EVALUATION OF SOME PROPERTIES OF AN OPAQUE PORCELAIN FIRED SIMULTANEOUSLY WITH THE BODY PORCELAIN

被引:5
作者
OBRIEN, WJ
BOENKE, KM
GROH, CL
机构
[1] School of Dentistry, The University of Michigan, Ann Arbor, MI
关键词
D O I
10.1016/0022-3913(94)90562-2
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Recently, a porcelain-fused-to-metal opaque porcelain was introduced that does not require a separate firing before application of the body porcelain. The objective of this study was to determine the properties of this new opaque porcelain and its ability to bond to metal. The properties studied included flexural strength, linear firing shrinkage, coefficient of thermal expansion, powder particle size, and ability to bond to body porcelain and dental alloys. Sintering of this opaque porcelain was complete when fired at 1760 degrees F (960 degrees C) with a linear firing shrinkage of 13.1% +/- 0.2%. No boundary between the opaque and body porcelains could be found with a scanning electron microscope after firing at 1760 degrees F (960 degrees C). The mean flexural strengths were 99 +/- 7 and 101 +/- 8 MPa respectively, for this opaque porcelain and a conventional opaque porcelain, and were not significantly different as assessed with Student's t-test (p = 0.548). The coefficient of thermal expansion for this opaque porcelain was 13.3 +/- 0.2 X 10(-6)/degrees C. Particle size analysis showed a 63% increase in the particles below 5 mu m for this opaque porcelain and bonding to two alloys was adequate as indicated by its cohesive failure. Simultaneous firing of this special opaque porcelain and body porcelain produced satisfactory sintering, strength, and bonding to metal.
引用
收藏
页码:414 / 419
页数:6
相关论文
共 50 条
[41]   Titanium-porcelain system .2. Bond strength of fired porcelain on nitrided pure titanium [J].
Oshida, Y ;
Fung, LW ;
Isikbay, SC .
BIO-MEDICAL MATERIALS AND ENGINEERING, 1997, 7 (01) :13-34
[42]   Low-fired porcelain with diopside and marshalite additions [J].
V. I. Vereshchagin ;
N. V. Mogilevskaya ;
D. V. Gorbachev .
Glass and Ceramics, 2013, 69 :401-404
[43]   Some types of porcelain. [J].
Riddlle, FH ;
McDanel, WW .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1918, 1 (09) :606-627
[44]   EFFECTS OF OPAQUE AND PORCELAIN SURFACE TEXTURE ON THE COLOR OF CERAMOMETAL RESTORATIONS [J].
OBREGON, A ;
GOODKIND, RJ ;
SCHWABACHER, WB .
JOURNAL OF PROSTHETIC DENTISTRY, 1981, 46 (03) :330-340
[45]   Low-Fired Electrotechnical Porcelain with Diopside Additives [J].
Vereshchagin, V. I. ;
Gorbachev, D. V. ;
Mogilevskaya, N. V. .
GLASS AND CERAMICS, 2021, 78 (1-2) :18-22
[46]   Effect of Environmental Exposure on Two Types of Opaque Dental Porcelain [J].
Kundie, Fathie ;
Ahmad, Zainal Arifin .
2ND INTERNATIONAL MATERIALS, INDUSTRIAL, AND MANUFACTURING ENGINEERING CONFERENCE, MIMEC2015, 2015, 2 :61-65
[47]   Low-fired porcelain with diopside and marshalite additions [J].
Vereshchagin, V. I. ;
Mogilevskaya, N. V. ;
Gorbachev, D. V. .
GLASS AND CERAMICS, 2013, 69 (11-12) :401-404
[48]   EFFECT OF METAL SURFACE TREATMENT ON MASKING POWER OF OPAQUE PORCELAIN [J].
HERZBERG, TW ;
WEBBER, RL ;
MOFFA, JP ;
GETTLEMAN, L .
JOURNAL OF DENTAL RESEARCH, 1972, 51 (02) :468-+
[49]   The influence of carbonates on the technological properties of an industrial porcelain type body [J].
Dagounaki, C. ;
Sikalidis, C. ;
Kassoli-Fournaraki, A. ;
Tsirambides, A. .
INDUSTRIAL CERAMICS, 2009, 29 (02) :99-105
[50]   Effect of calcined colemanite additions on properties of hard porcelain body [J].
Akpinar, S. ;
Evcin, A. ;
Ozdemir, Y. .
CERAMICS INTERNATIONAL, 2017, 43 (11) :8364-8371