Effect of Heat Treatment on Microstructure and Tensile Properties of A356/V2O5 Insitu Composites

被引:8
作者
Singla, Amneesh [1 ]
Garg, Rajnish [1 ]
Saxena, Mukesh [2 ]
机构
[1] Univ Petr & Energy Studies, Dept Mech Engn, Dehra Dun 248007, India
[2] Univ Technol & Management, Shillong 793003, Meghalaya, India
关键词
A356; Alloy; Hardness; Heat Treatment; Microstructure; Tensile Property; V2O5;
D O I
10.4018/IJMMME.2016070101
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A 356 alloy reinforced with insitu V2O5 particles by using stir casting technique. The composites were produced by the addition of oxide particles in different weight percentage. The effect of oxide powder addition on microstructure and mechanical properties of produced composites were investigated. The effect of heat treatment on microstructure and mechanical properties were investigated by optical microscope, Microhardness tester and tension test. A significant improvement in hardness and tensile strength was revealed in the produced composite as compared to the base alloy. With the addition of oxide particles, the shape and size of eutectic Si changed which in turn affects the properties. It was observed that 2h solutionizing followed by the artificial aging was sufficient to make the structure homogenize and to produce the hardening precipitates. The improvement in the mechanical properties has been observed due to the age hardening precipitates in addition with refinement of insitu V2O5 particles.
引用
收藏
页码:1 / 10
页数:10
相关论文
共 23 条
  • [1] Microstructural, mechanical and tribological properties of Al-7Si-(0-5)Zn alloys
    Alemdag, Yasin
    Beder, Murat
    [J]. MATERIALS & DESIGN, 2014, 63 : 159 - 167
  • [2] The effect of Mg on the microstructure and mechanical behavior of Al-Si-Mg casting alloys
    Caceres, CH
    Davidson, CJ
    Griffiths, JR
    Wang, QG
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (10): : 2611 - 2618
  • [3] Effect of grain refinement and modification on the dry sliding wear behaviour of eutectic Al-Si alloys
    Chandrashekharaiah, T. M.
    Kori, S. A.
    [J]. TRIBOLOGY INTERNATIONAL, 2009, 42 (01) : 59 - 65
  • [4] WEAR CHARACTERISTICS OF AS-CAST BINARY ALUMINIUM-SILICON ALLOYS
    CLARKE, J
    SARKAR, AD
    [J]. WEAR, 1979, 54 (01) : 7 - 16
  • [5] Dwivedi DK, 2001, T INDIAN I METALS, V54, P247
  • [6] The precipitation sequence in Al-Mg-Si alloys
    Edwards, GA
    Stiller, K
    Dunlop, GL
    Couper, MJ
    [J]. ACTA MATERIALIA, 1998, 46 (11) : 3893 - 3904
  • [7] Gruzleski J.E., 1990, AFS ILLIONS, P1
  • [8] The influence of impurity level and tin addition on the ageing heat treatment of the 356 class alloy
    Kliauga, A. M.
    Vieira, E. A.
    Ferrante, M.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 480 (1-2): : 5 - 16
  • [9] Sliding wear characteristics of Al-7Si-0.3Mg alloy with minor additions of copper at elevated temperature
    Kori, S. A.
    Prabhudev, M. S.
    [J]. WEAR, 2011, 271 (5-6) : 680 - 688
  • [10] Kumari SSS., 2002, INDIAN FOUNDRY J, V48, P27