OXIDATION WEIGHT-GAIN AND STRENGTH DEGRADATION OF SI3N4 WITH VARIOUS ADDITIVES

被引:8
作者
WU, CC
MCKINNEY, KR
RICE, RW
MCDONOUGH, WJ
FREIMAN, SW
机构
关键词
D O I
10.1007/BF00540318
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:3099 / 3104
页数:6
相关论文
共 14 条
[1]   The Rate Controlling Process in the Oxidation of Hot Pressed Silicon Nitride [J].
Cubicciotti, D. ;
Lau, K. H. ;
Jones, R. L. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1977, 124 (12) :1955-1956
[2]   KINETICS OF OXIDATION OF YTTRIA HOT-PRESSED SILICON-NITRIDE [J].
CUBICCIOTTI, D ;
LAU, KH .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (10) :1723-1728
[3]  
FREIMAN SW, 1978, 1977 P DEF ADV RES P, P655
[4]  
FREIMAN SW, 1977, CERAMIC MICROSTRUCTU, P824
[5]   PHASE RELATIONS IN SYSTEM SI3N4-SIO2-MGO AND THEIR INTERRELATION WITH STRENGTH AND OXIDATION [J].
LANGE, FF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1978, 61 (1-2) :53-56
[6]  
MCDONOUGH WJ, 1981, J AM CERAM SOC, V63, pC45
[7]  
PALM JA, 1980, AM CERAM SOC BULL, V59, P447
[8]  
RICE RW, 1978, CERAMICS HIGH PERFOR, V2, P669
[9]   THERMODYNAMICS AND KINETICS OF OXIDATION OF HOT-PRESSED SILICON-NITRIDE [J].
SINGHAL, SC .
JOURNAL OF MATERIALS SCIENCE, 1976, 11 (03) :500-509
[10]  
TANZILLI RA, 1979, 79SDR2324 GEN EL TEC