2004, 91 (03) : 258 - 264
  • [7] Periapical health related to the quality of coronal restorations and root fillings
    Hommez, GMG
    Coppens, CRM
    De Moor, RJG
    [J]. INTERNATIONAL ENDODONTIC JOURNAL, 2002, 35 (08) : 680 - 689
  • [8] Krejci I, 2003, OPER DENT, V28, P127
  • [9] Meerbeek BV, 2006, FUNDAMENTALS OPERATI, P200
  • [10] Effect of the Number of Residual Walls on Fracture Resistances, Failure Patterns, and Photoelasticity of Simulated Premolars Restored with or without Fiber-reinforced Composite Posts
    Nam, Sook-Hyun
    Chang, Hoon-Sang
    Min, Kyung-San
    Lee, Yoon
    Cho, Hye-Won
    Bae, Ji-Myung
    [J]. JOURNAL OF ENDODONTICS, 2010, 36 (02) : 297 - 301