EXPLOSIVE COMPACTION OF SILICON-NITRIDE POWDER WITHOUT ADDITIVES USING A WATER-PRESSURE MEDIUM

被引:0
|
作者
TOMOSHIGE, R
CHIBA, A
NISHIDA, M
IMAMURA, K
FUJITA, M
机构
[1] KUMAMOTO UNIV,DEPT MAT SCI & RESOURCE ENGN,KUMAMOTO 860,JAPAN
[2] KUMAMOTO UNIV,DEPT MECH ENGN,KUMAMOTO 860,JAPAN
关键词
SILICON NITRIDE WITHOUT ADDITIVES; UNDERWATERSHOCK WAVE; FRACTURE TOUGHNESS; SEM; TEM; GRAIN BOUNDARY;
D O I
暂无
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Silicon nitride powder compacts without additives were produced by underwater-shock wave. The as-compacted specimens and sintered ones at various temperatures were characterized by relative density, micro Vickers hardness and fracture toughness. Microstructural characterization was also made by SEM and TEM. The relative density of an as-compacted specimen was about 75%, but hardness value was quite low about 2 GPa. Mechanical properties were remarkably improved by sintering. Hardness and fracture toughness values of the specimen sintered at 1973 K for 5h were about 24 GPa and about 4 MPa square-root m, respectively. TEM observation of the compact sintered at 1973 K showed that there was no large glass pockets at grain boundary edges and that the glass phases at grain boundary surfaces were a few atoms thick.
引用
收藏
页码:1230 / 1234
页数:5
相关论文
共 21 条