From the Fe79Cr6.6B14.4 metallic glass ribbons (prepared in a longitudinal or transversal magnetic field) the strip-shape samples were cut and annealed without the field at temperatures 80 to 360-degrees-C. The maximum of the magnetomechanical coupling coefficient (k(m) = 0.20-0.25) was observed after annealing at 350-degrees-C.