共 15 条
- [1] EVOLUTION OF THE KINETIC-PROPERTIES IN A FAMILY OF SUBSTITUTED LANI5 HYDRIDES DURING ACTIVATING FORMATION-DECOMPOSITION CYCLING [J]. JOURNAL OF THE LESS-COMMON METALS, 1980, 73 (01): : 69 - 77
- [2] DEGRADATION PROCESSES IN A LANI5 ELECTRODE [J]. JOURNAL OF THE LESS-COMMON METALS, 1989, 155 (01): : 119 - 131
- [3] BOONSTRA AH, 1989, J LESS-COMMON MET, V159, P327
- [5] STABILITY OF RECHARGEABLE HYDRIDING ALLOYS DURING EXTENDED CYCLING [J]. JOURNAL OF THE LESS-COMMON METALS, 1984, 99 (01): : 1 - 14
- [7] OGAWA H, 1988, 16TH P INT POW SOURC, P393
- [8] PERCHERON A, 1977, P INT S HYDRIDES ENE, P485
- [9] Reichman B., 1987, US Patent, Patent No. [4,716,088, 4716088]
- [10] SOME FACTORS AFFECTING THE CYCLE LIVES OF LANI5-BASED ALLOY ELECTRODES OF HYDROGEN BATTERIES [J]. JOURNAL OF THE LESS-COMMON METALS, 1990, 161 (02): : 193 - 202